CN103253060A - Method for manufacturing paper tire clamp paint storage device - Google Patents

Method for manufacturing paper tire clamp paint storage device Download PDF

Info

Publication number
CN103253060A
CN103253060A CN2013101586966A CN201310158696A CN103253060A CN 103253060 A CN103253060 A CN 103253060A CN 2013101586966 A CN2013101586966 A CN 2013101586966A CN 201310158696 A CN201310158696 A CN 201310158696A CN 103253060 A CN103253060 A CN 103253060A
Authority
CN
China
Prior art keywords
paper
lacquer
ash
drying
paint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2013101586966A
Other languages
Chinese (zh)
Other versions
CN103253060B (en
Inventor
王炳根
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Ningbo City College of Vocational Technology
Original Assignee
Ningbo City College of Vocational Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ningbo City College of Vocational Technology filed Critical Ningbo City College of Vocational Technology
Priority to CN201310158696.6A priority Critical patent/CN103253060B/en
Publication of CN103253060A publication Critical patent/CN103253060A/en
Application granted granted Critical
Publication of CN103253060B publication Critical patent/CN103253060B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a method for manufacturing a paper tire clamp paint storage device. The method comprises the following steps of: shaping a cellular board; pasting 10-20 layers of bark paper; coating hog blood ash for 2-3 times; coating a waterproof coating for 2-4 times to form a waterproof coating layer; flatly mounting ramin on the surface of the waterproof coating layer; smearing coarse paint ash on the surface of the ramin; smearing medium paint ash on the coarse paint ash; smearing fine paint ash on the medium paint ash; coating a layer of primer on the surface of the fine paint ash; performing decoration; feeding finish, after the finish is dried in the shade, polishing the surface by hongqi stone ink, then drying the finish again in the shade, and grinding and flattening the painted surface by sand paper, hairs and a shanju carbon tool sequentially; and after the paint is dried, performing friction on a product in a reciprocating manner by soaking a hand of a user with olive oil and young ash. The manufacturing method is low in manufacturing cost; and the manufactured product is large in size and has various shapes.

