CN103114354A - 纯棉舒化技术 - Google Patents
纯棉舒化技术 Download PDFInfo
- Publication number
- CN103114354A CN103114354A CN2013100565638A CN201310056563A CN103114354A CN 103114354 A CN103114354 A CN 103114354A CN 2013100565638 A CN2013100565638 A CN 2013100565638A CN 201310056563 A CN201310056563 A CN 201310056563A CN 103114354 A CN103114354 A CN 103114354A
- Authority
- CN
- China
- Prior art keywords
- cotton
- fiber
- technology
- bat
- gentle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
纯棉舒化技术,涉及纺织技术领域,该技术采用柔压分离技术将皮棉中杂质与棉花长纤维分离;采用柔舒膨松技术对棉纤维梳理,提高棉纤维蓬松度,使其中短纤维和杂质脱落;采用柔铺舒芯技术使棉纤维交错均匀摊铺,并呈S形回环分布。本发明通过柔压分离、柔舒膨松和柔铺舒芯三大技术彻底地将皮棉中的杂质与棉花长纤维分离,棉纤维的蓬松度高,棉胎纤维交错均匀分布,呈S形回环形态,大大提高了棉胎纤维的回弹力,增强了棉胎的透气性,可水洗,不板结,保暖效果优良。
Description
技术领域
本发明涉及纺织技术领域,具体涉及一种纯棉舒化生产棉胎技术。
背景技术
棉胎就是棉被的芯,是棉花弹松铺开后用线包裹固定成被子的里子,现有的棉胎通常是采用皮棉经清杂、弹松、梳理、成型以及摊铺网纱而制成,具有保暖性好,吸湿性强的特点。但是目前棉胎的加工工艺不能有效地将皮棉中的棉籽、短纤维以及断纤维与长纤维分离,而且棉纤维的蓬松度比较差,同时现有技术加工的棉胎纤维大多为顺直分布,回弹力弱,吸湿后几乎失去回弹力,加之里面杂质分离不彻底,里面的水分得不到及时挥发会造成棉胎板结,最终导致棉胎失去保温效果,因此目前的面胎大多不能进行水洗。
发明内容
本发明提供了一种纯棉舒化技术,以解决现有技术存在的杂质分离不彻底、纤维蓬松度差以及回弹力差的问题。
本发明解决其技术问题所采用的技术方案是采用柔压分离技术将皮棉中杂质与棉花长纤维分离;采用柔舒膨松技术对棉纤维梳理,提高棉纤维蓬松度,使其中短纤维和杂质脱落;采用柔铺舒芯技术使棉纤维交错均匀摊铺,并呈S形回环分布,其具体步骤如下:
1、柔压分离:将皮棉放入圆盘自动抓棉机内并铺放均匀,通过圆盘自动抓棉机对皮棉进行开松混合,得到棉胎粗坯,然后依次启动第一凝棉器、清花机、混开棉机、第二凝棉器以及豪猪开棉机分离棉胎粗坯中的棉籽、短纤维以及断纤维杂质,从而得到棉胎纤维,棉胎纤维进入若干集棉箱中;
2、柔舒膨松:通过梳棉机对集棉箱内的棉胎纤维进行开松分梳,使所有呈卷曲块状的棉圈成为基本伸直的单纤维状态,并进一步清除棉胎纤维中的杂质;
3、柔铺舒芯:将梳棉机送来的平直棉纤维通过铺网机进行均匀折叠,先启动输送帘,再启动补偿帘、铺网帘以及成网帘,使棉纤维交错均匀摊铺,并呈S形回环分布,铺设至所需的宽度及厚度,从而得到棉胎。
上述柔铺舒芯工序中铺网机的输送帘、补偿帘、铺网帘的线速度相同。
与现有技术相比,本发明的有益效果是通过柔压分离、柔舒膨松和柔铺舒芯三大技术彻底地将皮棉中的杂质与棉花长纤维分离,棉纤维的蓬松度高,棉胎纤维交错均匀分布,呈S形回环形态,大大提高了棉胎纤维的回弹力,增强了棉胎的透气性,可水洗,不板结,保暖效果优良。
具体实施方式
一种纯棉舒化技术,采用柔压分离技术将皮棉中杂质与棉花长纤维分离;采用柔舒膨松技术对棉纤维梳理,提高棉纤维蓬松度,使其中短纤维和杂质脱落;采用柔铺舒芯技术使棉纤维交错均匀摊铺,并呈S形回环分布,其具体步骤如下:
1、柔压分离:采用高品质种子棉作为原料,将皮棉放入圆盘自动抓棉机内并铺放均匀,并检查房子铁丝等金属杂质带进抓棉机,通过圆盘自动抓棉机对皮棉进行开松混合,得到棉胎粗坯,然后依次启动第一凝棉器、清花机、混开棉机、第二凝棉器以及豪猪开棉机分离棉胎粗坯中的棉籽、短纤维以及断纤维杂质,从而得到棉胎纤维,棉胎纤维进入若干集棉箱中;
2、柔舒膨松:通过梳棉机对集棉箱内的棉胎纤维进行开松分梳,先启动锡林,再启动道夫,运转正常后,再向梳棉机中投料,使所有呈卷曲块状的棉圈成为基本伸直的单纤维状态,并进一步清除棉胎纤维中的杂质;
3、柔铺舒芯:将梳棉机送来的平直棉纤维通过铺网机进行均匀折叠,先检查铺网帘是否缠棉,有无堵塞,链条减速电机是否松动,光电系统是否正常,如无异常,先启动输送帘,再启动补偿帘、铺网帘以及成网帘,输送帘、补偿帘、铺网帘的线速度相同,使棉纤维交错均匀摊铺,并呈S形回环分布,铺设至所需的宽度及厚度,从而得到棉胎。
Claims (2)
1.一种纯棉舒化技术,其特征是采用柔压分离技术将皮棉中杂质与棉花长纤维分离;采用柔舒膨松技术对棉纤维梳理,提高棉纤维蓬松度,使其中短纤维和杂质脱落;采用柔铺舒芯技术使棉纤维交错均匀摊铺,并呈S形回环分布,其具体步骤如下:
(1)柔压分离:将皮棉放入圆盘自动抓棉机内并铺放均匀,通过圆盘自动抓棉机对皮棉进行开松混合,得到棉胎粗坯,然后依次启动第一凝棉器、清花机、混开棉机、第二凝棉器以及豪猪开棉机分离棉胎粗坯中的棉籽、短纤维以及断纤维杂质,从而得到棉胎纤维,棉胎纤维进入若干集棉箱中;
(2)柔舒膨松:通过梳棉机对集棉箱内的棉胎纤维进行开松分梳,使所有呈卷曲块状的棉圈成为基本伸直的单纤维状态,并进一步清除棉胎纤维中的杂质;
(3)柔铺舒芯:将梳棉机送来的平直棉纤维通过铺网机进行均匀折叠,先启动输送帘,再启动补偿帘、铺网帘以及成网帘,使棉纤维交错均匀摊铺,并呈S形回环分布,铺设至所需的宽度及厚度,从而得到棉胎。
2.根据权利要求1所述的纯棉舒化技术,其特征是柔铺舒芯工序中铺网机的输送帘、补偿帘、铺网帘的线速度相同。