CN103144175A CN 201110400329 CN201110400329A CN103144175A CN 103144175 A CN103144175 A CN 103144175A CN 201110400329 CN201110400329 CN 201110400329 CN 201110400329 A CN201110400329 A CN 201110400329A CN 103144175 A CN103144175 A CN 103144175A
Authority
CN
China
Prior art keywords
poplar
eucalyptus
veneer
lvl
enzyme
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201110400329
Other languages
English (en)
Inventor
朱捷
李绍成
朱典想
孙献娥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nanjing Forestry University
Original Assignee
Nanjing Forestry University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanjing Forestry University filed Critical Nanjing Forestry University
Priority to CN 201110400329 priority Critical patent/CN103144175A/zh
Publication of CN103144175A publication Critical patent/CN103144175A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Chemical And Physical Treatments For Wood And The Like (AREA)
  • Manufacture Of Wood Veneers (AREA)

Abstract

为了充分利用杨木、桉木速生材资源,降低木质楼梯扶手的生产成本,本发明提供了杨-桉LVL楼梯扶手的生产工艺方法:分别将杨木、桉木旋切成3mm以上的单板;对单板进行酶处理;对酶处理后的单板进行干燥处理,含水率控制在10~12%;将单板进行涂胶组坯;热压处理:热压的压力为1.2MPa左右,温度为100-150℃,时间按1min/mm进行控制;多片锯制条;仿形铣削;抛光及装配。

Description

杨-桉LVL楼梯扶手的生产方法
一、所属技术领域
本发明公开了一种杨-桉单板层积材楼梯扶手的生产方法,主要包括杨-桉单板层积材的制造方法,以及基于杨-桉单板层积材的楼梯扶手生产方法,属于木制品制造领域。
二、背景技术
随着生活水平的提高,人们对家居环境的要求越来越高,环保意识越来越强,对基于木质的楼梯扶手需求量越来越大。现有的木质楼梯扶手主要是由珍贵木材经过铣削加工而成的,浪费了大量的优质珍贵木材。随着木材资源的逐渐减少,生产这种木质楼梯扶手的成本越来越高。我国速生杨木、桉木资源非常丰富,利用杨木、桉木单板制作的层积材(Laminated Veneer Lumber,LVL),即杨-桉LVL,属于功能材料,其稳定性能优于实体木材,具有强度变异性小、许用应力高、尺寸稳定性好等优点。对杨-桉LVL进行仿形铣削加工得到的楼梯扶手不仅具有珍贵木材的纹理,装饰性好,立体感强,保留了天然木材的自然属性等优点,同时采用的是速生材,不需要珍贵木材,这对保护我国森林资源和生态环境具有十分重要的现实意义。因此,杨-桉LVL楼梯扶手在国内外市场具有较大的竞争力。
三、发明内容
1发明目的
利用杨-桉LVL生产楼梯扶手,一方面发挥杨-桉LVL楼梯扶手的优点,即具有珍贵木材的纹理,装饰性奸,立体感强,保留了天然木材的自然属性等优点;另一方面,有利于保护珍贵木材资源,有利于降低楼梯扶手的成本,从而提高其在国内外市场的竞争力。
2技术方案
1)分别将杨木、桉木旋切成3mm以上的单板;
2)对单板进行酶处理;
3)对酶处理后的单板进行干燥处理,含水率控制在10~12%;
4)将单板进行涂胶组坯;
5)热压处理:热压的压力为1.2MPa左右,温度为100~150℃,时间按1min/mm进行控制;
6)多片锯制条;
7)仿形铣削;
8)抛光及装配。
四、具体实施方式
杨-桉LVL楼梯扶手的生产过程如下:
1)分别将杨木、桉木旋切成3mm以上的单板;
2)对单板进行酶处理;
在酶处理工艺中,酶处理温度过高,酶活迅速减小,而温度低,酶的水解催化速度降低,因此,水浴温度保持50℃。
随着酶处理时间的增加,单板的力学性能及表面润湿性能均会增加,但是纤维素中糖苷键的断裂,可能引起力学性能及表面润湿性能的下降,因此,酶处理时间不宜过长。在一定范围内,酶用量的增加,对杨木表面性能的提高有利,但超过一定范围后,改性效果不再显著,且力学性能有可能下降。考虑到成本等因素,确定酶处理时间为6h,酶的添加量为1mL/g。
3)对酶处理后的单板进行干燥处理,含水率控制在10~12%;
4)将单板进行涂胶组坯;
5)通过热压处理形成板坯,热压的压力为1.2MPa左右,温度为100~150℃,时间按1min/mm进行控制;
6)采用多片锯对板坯进行制条,保证等宽等厚;
7)仿形铣削,用木工仿形铣床进行加工;
8)抛光及装配,用砂带抛光机进行抛光。