Description

The preparation method of paper tire folder Ramie lacquerware
Technical field
The present invention relates to the lacquerware technical field, specifically is a kind of preparation method of paper tire folder Ramie lacquerware.
Background technology
As one of representative of Chinese tratitional technology, lacquerware has its unique artistic charm and deep historical culture accumulation.The lacquerware of prior art is divided into tire lacquerware and bodiless lacquer, and it is tire with bamboo wood, pottery, metal that the tire lacquerware is wherein arranged; Bodiless lacquer is that raw material are made with earth, gypsum, wood then.There is following defective in above-mentioned two kinds of lacquerwares: 1, because the tire complex manufacturing technology of above-mentioned two kinds of lacquerwares, so its cost of manufacture is higher.2, because the bearing capacity of bodiless lacquer is little, poor stability and bending resistance are low, so it can only make undersized product.3, because the raw material that have the tire lacquerware to be impregnated limit, and the moulding of bodiless lacquer is limit by technology then, therefore the moulding of above-mentioned two kinds of lacquerwares is comparatively single.Therefore, for these reasons, demand urgently needing the preparation method that a kind of cost of manufacture is low, the making product size is big and paper tire various shapes presss from both sides the Ramie lacquerware, to address the above problem.
Summary of the invention
The technical problem to be solved in the present invention is, overcomes the defective of above prior art, and the preparation method that a kind of cost of manufacture is low, make the paper tire folder Ramie lacquerware of the big and various shapes of product size is provided.
Technical scheme of the present invention is, a kind of preparation method of paper tire folder Ramie lacquerware is provided, and may further comprise the steps:
A, cellular board is carried out moulding, make the paper loose tool;
B, at the lip-deep stick ground floor mulberry paper in the surface paper of paper loose tool of making of wood glue of paper loose tool, this step is repeated at ground floor mulberry paper paper second layer mulberry paper in back to be dried, papers 10~20 layers of mulberry paper;
C, treat above-mentioned last one deck mulberry paper drying after, spread upon the surface of last one deck mulberry paper equably with pig blood ash, treat to be coated with one deck pig blood ash again after the pig blood ash drying, repeat this step, apply 2~3 times;
D, wait to be coated in the pig blood ash drying on last one deck mulberry paper surface after, be coated with 2~4 road water-repellent paints on the surface of pig blood ash, constitute the water-repellent paint layer;
E, treat water-repellent paint layer drying after, with natural lacquer add flour as adhesive the flat surface of mounting at the water-repellent paint layer of ramie;
F, treat the ramie drying after, will coat with lacquer the cinder protective embankment earlier on the ramie surface and dry in the shade, wait to coat with lacquer the cinder drying after, polish flat with the sandstone wheel; Grey protective embankment after the grey drying, polishes flat with 600~800 purpose water mill sand in waiting to coat with lacquer coating with lacquer on the cinder and drying in the shade in will coating with lacquer then; To coat with lacquer thin grey protective embankment at last in lacquer on the ash and dry in the shade, wait to coat with lacquer thin grey drying after, polish flat with 100~400 purpose water mill sand;
G, be coated with one deck priming paint on the surface of the thin ash of lacquer;
H, on priming paint surface with mouse pen or writing brush instrument, be raw material with colored paint, gold and silver paper tinsel, decorate;
I, on through the surface of decorating on one finish paint, the back of drying in the shade is dipped in water with red auspicious stone and carried out pushing away light on the surface, and is smooth to coating with lacquer surface grinding with waterproof abrasive paper, hair, mountain beech carbon tool successively after drying in the shade again;
After j, the drying, the palm of personnel selection is stained with olive oil and young ash rubs back and forth.
The part by weight of described natural lacquer and flour is 8:2.
The part by weight of described lacquer cinder is: thick dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%; The part by weight of ash is in the described lacquer: middle dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%; The part by weight of the thin ash of described lacquer is: thin dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%.
The part by weight of described olive oil and children's ash is 10:1.
After adopting above method, the present invention compared with prior art has the following advantages:
1, paper tire folder Ramie lacquerware of the present invention is that raw material are made with the cellular board, by to cellular board folding, shear, making that splicing can be finished tire, this manufacture craft is with respect to the tire that tire lacquerware and bodiless lacquer are arranged, and its manufacture craft is very simple, so its cost of manufacture is low.2, because paper tire of the present invention folder Ramie lacquerware is raw material with the cellular board, utilize that the high strength string of the high strength of corrugated structure, mulberry paper of cellular board inside and ramie inside forms that a bearing capacity is big, good stability and the strong papery idiosome of bending resistance, so the present invention can make large-sized product (can reach more than 6 meters).3, because paper tire of the present invention folder Ramie lacquerware is raw material with paper, it is convenient to fold, shearing, bonding making various moulding, so the various shapes of the paper tire folder Ramie lacquerware made of the present invention.
The specific embodiment
The invention will be further described below in conjunction with the drawings and specific embodiments.
The preparation method of a kind of paper tire folder of the present invention Ramie lacquerware may further comprise the steps:
A, cellular board is carried out moulding, make the paper loose tool; Moulding namely is made into the product with definite shape with cellular board, as the stool of making a Tea Service and matching and use with Tea Service, all can be by folding, the shearing of cellular board, the bonding paper loose tool of making, because the structure of paper loose tool is different, therefore its preparation method is also different, so do not described in detail at this.
B, at the lip-deep stick ground floor mulberry paper in the surface paper of paper loose tool of making of wood glue of paper loose tool, this step is repeated at ground floor mulberry paper paper second layer mulberry paper in back to be dried, papers 10~20 layers of mulberry paper; Namely paper ground floor mulberry paper on paper loose tool surface, treat to paper second layer mulberry paper at ground floor mulberry paper after the wood glue drying, treat to paper the 3rd layer of mulberry paper at second layer mulberry paper again after the wood glue drying, repeat this step, until 10~20 layers of mulberry paper of paper, paper 10 layers of mulberry paper in the present embodiment and get final product.
C, treat above-mentioned last one deck mulberry paper drying after, spread upon the surface of last one deck mulberry paper equably with pig blood ash, treat to be coated with one deck pig blood ash again after the pig blood ash drying, repeat this step, apply 2~3 times; Above-mentioned last one deck mulberry paper the 10th layer of mulberry paper just in the present embodiment; Spread upon the surface of last one deck mulberry paper equably with pig blood ash, treat that the dry back of pig blood ash is coated with one deck pig blood ash again on the pig blood ash of drying, treat that the dry back of pig blood ash that is coated with for the second time is coated with one deck pig blood ash again on the pig blood ash that is coated with for the second time, be coated with three times altogether and get final product.
D, wait to be coated in the pig blood ash drying on last one deck mulberry paper surface after, be coated with 2~4 road water-repellent paints on the surface of pig blood ash, constitute the water-repellent paint layer; Water-repellent paint buy on the market again to polyurethane water-proof paint.
E, treat water-repellent paint layer drying after, with natural lacquer add flour as adhesive the flat surface of mounting at the water-repellent paint layer of ramie; Flat mounting namely launched ramie and is tiled in the water-repellent paint laminar surface and papers.
F, treat the ramie drying after, will coat with lacquer the cinder protective embankment earlier on the ramie surface and dry in the shade, wait to coat with lacquer the cinder drying after, polish flat with the sandstone wheel; Grey protective embankment after the grey drying, polishes flat with 600~800 purpose water mill sand in waiting to coat with lacquer coating with lacquer on the cinder and drying in the shade in will coating with lacquer then; To coat with lacquer thin grey protective embankment at last in lacquer on the ash and dry in the shade, wait to coat with lacquer thin grey drying after, polish flat with 100~400 purpose water mill sand; Protective embankment is namely smeared implements with lacquer and ash.Water mill sand is ink sand paper.
G, be coated with one deck priming paint on the surface of the thin ash of lacquer; Be generally black primer.
H, on priming paint surface with mouse pen or writing brush instrument, be raw material with colored paint, gold and silver paper tinsel, decorate; Decorate namely with mouse pen or writing brush instrument with colored paint gold and silver paper tinsel draw various patterns and font etc.
I, on through the surface of decorating on one finish paint, the back of drying in the shade is dipped in water with red auspicious stone and carried out pushing away light on the surface, and is smooth to coating with lacquer surface grinding with waterproof abrasive paper, hair, mountain beech carbon tool successively after drying in the shade again; Pushing away light is the mill of finish paint, the general name of wiping, pushing away.
After j, the drying, the palm of personnel selection is stained with olive oil and young ash rubs back and forth.Children's ash is thin ash to be gone into a barrel water mixing stir evenly post precipitation and anhydrate, after with shovel the thin dark grey taking-up of the superiors being dried, i.e. and very fine and smooth brick and tile ash.
The part by weight of described natural lacquer and flour is 8:2.
The part by weight of described lacquer cinder is: thick dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%; The part by weight of ash is in the described lacquer: middle dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%; The part by weight of the thin ash of described lacquer is: thin dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%.
The part by weight of described olive oil and children's ash is 10:1.
Below only be described with regard to most preferred embodiment of the present invention, but can not be interpreted as it is limitations on claims.The present invention is not limited only to above embodiment, and its concrete structure allows to change.All various variations of doing in the protection domain of independent claims of the present invention are all in protection scope of the present invention.

