CN102911569B - Waterproof paint - Google Patents

Waterproof paint Download PDF

Info

Publication number
CN102911569B
CN102911569B CN201210440856.1A CN201210440856A CN102911569B CN 102911569 B CN102911569 B CN 102911569B CN 201210440856 A CN201210440856 A CN 201210440856A CN 102911569 B CN102911569 B CN 102911569B
Authority
CN
China
Prior art keywords
waterproof paint
kaolin
gasoline
weight percent
ethylene glycol
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201210440856.1A
Other languages
Chinese (zh)
Other versions
CN102911569A (en
Inventor
姜晓强
石振宇
魏鑫
石刚
赵秀娟
刘慧慧
王承锋
曹瑞晓
张利刚
谭明忠
施雄
李桂兰
王英浩
孙振华
常爱玉
董英
渠文学
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiang Xiaoqiang
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201210440856.1A priority Critical patent/CN102911569B/en
Publication of CN102911569A publication Critical patent/CN102911569A/en
Application granted granted Critical
Publication of CN102911569B publication Critical patent/CN102911569B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a waterproof paint which has good anti-permeability and stability, and is low in cost, free from toxicity and environment-friendly. The waterproof paint comprises the components by weight percent: 5-10% of asphalt, 5-15% of polyvinyl chloride, 10-18% of polyvinyl alcohol, 6-20% of hydrated lime, 1-5% of mica powder, 5-10% of gasoline, 1-3% of kaolin, 1-5% of ethylene glycol phenyl ether, 5-8% of white emulsion, 3-8% of titanium dioxide, 1-6% of antioxidant, 1-3% of silicon dioxide, 2-5% of dispersing agent and the balance of water. The waterproof paint has good anti-permeability and stability, and is low in cost, free from toxicity and environment-friendly.

Description

A kind of waterproof paint
Technical field
The present invention relates to a kind of waterproof paint.
Background technology
Waterproof paint refers to that film that coating is formed can prevent a kind of coating of rainwater or underground water seepage.At present, the water-proof material on market has two large classes: one is polyurethane kind waterproof paint.This kind of material is generally be made up as starting material of Polyurethane and coal tar.The tar gas toxicity that it volatilizees is large, and is not easy to remove, and is therefore prohibited from using in 2000 in China.The polyurethane waterproofing coating still sold replaces coal tar as raw material with pitch.But when using this coating, general employing is diluted containing the organic solvent such as toluene, dimethylbenzene, thus also containing toxic; Another kind of is polymer cement-base waterproof coating.The emulsion that it is synthesized by multiple waterborne polymeric forms with the high grade cement being mixed with various additive, and the flexibility of polymkeric substance (resin) and the rigidity of cement became one, and makes it in impermeability with stability, show excellence.Its advantage is that easy construction, comprehensive cost are low, and the duration is short, and asepsis environment-protecting.Therefore, polyalcohol cement basis has become the leading role in waterproof paint market.
Summary of the invention
The object of the invention is, for overcoming above-mentioned the deficiencies in the prior art, a kind of waterproof paint to be provided, there is good impermeability and stability, and cost to be low, asepsis environment-protecting.
For achieving the above object, the present invention adopts following technical proposals:
A kind of waterproof paint, is made up of the component of following weight percent: pitch 5-10%, polyvinyl chloride 5-15%, polyvinyl alcohol 10-18%, white lime 6-20%, mica powder 1-5%, gasoline 5-10%, kaolin 1-3%, ethylene glycol phenyl ether 1-5%, white glue with vinyl 5-8%, titanium dioxide 3-8%, oxidation inhibitor 1-6%, silica 1-3%, dispersion agent 2-5%, surplus is water.
Described oxidation inhibitor is any one or two kinds of in antioxidant 264, irgasfos 168.
Described dispersion agent is lithium magnesium silicate or IW.
The invention has the beneficial effects as follows, there is good impermeability and stability, and cost is low, asepsis environment-protecting.
Embodiment
Below in conjunction with embodiment, the present invention will be further elaborated, should be noted that following explanation is only to explain the present invention, not limiting its content.
Embodiment 1:
The present invention is made up of the component of following weight percent: pitch 5%, polyvinyl chloride 5%, polyvinyl alcohol 10%, white lime 6%, mica powder 1%, gasoline 5%, kaolin 1%, ethylene glycol phenyl ether 1%, white glue with vinyl 5%, titanium dioxide 3%, antioxidant 264 is 1%, silica 1 %, lithium magnesium silicate is 2%, and surplus is water.
Embodiment 2:
The present invention is made up of the component of following weight percent: pitch 10%, polyvinyl chloride 10%, polyvinyl alcohol 18%, white lime 10%, mica powder 5%, gasoline 10%, kaolin 3%, ethylene glycol phenyl ether 5%, white glue with vinyl 8%, titanium dioxide 3%, irgasfos 168 is 6%, and silicon-dioxide 3%, IW is 5%, and surplus is water.
Embodiment 3:
The present invention is made up of the component of following weight percent: pitch 5%, polyvinyl chloride 15%, polyvinyl alcohol 10%, white lime 6%, mica powder 5%, gasoline 10%, kaolin 1%, ethylene glycol phenyl ether 1%, white glue with vinyl 8%, titanium dioxide 8%, antioxidant 264 and irgasfos 168 are 6%, silicon-dioxide 3%, lithium magnesium silicate is 2%, and surplus is water.
Embodiment 4:
The present invention is made up of the component of following weight percent: pitch 10%, polyvinyl chloride 5%, polyvinyl alcohol 18%, white lime 20%, mica powder 1%, gasoline 5%, kaolin 3%, ethylene glycol phenyl ether 1%, white glue with vinyl 8%, titanium dioxide 8%, irgasfos 168 is 1%, silica 1 %, lithium magnesium silicate is 5%, and surplus is water.
Embodiment 5:
The present invention is made up of the component of following weight percent: pitch 10%, polyvinyl chloride 15%, polyvinyl alcohol 10%, white lime 20%, mica powder 1%, gasoline 5%, kaolin 1-3%, ethylene glycol phenyl ether 1%, white glue with vinyl 5%, titanium dioxide 3%, antioxidant 264 is 1%, silica 1 %, IW are 2%, and surplus is water.
Although above-mentioned, the specific embodiment of the present invention is described; but not limiting the scope of the invention; on the basis of technical scheme of the present invention, those skilled in the art do not need to pay various amendment or distortion that creative work can make still within protection scope of the present invention.

