CN102229178A - Method for making environment-friendly attapulgite ash tray rough blank - Google Patents

Method for making environment-friendly attapulgite ash tray rough blank Download PDF

Info

Publication number
CN102229178A
CN102229178A CN2011100998688A CN201110099868A CN102229178A CN 102229178 A CN102229178 A CN 102229178A CN 2011100998688 A CN2011100998688 A CN 2011100998688A CN 201110099868 A CN201110099868 A CN 201110099868A CN 102229178 A CN102229178 A CN 102229178A
Authority
CN
China
Prior art keywords
acidifying
attapulgite
millimeters
controlled
convex
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2011100998688A
Other languages
Chinese (zh)
Other versions
CN102229178B (en
Inventor
许庆华
柏正基
许盛英
林光霞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU DUKE NEW ENERGY AUTOMOBILE CO., LTD.
Original Assignee
许庆华
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 许庆华 filed Critical 许庆华
Priority to CN 201110099868 priority Critical patent/CN102229178B/en
Publication of CN102229178A publication Critical patent/CN102229178A/en
Application granted granted Critical
Publication of CN102229178B publication Critical patent/CN102229178B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a method for making an environment-friendly attapulgite ash tray rough blank. The technical scheme is characterized in that the environment-friendly attapulgite ash tray rough blank is made by attapulgite clay having a function for purifying air, the lower part of the rough blank is provided with a bowl-shaped object, two cigarette extinguishing columns and cigarette extinguishing holes are arranged in the bowl-shaped object, a semi-circular groove is arranged on the edge of the upper plane, the upper part of the rough blank is provided with a hollow hemispheric object, and the front of the hemispheric object is provided with an open arc-shaped groove. The environment-friendly attapulgite ash tray rough blank is made into an environment-friendly attapulgite ash tray through the procedures of nature drying, slow baking, middle-temperature sintering, middle and high temperature sintering, cooling, grinding and putting of a stainless steel wire net. The environment-friendly attapulgite ash tray can effectively adsorb harmful gases produced when cigarettes burn, extinguished cigarettes and ash fall below the stainless steel wire net, the ash cannot freely drift, and the pollution to air is reduced. The method is suitable for making the rough blank of the environment-friendly attapulgite ash tray with the function for purifying air.

