CN103333646A - 一种环保低成本纸箱用胶粘剂及其制备方法 - Google Patents

一种环保低成本纸箱用胶粘剂及其制备方法 Download PDF

Info

Publication number
CN103333646A
CN103333646A CN2013102081723A CN201310208172A CN103333646A CN 103333646 A CN103333646 A CN 103333646A CN 2013102081723 A CN2013102081723 A CN 2013102081723A CN 201310208172 A CN201310208172 A CN 201310208172A CN 103333646 A CN103333646 A CN 103333646A
Authority
CN
China
Prior art keywords
starch
low
sodium
water
constitutive material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013102081723A
Other languages
English (en)
Inventor
王进
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI QIAITE ELECTRONIC TECHNOLOGY Co Ltd
Original Assignee
ANHUI QIAITE ELECTRONIC TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI QIAITE ELECTRONIC TECHNOLOGY Co Ltd filed Critical ANHUI QIAITE ELECTRONIC TECHNOLOGY Co Ltd
Priority to CN2013102081723A priority Critical patent/CN103333646A/zh
Publication of CN103333646A publication Critical patent/CN103333646A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种环保低成本纸箱用胶粘剂及其制备方法,其组成原料为:丙烯酸乳液、淀粉、钛白粉、硅酸钠、偏硅酸钠、柠檬酸钠、过硫酸铵、乙烯基三乙氧基硅烷、邻苯二甲酸酐、五氯酚钠、硬脂酸锌、羟基乙酸淀粉钠和水;本发明采用丙烯酸乳液和淀粉为主料,通过对淀粉的氧化处理,改善了淀粉的优良性能,增强了产品的粘结性,而且本发明环保无污染,制备方法简单,成本低,适合大规模生产。

Description

一种环保低成本纸箱用胶粘剂及其制备方法
技术领域
    本发明属于胶粘剂制备技术领域,具体涉及一种环保低成本纸箱用胶粘剂及其制备方法。
背景技术
目前,印刷行业的产品、材料很多,为了确保包装产品的质量,防止有毒物质、劣质包装产品的应用,必须把握好胶粘剂的使用,淀粉胶粘剂作为环境友好型天然胶粘剂越来越受到纸箱生产厂商的青睐,但是目前在纸箱生产行业所用的淀粉胶粘剂,主要是以淀粉、水、氢氧化钠、氧化剂等原材料制作而成,欠缺在于干燥速度慢、粘接强度低、耐水性差和储存性能不稳定等,从而在一定程度上限制了其在纸箱生产行业中的应用。
发明内容
本发明的目的在于提供一种环保低成本纸箱用胶粘剂及其制备方法。
本发明采用如下技术方案:
环保低成本纸箱用胶粘剂,其组成原料的重量份为:丙烯酸乳液65-70、淀粉8-12、钛白粉15-20、硅酸钠15-20、偏硅酸钠0.7-0.9、柠檬酸钠1.5-2.0、过硫酸铵1.1-1.3、乙烯基三乙氧基硅烷3.0-3.5、邻苯二甲酸酐18-22、五氯酚钠0.9-1.1、硬脂酸锌13-15、羟基乙酸淀粉钠3.0-4.0和水630-680。
环保低成本纸箱用胶粘剂,其组成原料的重量份为:丙烯酸乳液68、淀粉10、钛白粉18、硅酸钠18、偏硅酸钠0.8、柠檬酸钠1.8、过硫酸铵1.2、乙烯基三乙氧基硅烷3.2、邻苯二甲酸酐20、五氯酚钠1.0、硬脂酸锌14、羟基乙酸淀粉钠3.5和水650。
环保低成本纸箱用胶粘剂的制备方法,包括以下步骤:
(1)淀粉的处理:按组成原料的重量份称取淀粉加水糊化,然后加入相当于淀粉重量8-12%的硼酸,搅拌反应10-20min,再用3-5%的氢氧化钠溶液调节Ph至8-10,搅拌100-120min,即得;
(2)按组成原料的重量份称取各组成原料,先将上述步骤(1)处理后的淀粉、丙烯酸乳液和水混合,搅拌均匀,然后依次加入其它组成原料,再搅拌反应40-50min,得到。
本发明的有益效果:
本发明采用丙烯酸乳液和淀粉为主料,通过对淀粉的氧化处理,改善了淀粉的粘结性能,增强了产品的粘结性,而且本发明环保无污染,制备方法简单,成本低,适合大规模生产。
具体实施方式
实施例1:环保低成本纸箱用胶粘剂,其组成原料的重量份(斤)为:丙烯酸乳液68、淀粉10、钛白粉18、硅酸钠18、偏硅酸钠0.8、柠檬酸钠1.8、过硫酸铵1.2、乙烯基三乙氧基硅烷3.2、邻苯二甲酸酐20、五氯酚钠1.0、硬脂酸锌14、羟基乙酸淀粉钠3.5和水650。
环保低成本纸箱用胶粘剂的制备方法,包括以下步骤:
(1)淀粉的处理:按组成原料的重量份称取淀粉加水糊化,然后加入相当于淀粉重量8-12%的硼酸,搅拌反应10-20min,再用3-5%的氢氧化钠溶液调节Ph至8-10,搅拌100-120min,即得;
(2)按组成原料的重量份称取各组成原料,先将上述步骤(1)处理后的淀粉、丙烯酸乳液和水混合,搅拌均匀,然后依次加入其它组成原料,再搅拌反应45min,得到。
上述实施例1制得的胶粘剂用于纸箱经检测性能数据:
外观:乳白色;滴度:50-55滴/分钟;干燥时间15-17min;抗压强度:480-550Kgf;耐破强度:4750Kpa/10min;截穿强度:235Kgf.cm;耐水性:≥4.0h;成本:290元/吨。

Claims (3)

1.一种环保低成本纸箱用胶粘剂,其特征在于其组成原料的重量份为:丙烯酸乳液65-70、淀粉8-12、钛白粉15-20、硅酸钠15-20、偏硅酸钠0.7-0.9、柠檬酸钠1.5-2.0、过硫酸铵1.1-1.3、乙烯基三乙氧基硅烷3.0-3.5、邻苯二甲酸酐18-22、五氯酚钠0.9-1.1、硬脂酸锌13-15、羟基乙酸淀粉钠3.0-4.0和水630-680。
2.根据权利要求1所述的环保低成本纸箱用胶粘剂,其特征在于其组成原料的重量份为:丙烯酸乳液68、淀粉10、钛白粉18、硅酸钠18、偏硅酸钠0.8、柠檬酸钠1.8、过硫酸铵1.2、乙烯基三乙氧基硅烷3.2、邻苯二甲酸酐20、五氯酚钠1.0、硬脂酸锌14、羟基乙酸淀粉钠3.5和水650。
3.一种如权利要求1所述的环保低成本纸箱用胶粘剂的制备方法,其特征在于包括以下步骤:
(1)淀粉的处理:按组成原料的重量份称取淀粉加水糊化,然后加入相当于淀粉重量8-12%的硼酸,搅拌反应10-20min,再用3-5%的氢氧化钠溶液调节Ph至8-10,搅拌100-120min,即得;
(2)按组成原料的重量份称取各组成原料,先将上述步骤(1)处理后的淀粉、丙烯酸乳液和水混合,搅拌均匀,然后依次加入其它组成原料,再搅拌反应40-50min,得到。
CN2013102081723A 2013-05-30 2013-05-30 一种环保低成本纸箱用胶粘剂及其制备方法 Pending CN103333646A (zh)