CN102261538B - 煤气管道波纹补偿器在线修复方法 - Google Patents

煤气管道波纹补偿器在线修复方法 Download PDF

Info

Publication number
CN102261538B
CN102261538B CN 201110208858 CN201110208858A CN102261538B CN 102261538 B CN102261538 B CN 102261538B CN 201110208858 CN201110208858 CN 201110208858 CN 201110208858 A CN201110208858 A CN 201110208858A CN 102261538 B CN102261538 B CN 102261538B
Authority
CN
China
Prior art keywords
compensator
old
nitrogen
repair
new
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201110208858
Other languages
English (en)
Other versions
CN102261538A (zh
Inventor
刘学慧
辜庆九
李月明
王瑞红
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanxi Taigang Stainless Steel Co Ltd
Original Assignee
Shanxi Taigang Stainless Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanxi Taigang Stainless Steel Co Ltd filed Critical Shanxi Taigang Stainless Steel Co Ltd
Priority to CN 201110208858 priority Critical patent/CN102261538B/zh
Publication of CN102261538A publication Critical patent/CN102261538A/zh
Application granted granted Critical
Publication of CN102261538B publication Critical patent/CN102261538B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种煤气管道波纹补偿器在线修复方法,主要用于煤气架空管道上波纹补偿器的修复,其步骤包括:(1)、先将补偿器漏点进行堵漏;(2)、选择形状及波数与旧补偿器相同但直径比旧补偿器的直径大200mm的新补偿器,将新补偿器平均切割成八块补料。在其中一块补料的外侧靠近切口处的波峰处焊接一放散管,高出此波峰2m。(3)、到现场将八块补料进行拼接且套装在旧补偿器的外围,带有放散管的一块补料套装在原有补偿器的最上侧(保证放散管处于竖直状态)。采用连续焊缝焊接,焊接时往新补偿器的腔内通入氮气,氮气的压力是0.6MPa,流量根据所接氮气的管径定,将焦炉煤气赶出。本发明不会造成管道停运影响生产。

Description

煤气管道波纹补偿器在线修复方法
技术领域
 本发明主要用于煤气架空管道上波纹补偿器的修复,具体涉及一种管道波纹补偿器在线修复方法。
背景技术
波纹补偿器属于一种补偿元件。利用其工作主体波纹管的有效伸缩变形,以吸收管线由热胀冷缩、蠕动等原因而产生的尺寸变化。
目前,钢铁企业所用的煤气管道、压缩空气管道都设有补偿器。由于管道内介质随环境变化而发生变化,会引起管道的伸缩,补偿器经过长时间使用,会出现补偿器损坏或腐蚀出现沙眼,如果泄漏煤气危害极大,因此,及时修复或更换补偿器意义重大。
发明内容
为了防止因生产需要无法及时更换泄漏煤气补偿器引起人员伤亡等事故的发生,本发明提出在保证管道安全运行的情况下快速修复补偿器的一种管道补偿器在线修复方法。
本发明包括下述步骤:
(1)、先将补偿器漏点用木钉或抹黄泥进行堵漏;
(2)、选择形状及波数与旧波纹补偿器相同但直径比旧补偿器的直径大200 mm的新补偿器,将新补偿器平均切割成八块补料。在其中一块补料的外侧靠近切口处的波峰处焊接一放散管,高出此波峰2m。
(3)、到现场将八块补料进行拼接且套装在旧补偿器的外围,带有放散管的一块补料套装在原有补偿器的最上侧(保证放散管处于竖直状态)。采用连续焊缝焊接,焊接时往新补偿器的腔内通入氮气,氮气的压力是0.6MPa,流量根据所接氮气的管径定,将焦炉煤气赶出。
本发明的有益效果:
1、能够在线修复补偿器,不会造成管道停运影响生产,保证补偿器能够起到伸缩补偿作用;
2、新套装补偿器分八半套装,在对接过程中往新旧补偿器中的空腔内充入氮气防止煤气中毒及着火爆炸事故的发生;
3、新补偿器上加放散管,防止形成死空间而引起着火爆炸或氮气窒息,保证了施工人员的安全。
具体实施方式:
实施例:本实施例为山西太钢不锈钢股份有限公司能源动力总厂输配作业区五高炉DN2800插板阀前补偿器进行修复。
1、当发现补偿器出现腐蚀泄漏时,先将漏点用木钉进行堵漏,或抹黄泥进行堵漏。
2、按照需修复的补偿器形状及波数(五高炉DN2800插板阀前补偿器波数为2波),选择直径为3000mm的新补偿器,将新补偿器平均切割成八块补料,在其中一块补料的外侧靠近切口处的波峰处焊接一放散管,高出此波峰2m。 
3、到现场将八块补料进行拼接且套装在旧补偿器的外围,带有放散管的一块补料套装在原有补偿器的最上侧(保证放散管处于竖直状态)。采用连续焊缝焊接,焊接时往新补偿器的腔内通入氮气,氮气的压力是0.6MPa,流量根据所接氮气的管径定,将焦炉煤气赶出。防止形成死空间而引起着火爆炸或氮气窒息。

Claims (1)

1.一种煤气管道波纹补偿器在线修复方法,其步骤包括:
(1)、先将补偿器漏点进行堵漏;
(2)、选择形状及波数与旧补偿器相同但直径比旧补偿器的直径大200 mm的新补偿器,将新补偿器平均切割成八块补料;
在其中一块补料的外侧靠近切口处的波峰处焊接一放散管,高出此波峰2m;   
(3)、到现场将八块补料进行拼接且套装在旧补偿器的外围,带有放散管的一块补料套装在旧补偿器的最上侧,保证放散管处于竖直状态;
采用连续焊缝焊接,焊接时往新补偿器的腔内通入氮气,氮气的压力是0.6MPa,流量根据所接氮气的管径定,将焦炉煤气赶出。
CN 201110208858 2011-07-25 2011-07-25 煤气管道波纹补偿器在线修复方法 Expired - Fee Related CN102261538B (zh)