CN103115220A - 一种3pe防腐钢管法兰连接方法 - Google Patents
一种3pe防腐钢管法兰连接方法 Download PDFInfo
- Publication number
- CN103115220A CN103115220A CN2013100514725A CN201310051472A CN103115220A CN 103115220 A CN103115220 A CN 103115220A CN 2013100514725 A CN2013100514725 A CN 2013100514725A CN 201310051472 A CN201310051472 A CN 201310051472A CN 103115220 A CN103115220 A CN 103115220A
- Authority
- CN
- China
- Prior art keywords
- flanges
- flange
- steel pipe
- iron
- steel tube
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种3PE防腐钢管法兰连接方法,包括以下步骤:(1)在3PE防腐钢管一端焊接铁法兰,焊接完毕后在铁法兰表面喷上环氧树脂修补漆,用螺栓将两个焊接在钢管上的铁法兰连接紧固在一起;(2)从3PE防腐钢管另一端套入PE法兰,将PE法兰贴紧连接好的铁法兰,并用大约3cm热收缩带贴紧PE法兰缠绕在3PE防腐钢管上,加热热收缩带,使其径向收缩贴紧3PE防腐钢管;(3)在两个PE法兰与铁法兰中间的缝隙中灌满聚氨酯;(4)用热收缩带完全缠绕两PE法兰,中间不能出现裸露,加热热收缩带,使其径向收缩完全覆盖、贴紧PE法兰。有益效果:本发明设计合理,施工、维修方便,连接牢固稳定性好,外防腐性能好,解决了3PE防腐钢管用法兰连接的外防腐技术问题。
Description
技术领域
本发明涉及一种3PE防腐钢管法兰连接方法。
背景技术
由于3PE防腐钢管具有极高的密封性,良好的耐腐蚀和耐冲击性,抗介质渗透性强,有很高的防腐可靠性,使用寿命长等优点,广泛使用于热网供热、排水、燃气、石油输送、化工、污水排放、生物池防腐工程、印染等行业输送腐蚀性介质等,在使用过程中3PE防腐钢管的连接方法,通常采用焊接或活动接扣的方式,但是焊接方式存在施工难度大、拆卸不方便,活动接扣方式存在连接不牢固、密封性差等缺点,目前国内3PE防腐钢管的连接方式尚未出现法兰连接,主要是法兰连接的外防腐技术不成熟。
发明内容:
木发明的目的是针对现有技术的不足,提供一种设计合理,安装、维修方便,连接牢固稳定性强,外防腐性良好的3PE防腐钢管法兰连接方法。
本发明是通过以下技术方案实现的:一种3PE防腐钢管法兰连接方法,其特征在于:包括以下步骤:
(1)、在3PE防腐钢管一端焊接铁法兰,焊接完毕后在铁法兰表面喷上环氧树脂修补漆,用螺栓将两个焊接在钢管上的铁法兰连接紧固在一起;
(2)、从3PE防腐钢管另一端套入PE法兰,将PE法兰贴紧连接好的铁法兰,并用大约3cm热收缩带贴紧PE法兰缠绕在3PE防腐钢管上,加热热收缩带,使其径向收缩贴紧3PE防腐钢管;
(3)、在两个PE法兰与铁法兰中间的缝隙中灌满聚氨酯;
(4)、用热收缩带完全缠绕两PE法兰,中间不能出现裸露,加热热收缩带,使其径向收缩完全覆盖、贴紧PE法兰。
有益效果:本发明设计合理,施工、维修方便,连接牢固稳定性好,外防腐性能好,解决了3PE防腐钢管用法兰连接的外防腐技术问题。
附图说明
附图1、2、3为本发明的示意图。
图1、2、3中:1、3PE防腐钢管,2、铁法兰,3、PE法兰,4、PE法兰与铁法兰中间缝隙,5、热收缩带,6、热收缩带。
具体实施方式
下面结合具体实施例对本发明进一步说明。
如图1、2、3所示的实施例,一种3PE防腐钢管法兰连接方法;在3PE防腐钢管1一端焊接铁法兰2,焊接完毕后在铁法兰2表面喷上环氧树脂修补漆,用螺栓将两个焊接在钢管上的铁法兰2连接紧固在一起,从3PE防腐钢管1另一端套入PE法兰3,将PE法兰3贴紧连接好的铁法兰2,并用大约3cm热收缩带5贴紧PE法兰3缠绕在3PE防腐钢管1上,加热热收缩带5,使其径向收缩贴紧3PE防腐钢管1,在两个PE法兰与铁法兰中间的缝隙4中灌满聚氨酯,用热收缩带6完全缠绕两PE法兰3,中间不能出现裸露,加热热收缩带6,使其径向收缩完全覆盖、贴紧PE法兰3。
Claims (1)
1.一种3PE防腐钢管法兰连接方法,其特征在于:包括以下步骤:
(1)、在3PE防腐钢管一端焊接铁法兰,焊接完毕后在铁法兰表面喷上环氧树脂修补漆,用螺栓将两个焊接在钢管上的铁法兰连接紧固在一起;
(2)、从3PE防腐钢管另一端套入PE法兰,将PE法兰贴紧连接好的铁法兰,并用大约3cm热收缩带贴紧PE法兰缠绕在3PE防腐钢管上,加热热收缩带,使其径向收缩贴紧3PE防腐钢管;
(3)、在两个PE法兰与铁法兰中间的缝隙中灌满聚氨酯;
(4)、用热收缩带完全缠绕两PE法兰,中间不能出现裸露,加热热收缩带,使其径向收缩完全覆盖、贴紧PE法兰。