CN102642375A - 一种带有色彩的生态板的成型工艺 - Google Patents

一种带有色彩的生态板的成型工艺 Download PDF

Info

Publication number
CN102642375A
CN102642375A CN2012101575149A CN201210157514A CN102642375A CN 102642375 A CN102642375 A CN 102642375A CN 2012101575149 A CN2012101575149 A CN 2012101575149A CN 201210157514 A CN201210157514 A CN 201210157514A CN 102642375 A CN102642375 A CN 102642375A
Authority
CN
China
Prior art keywords
ecological plate
colors
plate
ecological
color
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012101575149A
Other languages
English (en)
Inventor
纪明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHENJIANG HENGJI WOODEN PRODUCTS CO Ltd
Original Assignee
ZHENJIANG HENGJI WOODEN PRODUCTS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHENJIANG HENGJI WOODEN PRODUCTS CO Ltd filed Critical ZHENJIANG HENGJI WOODEN PRODUCTS CO Ltd
Priority to CN2012101575149A priority Critical patent/CN102642375A/zh
Publication of CN102642375A publication Critical patent/CN102642375A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种带有色彩的生态板的成型工艺,包括以下步骤:将生态板加温至200-210度;将热压机加压至20-25mpa,将印刷有色彩的浸胶纸附在生态板上,热压50-70秒,使其粘贴在生态板上,得到带有色彩的生态板。本发明可将印刷有色彩的浸胶纸牢固地粘贴在生态板上,得到的带有色彩的生态板耐磨,永不褪色,防水,环保性能优异。

Description

一种带有色彩的生态板的成型工艺
技术领域
本发明涉及一种带有色彩的生态板,具体地说是一种带有色彩的生态板的成型工艺。
背景技术
  带有色彩的生态板属于高档装饰材料,在市场的销量不断加大,得到了广泛的应用。
  传统的带有色彩的生态板,表面色彩容易脱落,耐水性、耐磨性、耐热性差。为了在使用时不褪色,还需要在带有色彩的生态板表面再油漆。因此,存在以下缺点:1、加工工艺复杂,能耗大; 2、成本高。
发明内容
为了克服传统彩色生态板存在的问题,本发明的目的是提供一种带有色彩的生态板的成型工艺,该工艺可将印刷有色彩的浸胶纸牢固地粘贴在生态板上,得到的带有色彩的生态板耐磨,永不褪色,防水,环保性能优异。
本发明的目的是通过以下技术方案来实现的:
一种带有色彩的生态板的成型工艺,其特征在于:该工艺包括以下步骤:
1)将生态板加温至200-210度;生态板加温优选为200度。
2)将热压机加压至20-25mpa,将印刷有色彩的浸胶纸附在生态板上,热压50-70秒,使其粘贴在生态板上,得到带有色彩的生态板。优选地,热压机加压至20mpa,热压时间为60秒。
本发明中,所述生态板可以是各种厚度的胶合板或木工板。
   本发明将印刷成各种色彩的浸胶纸附在在各种厚度的胶合板或木工板上,使其粘贴在板上。与现有技术相比,本发明得到的带有色彩的生态板耐磨,无需油漆,永不褪色、脱落,防水,环保性能优异。可用于各种家俱的制作。
具体实施方式
实施例1
一种本发明所述的带有色彩的生态板的成型工艺,该工艺包括以下步骤:
1)将胶合板加温至200度;生态板是木工板。
2)将热压机加压至20mpa,将印刷有色彩的浸胶纸附在生态板上,热压60秒,使其粘贴在生态板上,得到带有色彩的生态板。
实施例2
又一种带有色彩的生态板的成型工艺,该工艺包括以下步骤:
1)将生态板加温至210度;生态板是胶合板。
2)将热压机加压至25mpa,将印刷有色彩的浸胶纸附在生态板上,热压50秒,使其粘贴在生态板上,得到带有色彩的生态板。

Claims (4)

1. 一种带有色彩的生态板的成型工艺,其特征在于:该工艺包括以下步骤:
1)将生态板加温至200-210度;
2)将热压机加压至20-25mpa,将印刷有色彩的浸胶纸附在生态板上,热压50-70秒,使其粘贴在生态板上,得到带有色彩的生态板。
2.根据权利要求1所述的带有色彩的生态板的成型工艺,其特征在于:所述生态板是胶合板或木工板。
3.根据权利要求1所述的带有色彩的生态板的成型工艺,其特征在于:步骤1)中,生态板加温为200度。
4.根据权利要求1所述的带有色彩的生态板的成型工艺,其特征在于:步骤2)中,热压机加压至20mpa,热压时间为60秒。
CN2012101575149A 2012-05-21 2012-05-21 一种带有色彩的生态板的成型工艺 Pending CN102642375A (zh)