CN102731853B - 耐油橡胶 - Google Patents

耐油橡胶 Download PDF

Info

Publication number
CN102731853B
CN102731853B CN2012102194888A CN201210219488A CN102731853B CN 102731853 B CN102731853 B CN 102731853B CN 2012102194888 A CN2012102194888 A CN 2012102194888A CN 201210219488 A CN201210219488 A CN 201210219488A CN 102731853 B CN102731853 B CN 102731853B
Authority
CN
China
Prior art keywords
rubber
oil
oil resistant
resistant rubber
dithienylglycolate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2012102194888A
Other languages
English (en)
Other versions
CN102731853A (zh
Inventor
钱佑武
钱必树
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuhu City Hongda Rubber Plastic Valve Manufacture Co Ltd
Original Assignee
Wuhu City Hongda Rubber Plastic Valve Manufacture Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuhu City Hongda Rubber Plastic Valve Manufacture Co Ltd filed Critical Wuhu City Hongda Rubber Plastic Valve Manufacture Co Ltd
Priority to CN2012102194888A priority Critical patent/CN102731853B/zh
Publication of CN102731853A publication Critical patent/CN102731853A/zh
Application granted granted Critical
Publication of CN102731853B publication Critical patent/CN102731853B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了耐油橡胶,所述的橡胶含有以下物质:天然橡胶、胎面胶、氧化锌、硬脂酸、碳黑N330、石蜡、古马隆、硫黄、沥青、2,2-二噻吩基乙醇酸甲酯、防老剂、促进剂。本发明与现有技术相比,通过在配方中加入2,2-二噻吩基乙醇酸甲酯,使天然橡胶的耐油性能提高到了8-10%。

Description

耐油橡胶
技术领域
本发明涉及橡胶,特别涉及用于管道衬套的耐油橡胶。
背景技术
在油田的管道运输中,所运输的介质为油和矿砂的混合物,故其管道衬套所用的橡胶通常是含有胎面胶的天然橡胶,虽然上述橡胶具有耐磨性能,但其耐油性很差,其耐油性能只能达到15%以上。
发明内容
本发明所要解决的技术问题是提供一种耐油性能达到8-10%的耐油橡胶。
本发明解决技术问题的技术方案为:耐油橡胶,含有以下物质及重量份:
Figure BDA0000182126801
Figure BDA0000182126802
所述的防老剂为:2,2,4-三甲基-1,2-二氢喹啉聚合物,防老剂RD。
所述的促进剂为:4-4'-二硫化二吗啉(DTDM)
本发明的制备方法与现有的橡胶的制备方法相同。
本发明与现有技术相比,通过在配方中加入2,2-二噻吩基乙醇酸甲酯,使天然橡胶的耐油性能提高到了8-10%。
具体实施方式:
下面结合实施例对本发明作详细的说明。
实施例1:
Figure BDA0000182126803
实施例2:
Figure BDA0000182126804
实施例3
Figure BDA0000182126805
Figure BDA0000182126806
本发明的耐油性能按照ASTM  D 471标准进行检测,单位为%;
实施例1、2、3的耐油性能(油浸泡后的膨胀率)分别为8%、8.5%、9%。

Claims (3)

1.耐油橡胶,其特征在于:含有以下物质及重量份:
Figure FDA0000343685381
2.根据权利要求1所述的耐油橡胶,其特征在于:所述的防老剂为2,2,4-三甲基-1,2-二氢喹啉聚合物。
3.根据权利要求1所述的耐油橡胶,其特征在于: 所述的促进剂为4,4'-二硫化二吗啉。
CN2012102194888A 2012-06-28 2012-06-28 耐油橡胶 Active CN102731853B (zh)