CN102728986A - 一种锚爪磨损的修复方法 - Google Patents
一种锚爪磨损的修复方法 Download PDFInfo
- Publication number
- CN102728986A CN102728986A CN2011100872139A CN201110087213A CN102728986A CN 102728986 A CN102728986 A CN 102728986A CN 2011100872139 A CN2011100872139 A CN 2011100872139A CN 201110087213 A CN201110087213 A CN 201110087213A CN 102728986 A CN102728986 A CN 102728986A
- Authority
- CN
- China
- Prior art keywords
- anchor jaw
- anchor
- anchor fluke
- electric welding
- jaw
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种锚爪磨损的修复方法,属船舶上必备附件的维护及修复。其特征是:在锚爪的末梢及两侧边缘的磨损部位,用电焊的方法将其堆焊起来,而后使用手提磨削机及手工工具修整,将其修复至恢复锚爪的原有外形。所述的电焊,其使用的电焊条的材料必须与锚爪的材质一致。使用本发明方法修复后的锚爪又可以与原锚爪一样进行使用了。由于本发明将锚爪末梢及两侧边缘的磨损处用电焊的方法堆焊起来,恢复至锚爪原有的外形,焊条的材料要与锚的材质一样,堆焊后对修补处进行打磨和修整,即可恢复锚的使用效能。同时,本发明的修复方法简单、实用,且修复后的锚爪与原锚爪具有同样的使用寿命。
Description
技术领域
本发明涉及船舶上必备附件的维护及修复,具体的说是一种锚爪磨损的修复方法。
背景技术
锚爪是船舶上的一个重要的必备附件,然而锚爪经过长时间的使用,其锚爪的末梢及边缘会磨损,使抛锚时的抓力削弱,严重时会产生走锚的现象,影响了船舶抛锚后的安全性。一但发生这种情况,则只有更换上新的锚爪再进行使用。
发明内容
为了克服现有锚爪磨损后难以修复等问题,本发明的目的是要提供一种简单有效的锚爪磨损的修复方法。
本发明解决其技术问题所采用的技术方案是:一种锚爪磨损的修复方法,其特征是:在锚爪的末梢及两侧边缘的磨损部位,用电焊的方法将其堆焊起来,而后使用手提磨削机及手工工具修整,将其修复至恢复锚爪的原有外形。
所述的电焊,其使用的电焊条的材料必须与锚爪的材质一致。
使用本发明方法修复后的锚爪又可以与原锚爪一样进行使用了。
本发明的有益效果:由于本发明将锚爪末梢及两侧边缘的磨损处用电焊的方法堆焊起来,恢复至锚爪原有的外形,焊条的材料要与锚的材质一样,堆焊后对修补处进行打磨和修整,即可恢复锚的使用效能。同时,本发明的修复方法简单、实用,且修复后的锚爪与原锚爪具有同样的使用寿命。
附图说明
以下结合附图及实施例对本发明进行进一步的描述。
图1是本发明修复锚爪后的示意图。
图中1锚爪本体,2堆焊区。
具体实施方式
实施例1:
请参阅图1,有一个锚爪本体1,锚爪本体1的周边磨损处为电焊的堆焊区。本实施例是在锚爪本体1的末梢及两侧边缘的磨损部位,用电焊的方法将其堆焊起来,使其成为一个略大于原锚爪的堆焊区,而后使用手提磨削机及手工修整,将其修复至恢复锚爪的原有外形。
所述的电焊,其使用的电焊条的材料必须与锚爪的材质一致。
Claims (2)
1.一种锚爪磨损的修复方法,其特征是:在锚爪的末梢及两侧边缘的磨损部位,用电焊的方法将其堆焊起来,而后使用手提磨削机及手工工具修整,将其修复至恢复锚爪的原有外形。
2.根据权利要求1所述的一种锚爪磨损的修复方法,其特征是:所述的电焊,其使用的电焊条的材料必须与锚爪的材质一致。