CN102914151A - 金属熔液保持器 - Google Patents
金属熔液保持器 Download PDFInfo
- Publication number
- CN102914151A CN102914151A CN2012104699887A CN201210469988A CN102914151A CN 102914151 A CN102914151 A CN 102914151A CN 2012104699887 A CN2012104699887 A CN 2012104699887A CN 201210469988 A CN201210469988 A CN 201210469988A CN 102914151 A CN102914151 A CN 102914151A
- Authority
- CN
- China
- Prior art keywords
- crucible
- molten metal
- metal
- metal retainer
- burning
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明揭示了一种金属熔液保持器,包括坩锅、燃烧架和数个烧嘴。坩锅由耐火材料制作,坩锅侧壁上具有固持部件,坩锅具有一盖。坩锅架设在燃烧架上。数个烧嘴安装在燃烧架上,数个烧嘴对准所述坩锅并加热坩锅。金属原料放置在坩锅中,盖上盖,控制工作的烧嘴的数量和功率使得金属原料在坩锅中熔化,调整工作的烧嘴的数量和功率使得坩锅中的金属保持熔融液态。本发明的金属熔液保持器将金属置于坩锅中,使得金属能够在坩锅这样一个封闭无氧的环境中被加热,可以避免氧化情况的发生。通过调节处于工作状态的烧嘴的数量和功率,能够使该金属熔液保持器工作熔化模式或者保持模式下。
Description
技术领域
本发明涉及冶金设备领域,尤其涉及一种金属熔液保持器。
背景技术
在冶金领域中,熔化金属是十分普遍而重要的工艺。熔化后的金属能够用于铸造各种造型的金属部件。由于金属的熔点高,因此熔化金属需要将金属加热到很高的温度。在高温下,氧化反应更加剧烈,金属可能会产生氧化反应而出现不希望的副产物,并引起对金属原料的消耗。这一现象在一些稀有金属的熔化过程中显得尤为明显,稀有金属价格昂贵,如果在熔化过程中因为氧化反应而出现损耗是十分重大的损失。
发明内容
本发明旨在提出一种适合于稀有金属的能在无氧状态下进行熔化的金属熔液保持器。
根据本发明的一实施例,提出一种金属熔液保持器,包括坩锅、燃烧架和数个烧嘴。坩锅由耐火材料制作,坩锅侧壁上具有固持部件,坩锅具有一盖。坩锅架设在燃烧架上。数个烧嘴安装在燃烧架上,数个烧嘴对准所述坩锅并加热坩锅。金属原料放置在坩锅中,盖上盖,控制工作的烧嘴的数量和功率使得金属原料在坩锅中熔化,调整工作的烧嘴的数量和功率使得坩锅中的金属保持熔融液态。
在一个实施例中,坩锅由石墨制作。固持部件是从坩锅的侧壁上突出的耳部。
在一个实施例中,盖包括基座和从基座上向下凸起的凸起部,凸起部的外径与坩锅的内径匹配,基座的外径大于坩锅的外径;凸起部嵌入坩锅内,基座盖于坩锅的开口上,盖封闭坩锅。盖是石墨制作。
在一个实施例中,坩锅通过固持部件架设在燃烧架的顶部。
在一个实施例中,数个烧嘴呈扇形布置在燃烧架的侧壁和底部,烧嘴的出口对准坩锅。
本发明的金属熔液保持器将金属置于坩锅中,使得金属能够在坩锅这样一个封闭无氧的环境中被加热,可以避免氧化情况的发生。通过调节处于工作状态的烧嘴的数量和功率,能够使该金属熔液保持器工作熔化模式或者保持模式下。
