CN103382682A - 一种高吸附性的滤清器滤纸及其制备方法 - Google Patents

一种高吸附性的滤清器滤纸及其制备方法 Download PDF

Info

Publication number
CN103382682A
CN103382682A CN2013102593806A CN201310259380A CN103382682A CN 103382682 A CN103382682 A CN 103382682A CN 2013102593806 A CN2013102593806 A CN 2013102593806A CN 201310259380 A CN201310259380 A CN 201310259380A CN 103382682 A CN103382682 A CN 103382682A
Authority
CN
China
Prior art keywords
parts
filter paper
filter
paper
sodium
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013102593806A
Other languages
English (en)
Inventor
金鑫
胡辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BENGBU SHOUCHUANG FILTER Co Ltd
Original Assignee
BENGBU SHOUCHUANG FILTER Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BENGBU SHOUCHUANG FILTER Co Ltd filed Critical BENGBU SHOUCHUANG FILTER Co Ltd
Priority to CN2013102593806A priority Critical patent/CN103382682A/zh
Publication of CN103382682A publication Critical patent/CN103382682A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种高吸附性的滤清器滤纸,它是由下述重量份的原料组成的:针叶木浆100-120、聚四氟乙烯纤维12-14、氯化石蜡2-3、陶瓷粉1-3、轻质碳酸钙1-3、明矾粉1-2、1,4-环己烷二甲醇1-2、己二酸丙二醇聚酯1-2、磷酸二氢铵0.3-0.5、海藻酸钠2-3、乙撑基双硬脂酰胺0.8-1、二氧化铈0.4-0.5、松香10-12、丙烯酸丁酯3-4、纳米二氧化硅3-5、无水乙醇20-25、羧甲基纤维素钠1-2、过硫酸钠0.2-0.4、水适量。本发明生产的滤纸滤清精度高,滤清效率高,空气阻力小,纳污能力强,环保,本发明的浸渍液,不仅改善了滤纸胶膜脆性大,对滤纸中纤维表面的粘结性不佳等缺点,还起到了多级过滤的效果,弥补了滤纸纤维间部分孔洞孔径较大的缺陷,提高了滤纸纤维间孔洞孔径的均匀性,强化了筛滤效应。

Description

一种高吸附性的滤清器滤纸及其制备方法
技术领域
    本发明主要涉及一种滤纸,尤其涉及一种高吸附性的滤清器滤纸及其制备方法。
背景技术
发动机有空气、机油、燃油三种滤清器,一般称作“三滤”。它们分别担负发动机进气系统、润滑系统和燃烧系统中介质的过滤。传统生产的滤清器滤纸因其滤纸孔径大、均匀性差、过滤效率低,不能将对发动机有害的杂质进行有效滤除,造成发动机早期磨损,滤清器滤纸用浸渍乳液现已由醇溶性向水溶性发展,常用的水溶性浸渍乳液如聚醋酸乙烯酯共聚乳液、苯丙乳液和纯丙烯酸酯系列乳液等,其中苯丙乳液最常用,但是经苯丙乳液浸渍后的滤纸胶膜脆性较大,对滤纸中纤维表面的粘结性不佳,且功能单体用量大、成本高,特别是挺度不高和不能在环境中降解。
发明内容
本发明目的就是提供一种高吸附性的滤清器滤纸及其制备方法。。
本发明是通过以下技术方案实现的:
一种高吸附性的滤清器滤纸,它是由下述重量份的原料组成的:
针叶木浆100-120、聚四氟乙烯纤维12-14、氯化石蜡2-3、陶瓷粉1-3、轻质碳酸钙1-3、明矾粉1-2、1,4-环己烷二甲醇1-2、己二酸丙二醇聚酯1-2、磷酸二氢铵0.3-0.5、海藻酸钠2-3、乙撑基双硬脂酰胺0.8-1、二氧化铈0.4-0.5、松香10-12、丙烯酸丁酯3-4、纳米二氧化硅3-5、无水乙醇20-25、羧甲基纤维素钠1-2、过硫酸钠0.2-0.4、水适量;
一种高吸附性的滤清器滤纸的制备方法,包括以下步骤:
将针叶木浆、聚四氟乙烯纤维加入碎浆机中,先疏解10-15分钟,打浆,加入浆料1-2%的乙烯基三乙氧基硅烷、乙撑基双硬脂酰胺,充分搅拌,再加入陶瓷粉、轻质碳酸钙、明矾粉,600-800转/分搅拌分散2-3分钟,得混合料;在上述混合料中加入除了松香、丙烯酸丁酯、纳米二氧化硅、无水乙醇、羧甲基纤维素钠、过硫酸钠以外的剩余各原料,加热至70-80℃,疏解、磨浆,加水至固含量为4-6%,由造纸机抄造成型,脱水;将松香加热熔解后,加入到无水乙醇中,搅拌分散,得分散液;将纳米二氧化硅分散到10-15倍水中,加入羧甲基纤维素钠、丙烯酸丁酯、过硫酸钠,在70-80℃下搅拌反应2-3小时,加入上述分散液,高速1600-2000转/分分散4-6分钟,过滤出料,得浸渍液;将脱水后的纸浸于上述新型浸渍液中浸渍2-3h,再用压力辊除去过量的浸渍液;在160-200℃下恒温烘干,喷涂聚乙二醇400,所述聚乙二醇400的用量为纸张重量的1-2%,120-130℃下烘干至干度95-98%,压光整理,即得所述高吸附性的滤清器滤纸。
本发明的优点是:
本发明生产的滤纸滤清精度高,滤清效率高,空气阻力小,纳污能力强,环保,本发明的浸渍液,不仅改善了滤纸胶膜脆性大,对滤纸中纤维表面的粘结性不佳等缺点,还起到了多级过滤的效果,弥补了滤纸纤维间部分孔洞孔径较大的缺陷,提高了滤纸纤维间孔洞孔径的均匀性,强化了筛滤效应。
具体实施方式
实施例1
一种高吸附性的滤清器滤纸,它是由下述重量份(公斤)的原料组成的:
针叶木浆120、聚四氟乙烯纤维14、氯化石蜡2、陶瓷粉3、轻质碳酸钙3、明矾粉2、1,4-环己烷二甲醇2、己二酸丙二醇聚酯2、磷酸二氢铵0.5、海藻酸钠3、乙撑基双硬脂酰胺1、二氧化铈0.5、松香12、丙烯酸丁酯4、纳米二氧化硅3、无水乙醇25、羧甲基纤维素钠1、过硫酸钠0.4、水适量;
一种高吸附性的滤清器滤纸的制备方法,包括以下步骤:
将针叶木浆、聚四氟乙烯纤维加入碎浆机中,先疏解15分钟,打浆,加入浆料2%的乙烯基三乙氧基硅烷、乙撑基双硬脂酰胺,充分搅拌,再加入陶瓷粉、轻质碳酸钙、明矾粉, 800转/分搅拌分散3分钟,得混合料;在上述混合料中加入除了松香、丙烯酸丁酯、纳米二氧化硅、无水乙醇、羧甲基纤维素钠、过硫酸钠以外的剩余各原料,加热至80℃,疏解、磨浆,加水至固含量为5%,由造纸机抄造成型,脱水;将松香加热熔解后,加入到无水乙醇中,搅拌分散,得分散液;将纳米二氧化硅分散到15倍水中,加入羧甲基纤维素钠、丙烯酸丁酯、过硫酸钠,在80℃下搅拌反应3小时,加入上述分散液,高速2000转/分分散4分钟,过滤出料,得浸渍液;将脱水后的纸浸于上述新型浸渍液中浸渍3h,再用压力辊除去过量的浸渍液;在200℃下恒温烘干,喷涂聚乙二醇400,所述聚乙二醇400的用量为纸张重量的2%,130℃下烘干至干度98%,压光整理,即得所述高吸附性的滤清器滤纸。
性能测试:
耐破度:328Kpa;
透气度:923L/m2 s;
气阻:0.80mbar。

