CN102674796A - 利用污泥制造建筑砖的方法 - Google Patents

利用污泥制造建筑砖的方法 Download PDF

Info

Publication number
CN102674796A
CN102674796A CN2011100607434A CN201110060743A CN102674796A CN 102674796 A CN102674796 A CN 102674796A CN 2011100607434 A CN2011100607434 A CN 2011100607434A CN 201110060743 A CN201110060743 A CN 201110060743A CN 102674796 A CN102674796 A CN 102674796A
Authority
CN
China
Prior art keywords
sludge
mud
utilizing
slag
flyash
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011100607434A
Other languages
English (en)
Inventor
高庆祥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2011100607434A priority Critical patent/CN102674796A/zh
Publication of CN102674796A publication Critical patent/CN102674796A/zh
Pending legal-status Critical Current

Abstract

本发明属于污泥的再利用领域,尤其涉及一种利用污泥制造建筑砖的方法,其特征在于:制备该建筑砖的原料组成及重量百分数为:含水率75%~85%的污泥20%~25%、煤矸石55%~60%、以任意配比混合的粉煤灰和炉渣15%~20%,按一定的生产工艺烧制而成。本方法充分利用了污泥含水量大、粘结性高、热值高等特点,利用其含水量大节约了搅拌时的水资源,利用其粘结性高解决了成坯问题,无需增加页岩和粘土等材料,利用其热值高满足建筑砖烧结过程中对热值的需求,节省了能源,通过这种方法对污泥进行废物再利用,保护环境的同时又节省了制砖成本。

Description

利用污泥制造建筑砖的方法
技术领域
本发明涉及一种利用污泥制造建筑砖的方法,属于污泥的再利用领域。
背景技术
近几年来,我国的污水处理工作有了前所未有的发展,污水处理厂在解决我国水污染问题方面起到了巨大的作用,在很大程度上缓解了我国水污染的危机。然而,污水处理厂产生的污泥大量堆放对环境已经造成了很大污染,已经影响到了人们的健康生活,在很大程度上影响了我国污水污染控制的成效,此问题已经引起了社会各界的高度关注,政府各部门和环保界的专家也在采取积极的对策来解决日益严重的污泥污染问题。据统计,2009年全国已建污水处理厂约为2000座,湿污泥产量约为10000万t/a(含水率约为80%),国内外对这些污泥的处理方法多数为填埋,此方法占用大量土地又造成环境的二次污染,已经成为社会公害。只有极少数的企业将污泥烘干后焚烧处理,此方法烘干时浪费大量热能及人工,处理成本非常高,焚烧后产生的炉渣仍然需要处置,此方法等同于把垃圾转化了形态而已,治标不治本。总之,人们采取了各种方式对污泥进行处理,却没有意识到污泥本身所具有的粘结性高、含水量大、热值高等优良特性,也不会利用这些特性对污泥进行废物再利用,因此污泥的再利用问题亟待解决。
发明内容
根据以上现有技术中的不足,本发明要解决的技术问题是:提供一种利用污泥制造建筑砖的方法,这种制砖方法能够充分利用污泥的含水量大、粘结性高、热值高等特点,既对污泥进行废物再利用、保护了环境,又节省了制砖成本。
本发明解决其技术问题所采用的技术方案是:一种利用污泥制造建筑砖的方法,其特征在于:制备该建筑砖的原料组成及重量百分数为:含水率75%~85%的污泥20%~25%、煤矸石55%~60%、以任意配比混合的粉煤灰和炉渣15%~20%,具体步骤如下:
(1)原材料混合:将污泥、煤矸石和粉煤灰、炉渣按比例混合,混合前先将煤矸石、粉煤灰和炉渣进行破碎并陈化,然后将未经任何处理的污泥与煤矸石、粉煤灰、炉渣搅拌混合均匀。搅拌混合时,将污泥经螺旋喂料机送入混合搅拌机进行搅拌,由于污泥水分很大,利用污泥的水分省去了搅拌时应加入的水,因此能够节省能源,通过混合搅拌机搅拌成的混合料经皮带机送入强力搅拌机进行强力搅拌,直至原材料搅拌混合均匀。
(2)成型:将混合料送入挤压机挤压、切坯、成型制成砖坯。由于污泥粘结性大、塑性好,因此不需要增加页岩和粘土等材料就能解决成坯问题,节省了资源,降低了制砖成本。
(3)烧结制成成品:砖坯经窑炉烧结成成品。烧结时,利用污泥中氨、磷等热值就能满足烧结制品对热值的需求,经窑炉烧结成为成品。
整个过程无需对污泥进行烘干,既节省了烘干的热能、搅拌时的水资源,又使污泥中的氨、磷等热值得到充分利用。
本发明所具有的有益效果是:提供一种利用污泥制造建筑砖的方法,充分利用了污泥含水量大、粘结性高、热值高等特点,利用其含水量大节约了搅拌时的水资源,利用其粘结性高解决了成坯问题,无需增加页岩和粘土等材料,利用其热值高满足建筑砖烧结过程中对热值的需求,节省了能源,通过这种方法对污泥进行废物再利用,保护环境的同时又节省了制砖成本。
具体实施方式
下面结合附图对本发明的实施例做进一步描述:
实施例一:制成本实施例建筑砖的原料组成及重量百分数为污泥(含水率80%)20%、煤矸石60%、粉煤灰5%、炉渣15%。
本实施例的制备方法包括以下步骤:
(1)原材料混合:将污泥、煤矸石和粉煤灰、炉渣按比例混合,混合前先将煤矸石、粉煤灰和炉渣进行破碎并陈化,然后将未经任何处理的污泥与煤矸石、粉煤灰、炉渣搅拌混合均匀。
(2)成型:将混合料送入挤压机挤压、切坯、成型制成砖坯。
(3)烧结制成成品:将砖坯送入窑炉内焙烧,最高烧成温度为1000℃,最终烧结成建筑砖。
实施例二:制成本实施例建筑砖的原料组成及重量百分数为污泥(含水率80%)25%、煤矸石58%、粉煤灰10%、炉渣7%。
本实施例的制备方法包括以下步骤:
(1)原材料混合:将污泥、煤矸石和粉煤灰、炉渣按比例混合,混合前先将煤矸石、粉煤灰和炉渣进行破碎并陈化,然后将未经任何处理的污泥与煤矸石、粉煤灰、炉渣搅拌混合均匀。
(2)成型:将混合料送入挤压机挤压、切坯、成型制成砖坯。
(3)烧结制成成品:将砖坯送入窑炉内焙烧,最高烧成温度为1000℃,最终烧结成建筑砖。

Claims (1)

1.一种利用污泥制造建筑砖的方法,其特征在于:制备该建筑砖的原料组成及重量百分数为:含水率75%~85%的污泥20%~25%、煤矸石55%~60%、以任意配比混合的粉煤灰和炉渣15%~20%,具体步骤如下:
(1)原材料混合:将污泥、煤矸石和粉煤灰、炉渣按比例混合,混合前先将煤矸石、粉煤灰和炉渣进行破碎并陈化,然后将未经任何处理的污泥与煤矸石、粉煤灰、炉渣搅拌混合均匀;
(2)成型:将混合料送入挤压机挤压、切坯、成型制成砖坯;
(3)烧结制成成品:砖坯经窑炉烧结成成品。
CN2011100607434A 2011-03-15 2011-03-15 利用污泥制造建筑砖的方法 Pending CN102674796A (zh)