CN103045774A - 一种皮革用阻燃剂及其制备方法 - Google Patents
一种皮革用阻燃剂及其制备方法 Download PDFInfo
- Publication number
- CN103045774A CN103045774A CN 201210584297 CN201210584297A CN103045774A CN 103045774 A CN103045774 A CN 103045774A CN 201210584297 CN201210584297 CN 201210584297 CN 201210584297 A CN201210584297 A CN 201210584297A CN 103045774 A CN103045774 A CN 103045774A
- Authority
- CN
- China
- Prior art keywords
- parts
- leather
- pvc
- flame retardant
- acetate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开了一种皮革用阻燃剂及其制备方法。以重量份计,本发明由以下组分组成:聚氯乙烯树脂:10~20,磷酸三甲酚酯:20~30,氯化石蜡:3~8,邻苯二甲亚酰胺:2~5,顺丁烯二酸二甲酯:10~20,氯化钙:2~6,醋酸钠:1~3,三乙醇胺:4~8,醋酸丁酯:30~50,水:400~600。与现有技术相比,本发明具有如下有益效果:(1)具有良好的阻燃效果,不损伤皮革表面;(2)制备工艺简单,原料易得,成本低廉。
Description
技术领域
本发明属于皮革助剂技术领域,更具体是涉及一种皮革用阻燃剂及其制备方法。
背景技术
皮革通常是由动物皮毛经加工处理而成,比较容易着火,皮革在制成皮革制品之前通常都需要进行阻燃处理,否则在其加工之后的使用过程中,容易产生安全隐患。
发明内容
本发明的目的在于克服现有技术存在的不足,提供一种皮革用阻燃剂。
本发明的另一目的在于提供该皮革用阻燃剂的制备方法。
为达到上述目的,本发明采取了如下的技术方案:
一种皮革用阻燃剂,以重量份计,由以下组分组成:
聚氯乙烯树脂:10~20,磷酸三甲酚酯:20~30,
氯化石蜡:3~8,邻苯二甲亚酰胺:2~5,
顺丁烯二酸二甲酯:10~20,氯化钙:2~6,醋酸钠:1~3,
三乙醇胺:4~8,醋酸丁酯:30~50,水:400~600。
所述的一种皮革用阻燃剂的制备方法,其特征在于,包括如下步骤:
(1)将顺丁烯二酸二甲酯溶于水中,混合均匀;
(2)将聚氯乙烯树脂、磷酸三甲酚酯、氯化石蜡及醋酸丁酯混合,搅拌均匀;
(3)将步骤(2)的产物加入步骤(1)的产物中,升温至50~60℃,反应1~3小时;
(4)冷却至室温后,加入其余组分,搅拌混合均匀后即可得成品。
与现有技术相比,本发明具有如下有益效果:
(1)具有良好的阻燃效果,不损伤皮革表面;
(2)制备工艺简单,原料易得,成本低廉。
具体实施方式
以下结合具体实施例来对本发明作进一步的描述。
实施例1
一种皮革用阻燃剂,以重量份计,由以下组分组成:
聚氯乙烯树脂:10,磷酸三甲酚酯:20,
氯化石蜡:3,邻苯二甲亚酰胺:2,
顺丁烯二酸二甲酯:10,氯化钙:2,醋酸钠:1,
三乙醇胺:4,醋酸丁酯:30,水:400。
实施例2
一种皮革用阻燃剂,以重量份计,由以下组分组成:
聚氯乙烯树脂:20,磷酸三甲酚酯:30,
氯化石蜡:8,邻苯二甲亚酰胺:5,
顺丁烯二酸二甲酯:20,氯化钙:6,醋酸钠:3,
三乙醇胺:8,醋酸丁酯:50,水:600。
实施例3
一种皮革用阻燃剂,以重量份计,由以下组分组成:
聚氯乙烯树脂:16,磷酸三甲酚酯:25,
氯化石蜡:6,邻苯二甲亚酰胺:4,
顺丁烯二酸二甲酯:15,氯化钙:4,醋酸钠:2,
三乙醇胺:6,醋酸丁酯:40,水:500。
上述实施例中,所述的一种皮革用阻燃剂的制备方法,包括如下步骤:
(1)将顺丁烯二酸二甲酯溶于水中,混合均匀;
(2)将聚氯乙烯树脂、磷酸三甲酚酯、氯化石蜡及醋酸丁酯混合,搅拌均匀;
(3)将步骤(2)的产物加入步骤(1)的产物中,升温至50~60℃,反应1~3小时;
(4)冷却至室温后,加入其余组分,搅拌混合均匀后即可得成品。
Claims (5)
1.一种皮革用阻燃剂,其特征在于,以重量份计,由以下组分组成:
聚氯乙烯树脂:10~20,磷酸三甲酚酯:20~30,
氯化石蜡:3~8,邻苯二甲亚酰胺:2~5,
顺丁烯二酸二甲酯:10~20,氯化钙:2~6,醋酸钠:1~3,
三乙醇胺:4~8,醋酸丁酯:30~50,水:400~600。
2.根据权利要求1所述的一种皮革用阻燃剂,其特征在于,以重量份计,由以下组分组成:
聚氯乙烯树脂:10,磷酸三甲酚酯:20,
氯化石蜡:3,邻苯二甲亚酰胺:2,
顺丁烯二酸二甲酯:10,氯化钙:2,醋酸钠:1,
三乙醇胺:4,醋酸丁酯:30,水:400。
3.根据权利要求1所述的一种皮革用阻燃剂,其特征在于,以重量份计,由以下组分组成:
聚氯乙烯树脂:20,磷酸三甲酚酯:30,
氯化石蜡:8,邻苯二甲亚酰胺:5,
顺丁烯二酸二甲酯:20,氯化钙:6,醋酸钠:3,
三乙醇胺:8,醋酸丁酯:50,水:600。
4.根据权利要求1所述的一种皮革用阻燃剂,其特征在于,以重量份计,由以下组分组成:
聚氯乙烯树脂:16,磷酸三甲酚酯:25,
氯化石蜡:6,邻苯二甲亚酰胺:4,
顺丁烯二酸二甲酯:15,氯化钙:4,醋酸钠:2,
三乙醇胺:6,醋酸丁酯:40,水:500。
5.权利要求1所述的一种皮革用阻燃剂的制备方法,其特征在于,包括如下步骤:
(1)将顺丁烯二酸二甲酯溶于水中,混合均匀;
(2)将聚氯乙烯树脂、磷酸三甲酚酯、氯化石蜡及醋酸丁酯混合,搅拌均匀;
(3)将步骤(2)的产物加入步骤(1)的产物中,升温至50~60℃,反应1~3小时;
(4)冷却至室温后,加入其余组分,搅拌混合均匀后即可得成品。