Claims (4)

1. the preparation method of paper tire folder Ramie lacquerware is characterized in that: may further comprise the steps:
A, cellular board is carried out moulding, make the paper loose tool;
B, at the lip-deep stick ground floor mulberry paper in the surface paper of paper loose tool of making of wood glue of paper loose tool, this step is repeated at ground floor mulberry paper paper second layer mulberry paper in back to be dried, papers 10~20 layers of mulberry paper;
C, treat above-mentioned last one deck mulberry paper drying after, spread upon the surface of last one deck mulberry paper equably with pig blood ash, treat to be coated with one deck pig blood ash again after the pig blood ash drying, repeat this step, apply 2~3 times;
D, wait to be coated in the pig blood ash drying on last one deck mulberry paper surface after, be coated with 2~4 road water-repellent paints on the surface of pig blood ash, constitute the water-repellent paint layer;
E, treat water-repellent paint layer drying after, with natural lacquer add flour as adhesive the flat surface of mounting at the water-repellent paint layer of ramie;
F, treat the ramie drying after, will coat with lacquer the cinder protective embankment earlier on the ramie surface and dry in the shade, wait to coat with lacquer the cinder drying after, polish flat with the sandstone wheel; Grey protective embankment after the grey drying, polishes flat with 600~800 purpose water mill sand in waiting to coat with lacquer coating with lacquer on the cinder and drying in the shade in will coating with lacquer then; To coat with lacquer thin grey protective embankment at last in lacquer on the ash and dry in the shade, wait to coat with lacquer thin grey drying after, polish flat with 100~400 purpose water mill sand;
G, be coated with one deck priming paint on the surface of the thin ash of lacquer;
H, on priming paint surface with mouse pen or writing brush instrument, be raw material with colored paint, gold and silver paper tinsel, decorate;
I, on through the surface of decorating on one finish paint, the back of drying in the shade is dipped in water with red auspicious stone and carried out pushing away light on the surface, and is smooth to coating with lacquer surface grinding with waterproof abrasive paper, hair, mountain beech carbon tool successively after drying in the shade again;
After j, the drying, the palm of personnel selection is stained with olive oil and young ash rubs back and forth.
2. according to the preparation method of the described paper tire folder of claim 1 Ramie lacquerware, it is characterized in that: the part by weight of described natural lacquer and flour is 8:2.
3. according to the preparation method of the described paper tire folder of claim 1 Ramie lacquerware, it is characterized in that: the part by weight of described lacquer cinder is: thick dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%; The part by weight of ash is in the described lacquer: middle dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%; The part by weight of the thin ash of described lacquer is: thin dark grey 50%, natural lacquer 30%, lithopone 10%, diluent 10%.
4. according to the preparation method of the described paper tire folder of claim 1 Ramie lacquerware, it is characterized in that: the part by weight of described olive oil and children's ash is 10:1.
CN201310158696.6A 2013-04-28 2013-04-28 Method for manufacturing paper tire clamp paint storage device Expired - Fee Related CN103253060B (en)