CN102533110A - 一种醇水溶性涂料的制备方法 - Google Patents

一种醇水溶性涂料的制备方法 Download PDF

Info

Publication number
CN102533110A
CN102533110A CN201010599138XA CN201010599138A CN102533110A CN 102533110 A CN102533110 A CN 102533110A CN 201010599138X A CN201010599138X A CN 201010599138XA CN 201010599138 A CN201010599138 A CN 201010599138A CN 102533110 A CN102533110 A CN 102533110A
Authority
CN
China
Prior art keywords
preparation
ethanol
water
solvent
soluble
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201010599138XA
Other languages
English (en)
Inventor
邱华东
郭永亮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201010599138XA priority Critical patent/CN102533110A/zh
Publication of CN102533110A publication Critical patent/CN102533110A/zh
Pending legal-status Critical Current

Abstract

一种醇水溶性涂料的制备方法是将乙醇或乙醇与水的混合溶液作为溶剂,加入溶剂质量的5-25%的虫胶片,在10-50℃下搅拌直至溶解,再加入其他的着色物质,加入量溶剂的0.01-0.5%。本发明具有染色力强,透明度高,着色均匀,不用苯、甲苯等有毒溶剂,相对绿色环保,工艺简单的优点。

Description

一种醇水溶性涂料的制备方法
技术领域:
本发明涉及一种醇水溶性涂料的制备方法,属精细化工领域。
技术背景:
目前国内外日常使用的涂料都是能形成坚韧连续涂膜(漆膜)的液体或固体高分子材料。旧称油漆、漆。主要用来对被涂表面起到装饰与保护作用。由成膜物质(即基料)、颜料、填料、涂料助剂、功能组分、有机溶剂或水组成。中国按涂料组成中成膜物质的种类不同,将涂料及其辅料分为18类,如油脂漆、天然树脂漆、酚醛树脂漆、沥青漆、醇酸树脂漆、氨基树脂漆、硝酸纤维素漆、纤维素酯漆、过氯乙烯漆、乙烯基树脂漆、丙烯酸酯漆、聚酯漆、环氧树脂漆、聚氨酯漆等,这些油漆的主要成分都是合成高分子,涂刷前,需要用有机溶剂溶解才能使用。由于有机溶剂要求既能分散高分子材料,又不与涂料里的其他成分发生反应,还有挥发性好,所以,大多涂料都使用苯作为涂料的溶剂。苯是一种无色具有特殊芳香气味的液体,对人体的伤害严重,所以专家们把它称为“芳香杀手”。
发明内容
本发明提供一种醇水溶性涂料的制备方法。
主要是采用乙醇和虫胶片作为原料,可以加入一些染料或颜料,简单混合而成。
具体操作步骤如下:
称量一定量的乙醇或乙醇与水的混合溶液作为溶剂,加入溶剂质量的5-25%的虫胶片,在10-50℃下搅拌直至溶解,再加入其他的着色物质,加入量溶剂的0.01-0.5%。
如上所述,乙醇与水的混合溶液是指V乙醇∶V=1∶1-99∶1的混合液。
如上所述油漆主要用于木器的涂料。
本发明的优点是染色力强,透明度高,着色均匀,不用苯、甲苯等有毒溶剂,相对绿色环保,工艺简单。
具体实施方式
实施例1
取95%的乙醇200g,加入25%的虫胶片,在50℃下,搅拌溶解,再加入0.02g的靛青,搅拌溶解,即制得成品。
实施例2
取50%(v/v)的乙醇200g,加入5%的虫胶片,在10℃下,搅拌溶解,再加入0.2g的铁红,搅拌溶解,即制得成品。
实施例3
取无水乙醇200g,加入15%的虫胶片,在20℃下,搅拌溶解,再加入0.6%的钛白,搅拌溶解,即制得成品。
实施例4
取75%的乙醇200g,加入10%的虫胶片,在30℃下,搅拌溶解,再加入1g的靛青,搅拌溶解,即制得成品。

Claims (2)

1.一种醇水溶性涂料的制备方法,其特征在于包括如下步骤:
将乙醇或乙醇与水的混合溶液作为溶剂,加入溶剂质量的5-25%的虫胶片,在10-50℃下搅拌直至溶解,再加入其他的着色物质,加入量溶剂的0.01-0.5%。
2.如权利要求1所述的一种醇水溶性涂料的制备方法,其特征在于所述的乙醇与水的混合溶液是V乙醇∶V=1∶1-99∶1的混合液。
CN201010599138XA 2010-12-14 2010-12-14 一种醇水溶性涂料的制备方法 Pending CN102533110A (zh)