CN102230261A - Method and device for reducing cashmere balling broken ends - Google Patents

Method and device for reducing cashmere balling broken ends Download PDF

Info

Publication number
CN102230261A
CN102230261A CN 201110165404 CN201110165404A CN102230261A CN 102230261 A CN102230261 A CN 102230261A CN 201110165404 CN201110165404 CN 201110165404 CN 201110165404 A CN201110165404 A CN 201110165404A CN 102230261 A CN102230261 A CN 102230261A
Authority
CN
China
Prior art keywords
cashmere
balling
cylinder
cashmere bar
spray
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 201110165404
Other languages
Chinese (zh)
Other versions
CN102230261B (en
Inventor
王强
商显芹
秦光
陈振
李连锋
王彦兰
李春霞
刘杰
种军
仇超
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shandong Jining Ruyi Woolen Textile Co Ltd
Original Assignee
Shandong Jining Ruyi Woolen Textile Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shandong Jining Ruyi Woolen Textile Co Ltd filed Critical Shandong Jining Ruyi Woolen Textile Co Ltd
Priority to CN 201110165404 priority Critical patent/CN102230261B/en
Publication of CN102230261A publication Critical patent/CN102230261A/en
Application granted granted Critical
Publication of CN102230261B publication Critical patent/CN102230261B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention provides a method and device for reducing cashmere balling broken ends. The method comprises the processing steps of: drying cashmere bars in a drying room after cleaning in a water tank; directly winding the dried cashmere bars on balling rollers; setting material spray nozzles above the balling rollers; evenly spraying material spray liquid containing an antistatic agent and a softening agent on the cashmere bars through the nozzles in the process of winding the cashmeres to drums; and forming the cashmeres into semi-finished products by fully winding on the drums and putting in a warehouse for later use, wherein the drying temperature of the drying room is controlled within 85-90 DEG C; and the drying time is about 4 minutes; the material spray liquid is composed of the antistatic agent (s-10), the softening agent (zk-38) and water in the batching ratio of 10: 1: 50; the preparation step is to add the antistatic agent and the softening agent in the water by the ratio for evenly mixing; the spray atomization degree and the atomization flow are kept in 1-2 litres/minute, or are subjected to the case that no liquid drops when the cashmere bars are wound on the drums.