Claims (2)

1.一种高吸附性的滤清器滤纸,其特征在于它是由下述重量份的原料组成的:
针叶木浆100-120、聚四氟乙烯纤维12-14、氯化石蜡2-3、陶瓷粉1-3、轻质碳酸钙1-3、明矾粉1-2、1,4-环己烷二甲醇1-2、己二酸丙二醇聚酯1-2、磷酸二氢铵0.3-0.5、海藻酸钠2-3、乙撑基双硬脂酰胺0.8-1、二氧化铈0.4-0.5、松香10-12、丙烯酸丁酯3-4、纳米二氧化硅3-5、无水乙醇20-25、羧甲基纤维素钠1-2、过硫酸钠0.2-0.4、水适量。
2.一种如权利要求1所述的高吸附性的滤清器滤纸的制备方法,其特征在于包括以下步骤:
将针叶木浆、聚四氟乙烯纤维加入碎浆机中,先疏解10-15分钟,打浆,加入浆料1-2%的乙烯基三乙氧基硅烷、乙撑基双硬脂酰胺,充分搅拌,再加入陶瓷粉、轻质碳酸钙、明矾粉,600-800转/分搅拌分散2-3分钟,得混合料;在上述混合料中加入除了松香、丙烯酸丁酯、纳米二氧化硅、无水乙醇、羧甲基纤维素钠、过硫酸钠以外的剩余各原料,加热至70-80℃,疏解、磨浆,加水至固含量为4-6%,由造纸机抄造成型,脱水;将松香加热熔解后,加入到无水乙醇中,搅拌分散,得分散液;将纳米二氧化硅分散到10-15倍水中,加入羧甲基纤维素钠、丙烯酸丁酯、过硫酸钠,在70-80℃下搅拌反应2-3小时,加入上述分散液,高速1600-2000转/分分散4-6分钟,过滤出料,得浸渍液;将脱水后的纸浸于上述新型浸渍液中浸渍2-3h,再用压力辊除去过量的浸渍液;在160-200℃下恒温烘干,喷涂聚乙二醇400,所述聚乙二醇400的用量为纸张重量的1-2%,120-130℃下烘干至干度95-98%,压光整理,即得所述高吸附性的滤清器滤纸。
CN2013102593806A 2013-06-26 2013-06-26 一种高吸附性的滤清器滤纸及其制备方法 Pending CN103382682A (zh)