CN102543325A - 绝缘子的制备方法 - Google Patents

绝缘子的制备方法 Download PDF

Info

Publication number
CN102543325A
CN102543325A CN2010106118085A CN201010611808A CN102543325A CN 102543325 A CN102543325 A CN 102543325A CN 2010106118085 A CN2010106118085 A CN 2010106118085A CN 201010611808 A CN201010611808 A CN 201010611808A CN 102543325 A CN102543325 A CN 102543325A
Authority
CN
China
Prior art keywords
insulator
processed
demoulding
framework
glass fiber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2010106118085A
Other languages
English (en)
Other versions
CN102543325B (zh
Inventor
张志强
许朝阳
龙洁
史亮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
State Grid Corp of China SGCC
Jiaozuo Power Supply Co of State Grid Henan Electric Power Co Ltd
Original Assignee
Jiaozuo Power Supply Co of Henan Electric Power Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiaozuo Power Supply Co of Henan Electric Power Co filed Critical Jiaozuo Power Supply Co of Henan Electric Power Co
Priority to CN201010611808.5A priority Critical patent/CN102543325B/zh
Publication of CN102543325A publication Critical patent/CN102543325A/zh
Application granted granted Critical
Publication of CN102543325B publication Critical patent/CN102543325B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种绝缘子的制备方法,包括以下步骤:a.将玻璃纤维束制成与绝缘子形状相配合的三维立体骨架,表面是玻璃纤维布,浸润环氧树脂;b.待开始凝固时,在表面均匀涂抹含陶瓷粉或玻璃粉的树脂放入绝缘子模具中;d.加温定型,固化后脱模,制成绝缘子。本发明制成的一体式的绝缘子,省去了将伞裙一个个依次套装在绝缘子芯棒上的工序,节省了人力,而且用此工艺制出的绝缘子,自重小,电气性能和机械性能较好。不管是用此工艺制成的空心绝缘子还是实心绝缘子,均具有较好的电气性能和机械性能,而且自身重量较轻。适合户外高压输电线路的使用。

Description

绝缘子的制备方法
技术领域
本发明属于绝缘子领域,具体的说是涉及一种绝缘子的制备方法。
背景技术
通常户外使用的高压支柱绝缘子一般是瓷棒绝缘子,绝缘子伞裙有瓷伞裙也有玻璃钢伞裙,还有是玻璃伞裙。随着科技水平的不断提高,人们对电站电器设备提出了更高的要求。对于电站用复合支柱绝缘子不仅要求具有较高的绝缘性能及各种电气性能,还要能承受运行中常受到导线的重力和张力、风力、覆冰重量、绝缘子自重、导线振动、设备操作机械力、短路电动力、地震和其他机械力的作用。复合绝缘子是由多片伞裙套设在瓷绝缘芯棒上,瓷绝缘子,表层的机械强度较差,易发生裂缝,从而毁坏绝缘子,而且自重较大。玻璃绝缘子和玻璃钢绝缘子的表层机械强度高,使表面不易发生裂缝,但是自身较重。因此不论是瓷伞裙绝缘子、玻璃伞裙绝缘还是玻璃钢伞裙绝缘子,其自身重量较大,在运行过程中会影响到绝缘子的机械性能,同时还会波及到运行中导线的正常使用。而且目前的绝缘子伞裙是一个个依次套在绝缘子芯棒上,然后用绝缘胶粘接,工艺比较复杂。
发明内容
本发明的目的就在于提供一种制作工艺简单的绝缘子的制备方法,用此方法制出的绝缘子是一体的,且自重大幅降低。
本发明的目的可通过以下技术方案来实现:
一种绝缘子的制备方法,包括以下步骤:
a.将玻璃纤维束制成与绝缘子形状相配合的三维立体骨架,表面是玻璃纤维布,浸润环氧树脂,
b. 待开始凝固时,在表面均匀涂抹含陶瓷粉或玻璃粉的树脂放入绝缘子模具中;
d.加温定型,固化后脱模,制成绝缘子。
上述绝缘子的制备方法,在步骤b后面加一步骤c. 在模具中心插入脱模管;所述步骤d. 加温定型,固化后拔出脱膜管,再脱模,制成空心绝缘子。
上述绝缘子的制作方法,在步骤b后面加一步骤c.在模具中间植入挤压的玻璃钢棒;所述步骤d. 加温定型,玻璃钢棒与绝缘子固化为一体,脱模,制成实心绝缘子。
上述绝缘子的制作方法,所述步骤b的玻璃钢棒的制作方法如下:将玻璃纤维束拧成麻花状,浸润环氧树脂,拉挤成实心绝缘子芯棒。
本发明是用玻璃纤维束制成与绝缘子形状相配合的三维立体骨架,表面是玻璃纤维布,浸润环氧树脂,在模具中固化脱模制成的一体式的绝缘子,省去了将伞裙一个个依次套装在绝缘子芯棒上的工序,节省了人力,而且用此工艺制出的绝缘子,自重小,电气性能和机械性能较好。不管是用此工艺制成的空心绝缘子还是实心绝缘子,均具有较好的电气性能和机械性能,而且自身重量较轻。适合户外高压输电线路的使用。
具体实施方式
实施例1:
空心绝缘子的制备方法,包括以下步骤:
a.将玻璃纤维束制成与绝缘子形状相配合的三维立体骨架,表面是玻璃纤维布,浸润环氧树脂,
b.待开始凝固时,在表面均匀涂抹含陶瓷粉或玻璃粉的树脂放入绝缘子模具中;
c.在模具中心插入脱模管;
d.加温定型,固化后拔出脱膜管,再脱模,制成空心绝缘子。
实施例2:
实心绝缘子的制备方法,包括以下步骤:
a.将玻璃纤维束制成与绝缘子形状相配合的三维立体骨架,表面是玻璃纤维布,浸润环氧树脂,
b.待开始凝固时,在表面均匀涂抹含陶瓷粉或玻璃粉的树脂放入绝缘子模具中;
c. 玻璃钢棒的制作方法:将玻璃纤维束拧成麻花状,浸润环氧树脂,拉挤成实心绝缘子芯棒;
d. 在模具中间植入挤压的玻璃钢棒,加温定型,玻璃钢棒与绝缘子固化为一体,脱模,制成实心绝缘子。

Claims (4)

1.一种绝缘子的制备方法,包括以下步骤:
a.将玻璃纤维束制成与绝缘子形状相配合的三维立体骨架,表面是玻璃纤维布,浸润环氧树脂,
b. 待开始凝固时,在表面均匀涂抹含陶瓷粉或玻璃粉的树脂放入绝缘子模具中;
d.加温定型,固化后脱模,制成绝缘子。
2.根据权利要求1所述的绝缘子的制备方法,其特征在于:在步骤b后面加一步骤c. 在模具中心插入脱模管;所述步骤d. 加温定型,固化后拔出脱膜管,再脱模,制成空心绝缘子。
3.根据权利要求1所述的绝缘子的制作方法,其特征在于:在步骤b后面加一步骤c.在模具中间植入挤压的玻璃钢棒;所述步骤d. 加温定型,玻璃钢棒与绝缘子固化为一体,脱模,制成实心绝缘子。
4.根据权利要求3所述的绝缘子的制作方法,其特征在于:所述步骤b的玻璃钢棒的制作方法如下:将玻璃纤维束拧成麻花状,浸润环氧树脂,拉挤成实心绝缘子芯棒。
CN201010611808.5A 2010-12-29 2010-12-29 绝缘子的制备方法 Active CN102543325B (zh)