Description

A kind of method and device thereof that reduces cashmere balling-up broken end
Technical field
The present invention relates to the method that breaks end in a kind of cashmere bar balling-up process that reduces after reinforced, the oven dry,, reduce the broken end in the cashmere bar balling-up process specifically by changing cashmere bar feed way.
Technical background
Cashmere fiber is enjoyed the great reputation of " fiber jewel " with its light, gentle, soft, sliding, glutinous characteristic.Its made cashmere product of while has comfortable and easy to wear, and warmth retention property is strong, and soft, sliding glutinous, the individual style that gloss is soft is subjected to consumer's favor deeply.
Conventional method, cashmere bar needed before balling-up through after backwashing groove, hopper and baking oven, and what wherein hopper added is the mixing material that closes crude oil+antistatic additive, and baking oven mainly plays the hyperthermia drying effect.
Yet because cashmere is descending through brute force after containing the hopper that closes crude oil+antistatic additive, through the oven dry of high temperature oven, cashmere bar brute force descends bigger again, makes the cashmere bar very many at broken end in balling-up roller balling-up process, influences its balling-up quality.
Summary of the invention
The objective of the invention is to change the first balling-up pre-treatment mode of feeding in raw material and afterwards drying,, make the balling-up pre-treatment become first the oven dry afterwards and feed in raw material, effectively reduce the end breakage rate of cashmere bar balling-up process, improve the quality by a kind of automatic material spray technology and device.
The technical scheme of automatic material-spraying device of the present invention realizes in the following manner: treatment step is as follows: the cashmere bar is after tank cleans, enter the drying room oven dry, cashmere bar after the oven dry, directly be wrapped on the balling-up roller, the top of balling-up roller is provided with the material spray shower nozzle, the material spray liquid that contains antistatic additive and softener sprays on the cashmere bar in the process that cylinder is reeled at the cashmere bar equably through shower nozzle, and the cashmere bar becomes the semi-finished product warehouse-in after being rolled up on the cylinder standby;
The drying room bake out temperature is controlled at 85-90 ℃, about 4 minutes of drying time;
Material spray liquid by: antistatic additive (s-10), softener (zk-38) and water are formed, and charge ratio=10: 1: 50, preparation process are that antistatic additive and softener add in proportion to stir in the entry and get final product;
The spray degree of atomization: the atomizing flow remain on the 1-2 liter/minute or when on cylinder, reeling with the cashmere bar no liquid drip and be as the criterion.
Reduce the treating apparatus of cashmere balling-up broken end, comprise, pending cashmere bar cylinder, rinse bath, baking room, cashmere bar spray cylinder and spray equipment, pending cashmere bar cylinder, rinse bath, baking room, cashmere bar spray cylinder are chained together by the cashmere bar; Spray equipment is made up of spice bucket, pressure regulating pump and shower nozzle, and the spice bucket is connected with pressure regulating pump by pipeline, and pressure regulating pump is connected with shower nozzle by pipeline, and shower nozzle is positioned at the top of cashmere bar spray cylinder, and material spray liquid is stored in the spice bucket.
Excellent effect of the present invention: change traditional back washer through the reinforced mode of advancing the drying room oven dry then of hopper, adopt the cashmere bar after tank cleans, directly enter the drying room oven dry, the cashmere bar after the oven dry is carrying out material spray in balling-up roller winding process.Avoided the cashmere bar bar that breaks, made the uniform and stable of cashmere bar oil-containing behind the spray and antistatic additive.Cashmere bar storage means after the balling-up is identical with the cashmere bar of conventional method balling-up, and promptly storage got final product in 24 hours under certain humiture.Concrete advantage is as follows:
(1) realized the cashmere bar automatic spray after the oven dry is closed crude oil+antistatic additive mixing material, this device can be by regulating compression pump control sprinkling amount, uniform and stable, powerful good advantage.
(2) the reinforced earlier finish that causes through the high temperature of baking oven again of traditional approach and the physics and the chemical change of antistatic additive have been avoided;
(3) process equipment have simple in structure, easy to operate, use flexible etc.
(4) Pen Lin mixing material can be the mixing material that closes crude oil+antistatic additive, also the mixing material of softener+antistatic additive etc.
Description of drawings
Fig. 1 reduces cashmere balling-up broken end treatment facility structural representation.
Description of reference numerals: pending cashmere bar cylinder 1, rinse bath 2, baking room 3, cashmere bar spray cylinder 4, shower nozzle 5, pressure regulating pump 6, spice bucket 7.
The specific embodiment
Below in conjunction with accompanying drawing reduction cashmere balling-up broken end method of the present invention and treatment facility thereof are described in further detail.
Reduction cashmere balling-up broken end method of the present invention, concrete treatment step is as follows: the cashmere bar is after tank cleans, enter the drying room oven dry, cashmere bar after the oven dry, directly be wrapped on the balling-up roller, the top of balling-up roller is provided with the material spray shower nozzle, and the material spray liquid that contains antistatic additive and softener sprays on the cashmere bar in the process that cylinder is reeled at the cashmere bar equably through shower nozzle, and the cashmere bar becomes the semi-finished product warehouse-in after being rolled up on the cylinder standby;
The drying room bake out temperature is controlled at 85-90 ℃, the about 3-4 of drying time minute;
Material spray liquid by: antistatic additive (s-10), softener (zk-38) and water are formed, and charge ratio=10: 1: 50, preparation process are that antistatic additive and softener add in proportion to stir in the entry and get final product;
The spray degree of atomization: the atomizing flow remain on the 1-2 liter/minute or when on cylinder, reeling with the cashmere bar no liquid drip and be as the criterion.
Reduce the treating apparatus of cashmere balling-up broken end, comprise, pending cashmere bar cylinder 1, rinse bath 2, baking room 3, cashmere bar spray cylinder 4 and spray equipment, pending cashmere bar cylinder 1, rinse bath 2, baking room 3, cashmere bar spray cylinder 4 are chained together by the cashmere bar; Spray equipment is made up of spice bucket 7, pressure regulating pump 6 and shower nozzle 5, and spice bucket 7 is connected with pressure regulating pump 6 by pipeline, and pressure regulating pump 6 is connected with shower nozzle 5 by pipeline, and shower nozzle 5 is positioned at the top of cashmere bar spray cylinder 4, and material spray liquid is stored in the spice bucket 7.
Embodiment
Concrete treatment step is as follows: the cashmere bar is after tank cleans, enter the drying room oven dry, cashmere bar after the oven dry, directly be wrapped on the balling-up roller, the top of balling-up roller is provided with the material spray shower nozzle, the material spray liquid that contains antistatic additive and softener sprays on the cashmere bar in the process that cylinder is reeled at the cashmere bar equably through shower nozzle, and the cashmere bar becomes the semi-finished product warehouse-in after being rolled up on the cylinder standby;
The drying room bake out temperature is controlled at 85-90 ℃, the about 3-4 of drying time minute;
Material spray liquid by: antistatic additive (s-10), softener (zk-38) and water are formed, and charge ratio=10: 1: 50, preparation process are that antistatic additive and softener add in proportion to stir in the entry and get final product;
The spray degree of atomization: the atomizing flow remain on the 1-2 liter/minute or when on cylinder, reeling with the cashmere bar no liquid drip and be as the criterion.
Material spray liquid for preparing in the antistatic additive mixing drum by the effect of mixer, makes mixing material even.By regulating the effect of compression pump, make the vaporific mixing material of shower nozzle ejection, the balling-up roller makes each layer of cashmere bar all be sprayed mixed liquor uniformly by constantly rotating.
Regulate compression pump and be mainly used to regulate expulsion pressure, i.e. emitted dose; Cut to go up valve and play the folding effect, whether the control shower nozzle hydrojet; Pipeline valve plays the folding effect to whole pipe, plays the effect of blocking when maintenance compression pump, motor and other need.
Except that the disclosed technical characterictic of specification of the present invention, be the public office technology of those skilled in the art.

