CN103094388A - 一种新型太阳电池封装技术 - Google Patents
一种新型太阳电池封装技术 Download PDFInfo
- Publication number
- CN103094388A CN103094388A CN2013100622611A CN201310062261A CN103094388A CN 103094388 A CN103094388 A CN 103094388A CN 2013100622611 A CN2013100622611 A CN 2013100622611A CN 201310062261 A CN201310062261 A CN 201310062261A CN 103094388 A CN103094388 A CN 103094388A
- Authority
- CN
- China
- Prior art keywords
- backboard
- glass
- cover plate
- solder
- solar cell
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种新型太阳电池封装技术,包括位于太阳电池下面的背板、位于太阳电池上部的盖板和盖板与背板之间钎料;所述背板和盖板都是玻璃制成的;所述钎料是熔点低于所述玻璃背板和盖板的填充物,其在低于玻璃的熔点、高于钎料熔点的温度下,利用液态钎料在玻璃表面润湿、铺展和在玻璃间隙中填缝,与玻璃相互溶解与扩散,而实现背板和盖板的密封;所述整个钎焊过程是在真空环境或惰性气体环境中将背板与盖板密封成一体。
Description
技术领域
本发明涉及太阳电池封装技术领域。
背景技术
太阳能发电是一种新型能源,具有环保、节能、取之不尽用之不竭等特点,在当前世界范围资源紧缺的环境下,太阳能发电以其固有的特点赢得了多数使用者的青睐。太阳能电池组件是太阳能发电系统中的核心部分,也是太阳能发电系统中价值最高的部分,其作用是将太阳能转化为电能。为了保证太阳电池在恶劣的户外环境下能可靠运行,必须对太阳电池组件进行封装,以达到隔离空气、保护电池片、增加透光率、延长寿命的目的。现有技术太阳能电池组件封装按照玻璃、EVA、电池串、EVA、背板的顺序敷设,通过层压机抽真空加热使EVA熔化,将玻璃、电池串及背板封装在一起。在加热使EVA熔化过程中,随着EVA流动及层压机施加的压力会使太阳能电池片偏离预定位置,可能造成电池片之间彼此接触,不仅影响外观,还会发生短路现象,影响太阳能电池组件的正常使用。
发明内容
本发明的目的在于克服现有技术存在的缺点,提供一种新型太阳电池封装技术,可以使太阳电池不受恶劣环境的影响,保证太阳电池具有稳定的光电转换效率,能够延长了太阳电池的使用寿命。
本发明解决技术问题采用如下技术方案:
一种新型太阳电池封装技术,其特征在于,包括位于太阳电池下面的背板、位于太阳电池上部的盖板和盖板与背板之间钎料;所述背板和盖板都是玻璃制成的;所述钎料是熔点低于所述玻璃背板和盖板的填充物,其在低于玻璃的熔点、高于钎料熔点的温度下,利用液态钎料在玻璃表面润湿、铺展和在玻璃间隙中填缝,与玻璃相互溶解与扩散,而实现背板和盖板的密封;所述整个钎焊过程是在真空环境或惰性气体环境中将背板与盖板密封成一体。
以上所述盖板和背板是玻璃材质的,所述盖板所用玻璃采用光的透过率高、耐冲击、使用寿命长的低铁钢化玻璃。
以上所述背板上有两个相互绝缘并且内外相通的电极连接腿;所述这两个相互绝缘且内外相通的电极连接腿与背板是密封为一体的。
以上所述太阳电池串安装在所述背板上,将太阳电池串的正负极与背板上的两个电极连接腿分别相连接。
