CN103483904B - 钛箐蓝塑料黑色印刷油墨制造方法 - Google Patents

钛箐蓝塑料黑色印刷油墨制造方法 Download PDF

Info

Publication number
CN103483904B
CN103483904B CN201310422824.3A CN201310422824A CN103483904B CN 103483904 B CN103483904 B CN 103483904B CN 201310422824 A CN201310422824 A CN 201310422824A CN 103483904 B CN103483904 B CN 103483904B
Authority
CN
China
Prior art keywords
clumps
trees
thf
ink
tetrahydrofuran
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310422824.3A
Other languages
English (en)
Other versions
CN103483904A (zh
Inventor
韦丽梅
李�杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Yu Yu Color Printing Co., Ltd.
Original Assignee
韦丽梅
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 韦丽梅 filed Critical 韦丽梅
Priority to CN201310422824.3A priority Critical patent/CN103483904B/zh
Publication of CN103483904A publication Critical patent/CN103483904A/zh
Application granted granted Critical
Publication of CN103483904B publication Critical patent/CN103483904B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明的钛箐蓝塑料黑色印刷油墨制造方法,原料配方以重量计,由丙烯酸改性松香钙树脂45-60份,桐油10-15份,萘酸钴3-5份,酞菁蓝2-4份,炭黑20-30份,四氢呋喃10-20份,环己酮15-30份组成;制备过程为:将丙烯酸改性松香钙树脂、桐油、萘酸钴、酞菁蓝、炭黑、四氢呋喃、环己酮混合;在60℃下加热,熔化完全后搅拌1小时,即得产品;具有工艺简单,易于控制,产品质量稳定,适应性强,无有害溶剂,节能环保,使用方便等优点。

