CN102694173A - 一种纳米线/棒状形貌硅酸锰锂的水热合成方法 - Google Patents
一种纳米线/棒状形貌硅酸锰锂的水热合成方法 Download PDFInfo
- Publication number
- CN102694173A CN102694173A CN2012101135717A CN201210113571A CN102694173A CN 102694173 A CN102694173 A CN 102694173A CN 2012101135717 A CN2012101135717 A CN 2012101135717A CN 201210113571 A CN201210113571 A CN 201210113571A CN 102694173 A CN102694173 A CN 102694173A
- Authority
- CN
- China
- Prior art keywords
- hydrothermal synthesis
- positive electrode
- lithium
- anode material
- synthesis method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (5)