Claims (2)

1.一种杨-桉LVL楼梯扶手的生产方法,其特征在于该方法包括以下内容:分别将杨木、桉木旋切成3mm以上的单板;对单板进行酶处理;对酶处理后的单板进行干燥处理,含水率控制在10~12%;将单板进行涂胶组坯;热压处理:热压的压力为1.2MPa左右,温度为100~150℃,时间按1min/mm进行控制;多片锯制条;仿形铣削;抛光及装配。
2.根据权利要求1所述的对单板进行酶处理方法,其特征是:在酶处理工艺中,酶处理温度为50℃,处理时间为6h,酶的添加量为1mL/g。
CN 201110400329 2011-12-06 2011-12-06 杨-桉lvl楼梯扶手的生产方法 Pending CN103144175A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201110400329 CN103144175A (zh) 2011-12-06 2011-12-06 杨-桉lvl楼梯扶手的生产方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201110400329 CN103144175A (zh) 2011-12-06 2011-12-06 杨-桉lvl楼梯扶手的生产方法

Publications (1)

Publication Number Publication Date
CN103144175A true CN103144175A (zh) 2013-06-12

Family

ID=48542634

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201110400329 Pending CN103144175A (zh) 2011-12-06 2011-12-06 杨-桉lvl楼梯扶手的生产方法

Country Status (1)

Country Link
CN (1) CN103144175A (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109732712A (zh) * 2019-02-27 2019-05-10 福建顺景机械工业有限公司 一种木质扶手板材拼接板材及扶手生产工艺

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109732712A (zh) * 2019-02-27 2019-05-10 福建顺景机械工业有限公司 一种木质扶手板材拼接板材及扶手生产工艺
CN109732712B (zh) * 2019-02-27 2021-08-31 福建顺景机械工业有限公司 一种木质扶手板材拼接板材及扶手生产工艺

Similar Documents

Publication Publication Date Title
CN101698311B (zh) 一种指接细木工板的生产工艺
EP2255937B1 (en) Manufacturing method for a surface-strengthened solid wood floor board
CN101357470B (zh) 一种重组木及其制造方法
CN101863058B (zh) 一种新型集成材及其制作方法
CN102107452B (zh) 一种软木实木地板及其制造方法
CN104626292A (zh) 一种可饰面定向刨花板及其制备工艺
CN101524859B (zh) 一种用超厚单板制造的实木复合板材及其制造方法
CN102398287A (zh) 一种竹木复合板生产方法
CN101544008A (zh) 一种木竹复合地板的制作方法
CN201385341Y (zh) 一种用超厚旋切单板制造的实木复合板材
CN105058520A (zh) 一种桉木胶合扇叶板及其制造方法
CN101712170A (zh) 机电包装用高强单板层积材的制造方法
CN110341009A (zh) 一种无甲醛释放的浸渍胶膜纸饰面细木工板及其生产工艺
CN102554992B (zh) 一种表面增强型木材型材及其制造方法
CN101293370A (zh) 一种重组单板面复合地板的生产方法
CN103448127A (zh) 一种装饰用单板层积板材的生产方法
CN105108877A (zh) 一种重组木制造方法
CN109434975A (zh) 综合速生材材质特征及建筑结构需求的正交胶合木及其制备方法
CN102431065A (zh) 一种直纹单板层积材、加工方法及其应用
CN103144175A (zh) 杨-桉lvl楼梯扶手的生产方法
CN209665647U (zh) 综合速生材材质特征及建筑结构需求的正交胶合木
CN101284593A (zh) 人造木饰面集装箱地板及其生产工艺
CN104890088A (zh) 一种实木复合地板生产工艺
CN204894127U (zh) 一种桉木胶合扇叶板
CN204266540U (zh) 一种柳杉三层实木复合地板

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C05 Deemed withdrawal (patent law before 1993)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20130612