Claims (2)

1. method that reduces cashmere balling-up broken end side, it is characterized in that, treatment step is as follows: the cashmere bar is after tank cleans, enter the drying room oven dry, cashmere bar after the oven dry directly is wrapped on the balling-up roller, and the top of balling-up roller is provided with the material spray shower nozzle, the material spray liquid that contains antistatic additive and softener sprays on the cashmere bar in the process that cylinder is reeled at the cashmere bar equably through shower nozzle, and the cashmere bar becomes the semi-finished product warehouse-in after being rolled up on the cylinder standby;
The drying room bake out temperature is controlled at 85-90 ℃, about 4 minutes of drying time;
Material spray liquid by: antistatic additive (s-10), softener (zk-38) and water are formed, and charge ratio=10: 1: 50, preparation process are that antistatic additive and softener add in proportion to stir in the entry and get final product;
The spray degree of atomization: the atomizing flow remain on the 1-2 liter/minute or when on cylinder, reeling with the cashmere bar no liquid drip and be as the criterion.
2. one kind is reduced the treating apparatus that the cashmere balling-up is breaked end, it is characterized in that comprising, pending cashmere bar cylinder, rinse bath, baking room, cashmere bar spray cylinder and spray equipment, pending cashmere bar cylinder, rinse bath, baking room, cashmere bar spray cylinder are chained together by the cashmere bar; Spray equipment is made up of spice bucket, pressure regulating pump and shower nozzle, and the spice bucket is connected with pressure regulating pump by pipeline, and pressure regulating pump is connected with shower nozzle by pipeline, and shower nozzle is positioned at the top of cashmere bar spray cylinder, and material spray liquid is stored in the spice bucket.
CN 201110165404 2011-06-20 2011-06-20 Method and device for reducing cashmere balling broken ends Active CN102230261B (en)