附图说明
图1揭示了根据本发明的一实施例的金属熔液保持器的结构图。
具体实施例方式
参考图1所示,图1揭示了根据本发明的一实施例的金属熔液保持器的结构图。该金属熔液保持器100包括坩锅102、燃烧架104和数个烧嘴106。
坩锅102由耐火材料制作,在一个实施例中,坩锅102由石墨制作。坩锅102的侧壁上具有固持部件121,在图示的实施例中,固持部件121是从坩锅102的侧壁上突出的耳部,耳部一般为两个,布置在坩锅对称的两侧。
坩锅102具有一盖122。在图示的实施例中,盖122包括基座123和从基座123上向下凸起的凸起部124,凸起部124的外径与坩锅102的内径匹配,基座123的外径大于坩锅102的外径。在盖122盖在坩锅102上时,凸起部124嵌入坩锅102内,基座123盖于坩锅102的开口上,利用凸起部124和坩锅102的尺寸配合,基本可以隔绝外界空气进入坩锅内部。从而使得盖122封闭坩锅102。在一个实施例中,盖122也是由耐火材料,比如石墨制作。
坩锅102架设在燃烧架104上。燃烧架104可以是方形结构,也可以设计成其他的形状。燃烧架104可以是开放式的,也可以是封闭式的。坩锅102通过固持部件121架设在燃烧架104的顶部。
数个烧嘴106安装在燃烧架104上,数个烧嘴106对准坩锅102并加热坩锅。在图示的实施例中,数个烧嘴106呈扇形布置在燃烧架104的侧壁和底部,每一个烧嘴106的出口对准坩锅102。
该金属熔液保持器100具有两种工作模式:熔化模式和保持模式。在熔化模式中,数量较多的烧嘴将被开启并调节至较大的功率,充分加热坩锅,使得坩锅中的金属原料熔解。在保持模式中,金属已经熔解成为熔融液态,此时处于工作状态的烧嘴的数量可以适当减少,并且功率也可以适当减小。该金属熔液保持器100的工作过程可以如下:首先打开盖,将金属原料放置在坩锅中。盖上盖,按照熔化模式控制工作的烧嘴的数量和功率,使得金属原料在坩锅中熔化。调节工作模式成为保持模式,调整工作的烧嘴的数量和功率使得坩锅中的金属保持熔融液态。
本发明的金属熔液保持器将金属置于坩锅中,使得金属能够在坩锅这样一个封闭无氧的环境中被加热,可以避免氧化情况的发生。通过调节处于工作状态的烧嘴的数量和功率,能够使该金属熔液保持器工作熔化模式或者保持模式下。
Claims (7)
1.一种金属熔液保持器,其特征在于,包括:
坩锅,坩锅由耐火材料制作,坩锅侧壁上具有固持部件,坩锅具有一盖;
燃烧架,坩锅架设在所述燃烧架上;
数个烧嘴,数个烧嘴安装在所述燃烧架上,数个烧嘴对准所述坩锅并加热所述坩锅;
金属原料放置在所述坩锅中,盖上盖,控制工作的烧嘴的数量和功率使得金属原料在坩锅中熔化,调整工作的烧嘴的数量和功率使得坩锅中的金属保持熔融液态。
2.如权利要求1所述的金属熔液保持器,其特征在于,所述坩锅由石墨制作。
3.如权利要求1所述的金属熔液保持器,其特征在于,所述固持部件是从坩锅的侧壁上突出的耳部。
4.如权利要求1所述的金属熔液保持器,其特征在于,所述盖包括基座和从基座上向下凸起的凸起部,所述凸起部的外径与坩锅的内径匹配,所述基座的外径大于坩锅的外径;凸起部嵌入坩锅内,基座盖于坩锅的开口上,盖封闭所述坩锅。
5.如权利要求1所述的金属熔液保持器,其特征在于,所述盖是石墨制作。
6.如权利要求1所述的金属熔液保持器,其特征在于,所述坩锅通过固持部件架设在燃烧架的顶部。
7.如权利要求6所述的金属熔液保持器,其特征在于,数个烧嘴呈扇形布置在燃烧架的侧壁和底部,烧嘴的出口对准所述坩锅。