Description

钛箐蓝塑料黑色印刷油墨制造方法
技术领域
本发明属于一种油墨制造方法。
背景技术
目前,用于书刊、包装装潢、建筑装饰等各种印刷。随着社会需求增大,油墨品种和产量也相应扩展和增长。两千年前作为印刷的物质基础之一的墨便已出现了,国际间公认中国为古代文明中最先使用墨的国家,早在西汉时期(公元前200年)就开始使用墨了,这种墨可以在竹帛上写字传递信息,其某些功能与当代油墨可以类比的。公元1000年左右,北宋时期的毕升发明了胶泥活字印刷,大大提高了印刷效率。为了进一步提高生产效率和降低成本,缩短刻周期,有些地方开始使用软木刻版,这种刻版容易制作,出书快,成本低。元代印刷技术除了在安徽江西有大的发展以外,福建与浙江也成为印刷发展地区。明代是我国封建社会后期的文化昌盛的时代,也是印刷术发展的时期。从印刷技术的角度看明代的发展有如下特点:①已经发展了多色套版技术;②制墨技术又有很大进步;③印刷技术使用范围进一步扩大,书刊、报纸、广告、信纸皆是明代著名的印刷品;④活字版印书也有很大发展;⑤线装书广泛应用。15世纪德国的谷登堡发明了铅合金活字印刷,油墨有了改进,用灯黑作为颜料,亚麻油为连结料,用手工将其均匀混合但制成了当时的油墨。但是直到19世纪中叶,科学尤其是化学的进步,使得煤焦油染料以及色彩科学的发展,油墨制造商才能根据用户需要为用户制出具有不同色相、明度、不饱和度的各种颜色来。油墨生产进入了新的发展阶段。油墨的种类很多,物理性质各不相同,有的很稠、很黏,有的却相当稀。它的成分可以分为三大部分:其中液体成分称为连结料:固体成分为色料(颜料或染料)以及各种助剂。不同的油墨其干燥方式也不同;不同印刷过程所使用的油墨不同;不同的承印物材料使用的油墨也不同。以下按照油墨的干燥方式、不同的印刷过程以及承印物材料对油墨进行分类。使得油墨满足各种印刷过程的印刷适性。油墨应该具有一定的流动性,并且满足各种印刷过程所要求的性质,能够在印品上迅速干燥,干燥后的墨膜应该具有相应的各种耐水、耐酸、耐碱、耐光、耐擦、耐磨等耐抗性、色料(颜料或染料)以及各种助剂。对油墨来说,颜色、身骨(通常将稀稠度、流动性等油墨的流变性质称为油墨的身骨)和干燥性能是油墨三个最重要的性质,油墨是用于包装材料印刷的重要材料,它通过印刷将图案、文字表现在承印物上油墨中包括主要成分和辅助成分、颜料的配方配比等组成,是至关重要的,稍微改变,就会产生较大的差异,又以颜料对颜色最为敏感。
经中国公开专利检索,查到油墨的发明专利案3364件,没有发现与本发明相同的方案。
发明内容:
本发明的目的在于,提出一种钛箐蓝塑料黑色印刷油墨制造方法。
本发明的钛箐蓝塑料黑色印刷油墨制造方法,其特征在于:原料配方以重量计,由丙烯酸改性松香钙树脂45-60份,桐油10-15份,萘酸钴3-5份,酞菁蓝2-4份,炭黑20-30份,四氢呋喃10-20份,环己酮15-30份组成;制备过程为:将丙烯酸改性松香钙树脂、桐油、萘酸钴、酞菁蓝、炭黑、四氢呋喃、环己酮混合;在60℃下加热,熔化完全后搅拌1小时,即得产品。
本发明与现有技术相比其有益效果是:具有工艺简单,易于控制,产品质量稳定,适应性强,无有害溶剂,节能环保,使用方便等优点。
具体的实施方式:
实施例1
本发明的钛箐蓝塑料黑色印刷油墨制造方法,其特征在于:原料配方以重量计,由丙烯酸改性松香钙树脂45-60份,桐油10-15份,萘酸钴3-5份,酞菁蓝2-4份,炭黑20-30份,四氢呋喃10-20份,环己酮15-30份组成;制备过程为:将丙烯酸改性松香钙树脂、桐油、萘酸钴、酞菁蓝、炭黑、四氢呋喃、环己酮混合;在60℃下加热,熔化完全后搅拌1小时,即得产品。
实施例2
本发明的钛箐蓝塑料黑色印刷油墨制造方法,其特征在于:原料配方以重量计,由丙烯酸改性松香钙树脂45份,桐油10份,萘酸钴3份,酞菁蓝2份,炭黑20份,四氢呋喃10份,环己酮15份组成;制备过程为:将丙烯酸改性松香钙树脂、桐油、萘酸钴、酞菁蓝、炭黑、四氢呋喃、环己酮混合;在60℃下加热,熔化完全后搅拌1小时,即得产品。
实施例3
本发明的钛箐蓝塑料黑色印刷油墨制造方法,其特征在于:原料配方以重量计,由丙烯酸改性松香钙树脂60份,桐油15份,萘酸钴5份,酞菁蓝4份,炭黑30份,四氢呋喃20份,环己酮30份组成;制备过程为:将丙烯酸改性松香钙树脂、桐油、萘酸钴、酞菁蓝、炭黑、四氢呋喃、环己酮混合;在60℃下加热,熔化完全后搅拌1小时,即得产品。
实施例4
本发明的钛箐蓝塑料黑色印刷油墨制造方法,其特征在于:原料配方以重量计,由丙烯酸改性松香钙树脂50份,桐油13份,萘酸钴4份,酞菁蓝3份,炭黑25份,四氢呋喃15份,环己酮20份组成;制备过程为:将丙烯酸改性松香钙树脂、桐油、萘酸钴、酞菁蓝、炭黑、四氢呋喃、环己酮混合;在60℃下加热,熔化完全后搅拌1小时,即得产品。
实施例5
本发明的钛箐蓝塑料黑色印刷油墨制造方法,其特征在于:原料配方以重量计,由丙烯酸改性松香钙树脂60份,桐油10份,萘酸钴5份,酞菁蓝2份,炭黑23份,四氢呋喃20份,环己酮10份组成;制备过程为:将丙烯酸改性松香钙树脂、桐油、萘酸钴、酞菁蓝、炭黑、四氢呋喃、环己酮混合;在60℃下加热,熔化完全后搅拌1小时,即得产品。
本发明的钛箐蓝塑料黑色印刷油墨,所需原料均可在市场上购买获得。具有工艺简单,易于控制,产品质量稳定,适应性强,无有害溶剂,节能环保,使用方便等优点。

Claims (1)

1.一种钛箐蓝塑料黑色印刷油墨制造方法,其特征在于:原料配方以重量计,由丙烯酸改性松香钙树脂45-60份,桐油10-15份,萘酸钴3-5份,酞菁蓝2-4份,炭黑20-30份,四氢呋喃10-20份,环己酮15-30份组成;制备过程为:将丙烯酸改性松香钙树脂、桐油、萘酸钴、酞菁蓝、炭黑、四氢呋喃、环己酮混合;在60℃下加热,熔化完全后搅拌1小时,即得产品。
CN201310422824.3A 2013-09-17 2013-09-17 钛箐蓝塑料黑色印刷油墨制造方法 Active CN103483904B (zh)