Description

The preparation method of attapulgite environmental-friendly ashtray crude green body
Technical field
The present invention relates to environment-friendly materials, be specifically related to a kind of preparation method of attapulgite environmental-friendly ashtray crude green body.
Background technology
Ashtray is an instrument of containing cigarette ash, stub, with make pottery, porcelain is for seeing more, also has with glass or metal material making, its shape, size all do not have fixing, but all bear obvious signs, that is exactly all to have several roads cigarette to prop up the groove of thickness on the ashtray, aims to place cigarette and design.
The ashtray of some environment-friendly type absorbs pernicious gas by the filtration of active carbon (net), and adding a cover ashtray is that stub is put into cylinder, Fireproof ashtray, and the cigarette that is used on the ashtray limit is flame-out, but complex structure uses inconvenient.
Without any blocking, pernicious gas and cigarette ash meeting freedom are drift about everywhere, directly have influence on indoor environment and air mostly for existing ashtray.
Summary of the invention
The objective of the invention is to overcome weak point in the prior art, a kind of preparation method of attapulgite environmental-friendly ashtray crude green body is provided.
The preparation method of attapulgite environmental-friendly ashtray crude green body is: be made into attapulgite environmental-friendly ashtray crude green body with the concavo-convex excellent pottery mud with air purification function, the bottom of crude green body is a bowl-shape object, two the go out column of smoke and extinguishing holes are arranged in the bowl-shape object, the semi arch groove is arranged on the last horizontal edge, the top of crude green body is a hollow hemispherical object, and the front of hemispherical object is a unlimited circular groove.
Concavo-convex excellent pottery mud with air purification function is made up of paste attapulgite clay, attapulite constant humidity amendment, natural-minerals adsorptive filter medium, cacumen biotae, alumina silicate fibre, polyacrylamide and water.
Described paste attapulgite clay is to use concavo-convex excellent ore pul making production technology, the screening of mineral such as the hydromica in the Concave-convex clay rod, quartz, opal and carbonate is got rid of, obtain a kind of paste attapulgite clay, paste attapulgite clay is through powerful stirring at a high speed, become the special good natural gelinite of a kind of thixotropy and gumminess, viscosity is up to more than the 10000mPas, help the bonding between the raw material, have the characteristics of ultrafine dust, friction little, the no sand feeling of hardness and soft fine and smooth free from extraneous odour.The dry after-contraction of paste attapulgite clay is little, does not produce be full of cracks, and has good, the high temperature resistant and anti-good properties such as saline and alkaline of thixotropy.
Rice hulls, quick dissolved sodium silicate and the zeolite powder of attapulite constant humidity amendment after by Concave-convex clay rod, montmorillonite, acidifying formed.Attapulite constant humidity amendment not only hydroscopicity is good, and after ambient humidity descends, has been adsorbed on the moisture in its duct, will outwards discharge slowly, remains a more stable hydroscopicity, is a kind of constant humidity conditioner of superior performance.Harmful substances such as formaldehyde, ammonia and benzene reduce the infringement healthy to people in the effective absorbed air of attapulite constant humidity amendment energy.
Zeolite, Concave-convex clay rod acidifying after, bentonite acidifying after, diatomite acidifying after, volcanic rock and the alumine of the batching of natural-minerals adsorptive filter medium after by acidifying formed.The natural-minerals adsorptive filter medium particle surface is coarse, and there is a large amount of micropores inside, has light specific gravity, specific area is big and absorption property is good characteristics.
Cacumen biotae is spray and the leaf of Cupressaceae plant arbor-vitae, and summer, autumn gather, and the clip sprig is dried.The cacumen biotae multi-branched, sprig is flat, and the tiny flakey of leaf alternately to life, is pasted and is lied prostrate on branch, bottle green or yellow green, matter is crisp, frangibility, gas delicate fragrance, bitter and puckery flavor, little suffering.It is the charred CACUMEN PLATYCLADI that cacumen biotae is generated pitchy after anoxycausis that cacumen biotae is used for the present invention, has the characteristic of active carbon, has not only increased the porosity of pottery mud product, has also improved the adsorption capacity of pottery mud product.
Alumina silicate fibre is ceramic fibre again, and this material has that thermal capacitance is little, fiber long, in light weight, characteristics such as tensile strength big, the slag ball is few, heat endurance is high, anti-erosion and sound absorption qualities are good.Be used for cracking and improving when the present invention helps avoiding making crude green body the intensity of pottery mud product.
Polyacrylamide has good water-solubility and thickening property, the plasticity when being used for the present invention and helping improving pottery mud and make crude green body.
The present invention is achieved by following technical proposals:
1, the preparation method of attapulgite environmental-friendly ashtray crude green body: (1) is made into attapulgite environmental-friendly ashtray crude green body with the concavo-convex excellent pottery mud with air purification function, the bottom of crude green body is a bowl-shape object, the upper diameter of bowl-shape object is controlled at 80~150 millimeters, highly be controlled at 35~65 millimeters, the base plate of a sealing is arranged at the bottom in the bowl-shape object, the diameter of base plate is controlled at 40~80 millimeters, design has two columns of smoke that go out on the floor level center line, going out, the diameter on plane is controlled at 14~24 millimeters on the column of smoke, the diameter of column of smoke lower plane of going out is controlled at 16~26 millimeters, there is an extinguishing hole at the column of smoke center of going out, the diameter of extinguishing hole is controlled at 6~10 millimeters, designing respectively on the last horizontal edge of bowl-shape object has 3 semi arch grooves, and the diameter of semi arch groove is controlled at 8~12 millimeters; The top of crude green body is a hollow hemispherical object, and the diameter of hemispherical object is identical with the upper diameter of bowl-shape object, and the front of hemispherical object is designed to a unlimited circular groove, and the radius of circular groove is controlled at 25~50 millimeters.
