CN103510519A - 一种快速凝固水泥土的施工方法 - Google Patents

一种快速凝固水泥土的施工方法 Download PDF

Info

Publication number
CN103510519A
CN103510519A CN201310215598.1A CN201310215598A CN103510519A CN 103510519 A CN103510519 A CN 103510519A CN 201310215598 A CN201310215598 A CN 201310215598A CN 103510519 A CN103510519 A CN 103510519A
Authority
CN
China
Prior art keywords
soil
cement
cemented soil
anchoring section
anchor hole
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310215598.1A
Other languages
English (en)
Inventor
徐萍
吴鸣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310215598.1A priority Critical patent/CN103510519A/zh
Publication of CN103510519A publication Critical patent/CN103510519A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种快速凝固水泥土的施工方法,包含以下步骤:一、将加热带埋入设有锚具的锚孔中;然后往锚孔中注入水泥,使加热带设置在锚固段水泥土中;二、给加热带通电,并控制加热带的温度在40-60之间,继续时间在5-7天,锚固段水泥土即可凝固,并达到设计要求的强度;本发明所述的快速凝固水泥土的施工方法,可以使锚孔中锚固段水泥土快速凝固,同时,加热带的温度可控且适度,可以防止加热带温度过高而烧坏锚固段水泥土,影响凝固后的锚固段水泥土的性能;本发明所述的快速凝固水泥土的施工方法,可以在5-7天的时间内快速使锚孔中锚固段水泥土凝固,并达到下步施工的技术要求,比起现有的水泥土80-100天的凝固期,可大大的缩短了工期。

Description

一种快速凝固水泥土的施工方法
技术领域
本发明涉及一种施工方法,特别是一种可使锚孔中的水泥土快速凝固,以缩短施工工期的快速凝固水泥土的施工方法。
背景技术
随着城市化进程的推进,地下停车场、地下行人通道、地下商业街、地下铁道等地下设施的建设均需要进行基坑及边坡支护。
现有基坑及边坡支护技术中,通常利用钻头在岩土体中钻出锚孔,并在锚孔的底部钻出扩大部;然后将锚具放置扩大部中,再往锚孔中注入水泥,直至扩大部中的水泥土凝固,再进行下一步的施工,目前,扩大部中的水泥土凝固时间大概要80-100天,这样就导致整个施工期过长。有些工地,为了赶工期,不等扩大部中的水泥土凝固,就进行下一步施工,这样就会产生因水泥土的强度不够而产生的质量问题,严重的甚至会造成人员伤亡事件及豆腐渣工程。
发明内容
针对上述存在的技术问题,本发明的目的是:提出了一种可使锚孔中的水泥土快速凝固,以缩短施工工期的快速凝固水泥土的施工方法。
本发明的技术解决方案是这样实现的:一种快速凝固水泥土的施工方法,包含以下步骤:
一、将加热带埋入设有锚具的锚孔中;然后往锚孔中注入水泥,使加热带设置在锚固段水泥土中;
二、给加热带通电,并控制加热带的温度在40-60之间,继续时间在5-7天,锚固段水泥土即可凝固,并达到设计要求的强度。
由于上述技术方案的运用,本发明与现有技术相比具有下列优点:
本发明所述的快速凝固水泥土的施工方法,可以使锚孔中锚固段水泥土快速凝固,同时,加热带的温度可控且适度,可以防止加热带温度过高而烧坏锚固段水泥土,影响凝固后的锚固段水泥土的性能;本发明所述的快速凝固水泥土的施工方法,可以在5-7天的时间内快速使锚孔中锚固段水泥土凝固,并达到下步施工的技术要求,比起现有的水泥土80-100天的凝固期,可大大的缩短了工期。
附图说明
下面结合附图对本发明技术方案作进一步说明:
附图1为本发明所述的快速凝固水泥土的施工方法的施工示意图;
附图2为本发明所述的快速凝固水泥土的施工方法的试验时温度-时间曲线图;
附图3为本发明所述的快速凝固水泥土的施工方法的试验时强度-时间曲线图;
其中:1、水泥土;2、加热带;3、岩土层;4、导线;5、隔离套管。
具体实施方式
下面结合附图来说明本发明。
本发明所述的一种快速凝固水泥土的施工方法,包含以下步骤:
一、将加热带埋入设有锚具的锚孔中;然后往锚孔中注入水泥,使加热带设置在锚固段水泥土中;
二、给加热带通电,并控制加热带的温度在40-60之间,继续时间在5-7天,锚固段水泥土即可凝固,并达到设计要求的强度。
如附图1所示为本实施例的具体试验的示意图,本实施例所述的快速凝固水泥土的施工方法,步骤如下:
1、取三轴搅拌桩返浆的水泥土,水泥掺量约20%;
2、水泥土放置在直径60cm,长度80cm的圆柱体岩土层3内,在水泥土1中心放置功率200kw的加热带2,所述加热带2的长度为80cm、宽度为3cm;所述加热带2与导线4的一端相连,导线4的另一端伸出岩土层3与电压调节器(未示出)相连;所述导线的中部穿过隔离套管5;
3、放置好加热带2后通电,用调节器控制电压在110kv,控制加热带的温度在40-60度之间,以避免温度太高会直接烧坏水泥土;
4、水泥土试件放置在室内,室温控制恒温10度,湿度在95%左右。
试验发现,见附图2、3,继续时间5-7天,水泥土的强度可达1.2-1.8MPa,达到设计要求的强度,并达到满足下步施工的技术要求,可大大缩短水泥土凝固时间,提高施工效率,缩短施工工期。
由于上述技术方案的运用,本发明与现有技术相比具有下列优点:
本发明所述的快速凝固水泥土的施工方法,可以使锚孔中锚固段水泥土快速凝固,同时,加热带的温度可控且适度,可以防止加热带温度过高而烧坏锚固段水泥土,影响凝固后的锚固段水泥土的性能;本发明所述的快速凝固水泥土的施工方法,可以在5-7天的时间内快速使锚孔中锚固段水泥土凝固,并达到下步施工的技术要求,比起现有的水泥土80-100天的凝固期,可大大的缩短了工期。
上述实施例只为说明本发明的技术构思及特点,其目的在于让熟悉此项技术的人士能够了解本发明的内容并加以实施,并不能以此限制本发明的保护范围,凡根据本发明精神实质所作的等效变化或修饰,都应涵盖在本发明的保护范围内。

Claims (1)

1.一种快速凝固水泥土的施工方法,包含以下步骤:
一、将加热带埋入设有锚具的锚孔中;然后往锚孔中注入水泥,使加热带设置在锚固段水泥土中;
二、给加热带通电,并控制加热带的温度在40-60之间,继续时间在5-7天,锚固段水泥土即可凝固,并达到设计要求的强度。
CN201310215598.1A 2013-06-03 2013-06-03 一种快速凝固水泥土的施工方法 Pending CN103510519A (zh)