以上所述钎料位于所述盖板和所述背板连接缝之间,其熔点低于所述玻璃背板和盖板的熔点,在真空或惰性气体环境中,钎料被加热到稍高于钎料熔点低于背板与盖板玻璃熔点温度后,钎料熔化,并借助毛细管作用被吸入和充满背板与盖板玻璃间隙之间,液态钎料与背板与盖板玻璃相互扩散溶解,最后把太阳电池串密封于盖板和背板之间。
本发明与现有技术相比,使太阳电池封装的盖板和背板都使用玻璃,在真空或惰性气体环境中用钎焊封装技术进行封装,不会出现氧化,增碳,脱碳及污染变质等现象,可以使太阳电池不受恶劣环境的影响,保证太阳电池具有稳定的光电转换效率,能够延长太阳电池的使用寿命,并且钎焊时,钎焊温度低于玻璃的熔点,对玻璃影响小,且整体受热均匀,热应力小,这样杜绝了太阳电池串因为压力作用偏离预定位置引发短路的问题,并且在此技术下封装的太阳电池结构美观,透光性能好。
附图说明
图1为本发明新型太阳电池封装技术的示意图。
图中:(1)盖板;(2)背板;(3)太阳电池串;(4)钎料;(5)~(6)电极连接腿。
具体实施方式:
为了进一步说明本发明的结构和特征,以下结合实施例和附图对本发明作进一步的说明。
如图1所示的新型太阳电池封装技术的示意图,包括盖板(1)、背板(2)、太阳电池串(3)、钎料(4)、电极连接腿(5)~(6);所述背板(2)和盖板(1)都是玻璃制成的;所述钎料(4)是熔点低于所述玻璃背板和盖板的填充物;这样首先将太阳电池串(3)安装在背板(2)上,然后将太阳电池串的正负电极分别与背板上的两个电极连接腿相连接;最后在真空或惰性气体环境中,利用钎焊技术,在低于玻璃的熔点、高于钎料熔点的温度下,利用液态钎料在玻璃表面润湿、铺展和在玻璃间隙中填缝,与玻璃相互溶解与扩散,而实现盖板(1)和背板(2)的密封,将太阳电池串密封于背板与盖板所密封的内部,其成为一体,所用技术简单,封装后的太阳电池结构美观,透光性能好。
Claims (5)
1.一种新型太阳电池封装技术,包括太阳电池串(3),其特征在于,包括位于太阳电池上部的盖板(1)、位于太阳电池下面的背板(2)和盖板与背板之间钎料(4);所述背板(2)和盖板(1)都是玻璃制成的;所述钎料(4)是熔点低于所述玻璃背板和盖板的填充物,其在低于玻璃的熔点、高于钎料熔点的温度下,利用液态钎料在玻璃表面润湿、铺展和在玻璃间隙中填缝,与玻璃相互溶解与扩散,而实现盖板(1)和背板(2)的密封;所述整个钎焊过程是在真空环境或惰性气体环境中将背板与盖板密封成一体。
2.根据权利要求1所述的一种新型太阳电池封装技术,其特征在于,所述盖板(1)和背板(2)是玻璃材质的;所述盖板所用玻璃采用光的透过率高、耐冲击、使用寿命长的低铁钢化玻璃。
3.根据权利要求1所述的一种新型太阳电池封装技术,其特征在于,所述背板(2)上有两个相互绝缘并且内外相通的电极连接腿(5;6);所述这两个相互绝缘且内外相通的电极连接腿(5;6)与背板(2)是密封为一体的。
4.根据权利要求1所述的一种新型太阳电池封装技术,其特征在于,所述太阳电池串(3)安装在所述背板(2)上和所述盖板(1)下,将太阳电池串的正负极与背板上的两个电极连接腿(5;6)分别相连接。
5.根据权利要求1所述的一种新型太阳电池封装技术,其特征在于,所述钎料(4)位于所述盖板(1)和所述背板(2)连接缝之间,其熔点低于所述玻璃背板和盖板的熔点,在真空或惰性气体环境中,钎料(4)被加热到稍高于钎料熔点低于背板与盖板玻璃熔点温度后,钎料熔化,并借助毛细管作用被吸入和充满背板与盖板玻璃间隙之间,液态钎料与背板与盖板玻璃相互扩散溶解,最后把太阳电池串(3)密封于所述盖板(1)和背板(2)之间。