Claims (5)

1. a waterproof paint, is characterized in that, is made up of the component of following weight percent: pitch 5 %, polyvinyl chloride 5 %, polyvinyl alcohol 10 %, white lime 6 %, mica powder 1 %, gasoline 5 %, kaolin 1 %, ethylene glycol phenyl ether 1 %, white glue with vinyl 5 %, titanium dioxide 3 %, antioxidant 264 is 1%, silica 1 %, lithium magnesium silicate is 2 %, and surplus is water.
2. a waterproof paint, is characterized in that, is made up of the component of following weight percent: pitch 10 %, polyvinyl chloride 10 %, polyvinyl alcohol 18 %, white lime 10 %, mica powder 5 %, gasoline 10 %, kaolin 3 %, ethylene glycol phenyl ether 5 %, white glue with vinyl 8 %, titanium dioxide 3 %, irgasfos 168 is 6%, silicon-dioxide 3 %, dispersion agent IW are 5 %, and surplus is water.
3. a waterproof paint, is characterized in that, is made up of the component of following weight percent: pitch 5 %, polyvinyl chloride 15 %, polyvinyl alcohol 10 %, white lime 6 %, mica powder 5 %, gasoline 10 %, kaolin 1 %, ethylene glycol phenyl ether 1%, white glue with vinyl 8 %, titanium dioxide 8 %, antioxidant 264 and irgasfos 168 are 6%, silicon-dioxide 3 %, lithium magnesium silicate is 2 %, and surplus is water.
4. a waterproof paint, is characterized in that, is made up of the component of following weight percent: pitch 10 %, polyvinyl chloride 5 %, polyvinyl alcohol 18 %, white lime 20 %, mica powder 1 %, gasoline 5 %, kaolin 3 %, ethylene glycol phenyl ether 1 %, white glue with vinyl 8 %, titanium dioxide 8 %, irgasfos 168 is 1%, silica 1 %, lithium magnesium silicate is 5 %, and surplus is water.
5. a waterproof paint, is characterized in that, is made up of the component of following weight percent: pitch 10 %, polyvinyl chloride 15 %, polyvinyl alcohol 10 %, white lime 20 %, mica powder 1%, gasoline 5 %, kaolin 1-3 %, ethylene glycol phenyl ether 1%, white glue with vinyl 5%, titanium dioxide 3%, antioxidant 264 is 1%, silica 1 %, dispersion agent IW are 2 %, and surplus is water.
CN201210440856.1A 2012-11-07 2012-11-07 Waterproof paint Expired - Fee Related CN102911569B (en)