CN103234089A - 一种钢衬聚四氟乙烯取样环及其制作工艺 - Google Patents
一种钢衬聚四氟乙烯取样环及其制作工艺 Download PDFInfo
- Publication number
- CN103234089A CN103234089A CN2013101407862A CN201310140786A CN103234089A CN 103234089 A CN103234089 A CN 103234089A CN 2013101407862 A CN2013101407862 A CN 2013101407862A CN 201310140786 A CN201310140786 A CN 201310140786A CN 103234089 A CN103234089 A CN 103234089A
- Authority
- CN
- China
- Prior art keywords
- arm
- overcoat
- charge
- person
- steel lining
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种钢衬聚四氟乙烯取样环及其制作工艺,主管内衬材料可以是相同规格管材使用后多余的部分,也可以是根据长度需要而焊接成型的管材,是在主管与支管之间采用锥形配合进行密封的新型工艺,利用本技术生产的取样环具有结构简单、加工方便、成本较低等特性,极大地提高了生产效率和产品一次合格率。
Description
技术领域
本发明涉及一种取样环及其制作工艺,尤其是一种钢衬聚四氟乙烯取样环及其制作工艺。
背景技术
对于口径在DN400以上的钢衬聚四氟乙烯取样环,传统的工艺是采用模压法制作,需要经过填粉、模压、烧结等流程,制品在制作过程中由于设计不合理、钢件制作的尺寸偏差、填粉不均匀等原因而造成制品的合格率也不高,材料浪费多,生产效率较低,增加企业了生产成本。
发明内容
本发明的目的是改变传统的钢衬聚四氟乙烯取样环的制作工艺的工艺复杂、合格率不高的弊端,提供一种结构和加工工艺简单方便、合格率高、成本低的钢衬聚四氟乙烯取样环及其制作工艺,本发明的技术方案是如此实现的:
一种钢衬聚四氟乙烯取样环,包括主管和支管,主管和支管内侧分别设有主管内衬和支管内衬,支管外侧设有支管外套,支管和支管外套的近主管一端均为扩口端,所述支管的顶部设有支管法兰,所述法兰与支管外套顶部之间设有锁紧螺母。
一种钢衬聚四氟乙烯取样环的制作工艺,其特征在于包括以下步骤:
A.根据尺寸要求,将支管外套焊接在主管相应位置上;
B.将搭接成管状的聚四氟乙烯板材放入主管内,在支管位置的中心开一孔,孔的直径比支管外套的内径小20~40mm,并加热扩口,扩口后的锥度与支管外套扩口处一致;
C.将相应规格的聚四氟乙烯管衬入支管内,在扩口端翻边,外包长度为20~40mm,并进行修整;
D.将翻边后的支管从主管内部插入支管外套内,用锁紧螺母将支管拧紧;
E.用10~12kv电火花检测主管和支管的连接处,无击穿现象为合格。
作为优选,支管外套与支管配合处的锥度保持一致,支管外套的内径比支管的外径大0.5~2mm。
作为优选,所述聚四氟乙烯管板材的密度为2.1~2.2g/cm3,厚度为3~4mm。
本发明设计的钢衬聚四氟乙烯取样环及其制作工艺,主管内衬材料可以是相同规格管材使用后多余的部分,也可以是根据长度需要而焊接成型的管材,是在主管与支管之间采用锥形配合进行密封的新型工艺,利用本技术生产的取样环具有结构简单、加工方便、成本较低等特性,极大地提高了生产效率和产品一次合格率。
附图说明
附图是本发明的一种结构示意图。
具体实施方式
下面通过实施例,对本发明的技术方案作进一步具体的说明。
实施例:参考附图,一种钢衬聚四氟乙烯取样环,包括主管6和支管4,主管6和支管4内侧分别设有主管内衬7和支管内衬1,支管4外侧设有支管外套5,支管4和支管外套5的近主管6一端均为扩口端,所述支管4的顶部设有支管法兰2,所述法兰2与支管外套5顶部之间设有锁紧螺母3。
加工工艺过程包括以下几个步骤:
A、根据尺寸要求,将支管外套5焊接在取样环主管6的相应位置上;
B、将由密度为2.1g/cm3、厚度为3mm的聚四氟乙烯板搭接而成的取样环主管内衬7衬入主管6内,在支管4位置的中心处开一小孔,孔的直径比支管外套5的内径小30mm,并加热扩口,扩口后的锥度与支管外套5扩口处一致;
C、将相应规格的聚四氟乙烯管衬入支管4内,在扩口端翻边,外包长度为30mm,并进行修整;
D、将翻边后的支管4从取样环主管6内部插入支管外套5内,用锁紧螺母3将支管4拧紧;
E、用10kv电火花检测取样环主管6和支管4的连接处,无击穿现象为合格,然后在支管4上装上支管法兰2,在取样环主管6和支管4的密封面处翻边。
Claims (4)
1.一种钢衬聚四氟乙烯取样环,包括主管(6)和支管(4),其特征在于主管(6)和支管(4)内侧分别设有主管内衬(7)和支管内衬(1),支管(4)外侧设有支管外套(5),支管(4)和支管外套(5)的近主管(6)一端均为扩口端,所述支管(4)的顶部设有支管法兰(2),所述法兰(2)与支管外套(5)顶部之间设有锁紧螺母(3)。
2.一种钢衬聚四氟乙烯取样环的制作工艺,其特征在于包括以下步骤:
A.根据尺寸要求,将支管外套(5)焊接在主管(6)相应位置上;
B.将搭接成管状的聚四氟乙烯板材放入主管(6)内,在支管(4)位置的中心开一孔,孔的直径比支管外套(5)的内径小20~40mm,并加热扩口,扩口后的锥度与支管外套(5)扩口处一致;
C.将相应规格的聚四氟乙烯管衬入支管(4)内,在扩口端翻边,外包长度为20~40mm,并进行修整;
D.将翻边后的支管(4)从主管(6)内部插入支管外套(5)内,用锁紧螺母(3)将支管(4)拧紧;
E.用10~12kv电火花检测主管(6)和支管(4)的连接处,无击穿现象为合格。
3.根据权利要求1所述的一种钢衬聚四氟乙烯取样环,其特征在于支管外套(5)与支管(4)配合处的锥度保持一致,支管外套(5)的内径比支管(4)的外径大0.5~2mm。
4.根据权利要求2所述的一种钢衬聚四氟乙烯取样环的制作工艺,其特征在于所述聚四氟乙烯管板材的密度为2.1~2.2g/cm3,厚度为3~4mm。