CN102965479A - 高耐蚀奥氏体不锈钢表层的快速制备方法 - Google Patents
高耐蚀奥氏体不锈钢表层的快速制备方法 Download PDFInfo
- Publication number
- CN102965479A CN102965479A CN2012105275764A CN201210527576A CN102965479A CN 102965479 A CN102965479 A CN 102965479A CN 2012105275764 A CN2012105275764 A CN 2012105275764A CN 201210527576 A CN201210527576 A CN 201210527576A CN 102965479 A CN102965479 A CN 102965479A
- Authority
- CN
- China
- Prior art keywords
- stainless steel
- corrosion
- frequency induction
- sample
- top layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
输出频率/KHz | 输出电流/A | 加热时间/s |
50 | 400-600 | 15-45 |
Claims (5)