Described production method with concavo-convex excellent pottery mud of air purification function is: (1) will have after the batch mixes of concavo-convex excellent pottery mud of air purification function and stir in the input mixer; (2) carry out wet ball grinding in the mixture after being mixed input ball mill, the grain fineness of ball milling disposed slurry is less than 0.044 millimeter; (3) will carry out the old semi-finished product that are treated in the input of the slurry behind the ball milling sedimentation basin, half-finished water content is less than 45%, and the old time was controlled at 3~30 days; (4) semi-finished product are imported in the vacuum-extruder extruding and cut into rectangular block, the thickness of the block thing of rectangle is less than 50 millimeters, for having the concavo-convex excellent pottery mud of air purification function;
Batching with concavo-convex excellent pottery mud of air purification function is made up of following component by weight percentage: paste attapulgite clay 45~75%, attapulite constant humidity amendment 5~30%, natural-minerals adsorptive filter medium 5~15%, cacumen biotae 2~10%, alumina silicate fibre 1~5%, polyacrylamide 0.1~3% and water 1~35%.
Concavo-convex excellent pottery mud with air purification function has been applied for patent of invention by the applicant on February 25th, 2011, and number of patent application is: 201110044982.0.
The production technology of described paste attapulgite clay: will stir in the concavo-convex excellent ore deposit input mixer, after extruder is squeezed into sheet, import once more in the mixer and stir, natural drying after extruder is squeezed into sheet, the concavo-convex excellent ore deposit of drying is transported in the feed reservoir soaks, dash with air pump and to turn over, post precipitation is emitted immersion water, the sieve decontamination in the input semi-finished product pond, is soaked again, dash with air pump and to turn over, post precipitation is emitted immersion water, and the slurry transportation of post precipitation is arrived in the finished product pond, is paste attapulgite clay.
Described paste attapulgite clay is made up of following component by weight percentage: Concave-convex clay rod 25~60%, water 40~75%.
This production technology is to adopt " the concavo-convex excellent ore pul making production technology " in application on January 6th, 2004 by the inventor, and the Chinese patent Granted publication number is: CN1287965C, Granted publication day: on December 6th, 2006.
Rice hulls, quick dissolved sodium silicate and the zeolite powder of described attapulite constant humidity amendment after by Concave-convex clay rod, montmorillonite, acidifying formed; The production method of attapulite constant humidity amendment is: the rice hulls after the acidifying and Concave-convex clay rod and montmorillonite are mixed by batching, extrusion modification slabbing mixture, abrasive dust after airing mixes by batching with quick dissolved sodium silicate and zeolite powder and is attapulite constant humidity amendment;
The batching of attapulite constant humidity amendment is made up of following component by weight percentage: the semi-finished product 55~90% of attapulite constant humidity amendment, quick dissolved sodium silicate 2~8% and zeolite powder 5~40%; The half-finished batching of attapulite constant humidity amendment is made up of following component: the rice hulls 5~15% after the acidifying, Concave-convex clay rod 35~55%, montmorillonite 5~15% and water 35~55% by weight percentage;
Aforementioned production method is to adopt " production method of attapulite constant humidity amendment " in application on August 30th, 2007 by the inventor, and the Chinese patent Granted publication number is: CN100528337C, Granted publication day: on August 19th, 2009.
Zeolite, Concave-convex clay rod acidifying after, bentonite acidifying after, diatomite acidifying after, volcanic rock and the alumine of the batching of described natural-minerals adsorptive filter medium after by acidifying formed; The preparation method of natural-minerals adsorptive filter medium is: is natural-minerals adsorptive filter medium with the batching of natural-minerals adsorptive filter medium through mixing, pulverize, sieving.
The batching of natural-minerals adsorptive filter medium is made up of following component by weight percentage: the zeolite 15~35% after the acidifying, the Concave-convex clay rod 15~35% after the acidifying, the bentonite 15~25% after the acidifying, the diatomite 10~20% after the acidifying, volcanic rock 5~10% and alumine 5~10%.
Natural-minerals adsorptive filter medium adopts " natural-minerals adsorptive filter medium " in application on May 30th, 2006 by the inventor, and the Chinese patent Granted publication number is: CN100502999C, Granted publication day: on June 24th, 2009.
The present invention is applicable to the crude green body of making the attapulgite environmental-friendly ashtray with air purification function.
Attapulgite environmental-friendly ashtray crude green body through air dry, slowly oven dry, middle temperature are burnt till, middle high temperature burns till, cools off, polish and places behind the stainless steel steel wire is the attapulgite environmental-friendly ashtray.
Using method: after smoker's smoking, cigarette can be placed directly in the semi arch groove, the centre bore of one end of cigarette burning stainless steel steel wire in the attapulgite environmental-friendly ashtray, the cigarette ash that produces from an end of cigarette burning can directly fall into below the attapulgite environmental-friendly ashtray stainless steel steel wire; After the smoker sucked cigarette, the end with the cigarette burning directly inserted in the extinguishing hole of attapulgite environmental-friendly ashtray earlier, and the cigarette after will extinguishing again takes out, and puts into attapulgite environmental-friendly ashtray inside from stainless steel steel wire centre bore; During cleaning attapulgite environmental-friendly ashtray, elder generation takes out the stainless steel steel wire, and pours out cigarette and cigarette ash after extinguishing, again with standby behind the attapulgite environmental-friendly ashtray scrub.
The pernicious gas that the attapulgite environmental-friendly ashtray produces in the time of effectively adsorbing the cigarette burning, when cigarette is put into flue gas that the attapulgite environmental-friendly ashtray produced and is risen, flue gas can produce turning down in hollow hemispherical object, the pernicious gas that produces in the time of obstructing the cigarette burning overflows fast, helps improving the efficient of attapulgite environmental-friendly ashtray absorption pernicious gas; Cigarette after extinguishing and cigarette ash are below the stainless steel steel wire, and it is drift about everywhere that cigarette ash can freedom, reduce the pollution to air.
There are a large amount of micropores and active carbon in attapulgite environmental-friendly ashtray inside; the function that not only has drier; effective harmful substances such as formaldehyde, ammonia and benzene in the absorbed air; protection environment and enhancement people's is healthy; the attapulgite environmental-friendly ashtray is elegant in appearance, and being placed on indoor is again a handicraft.
Description of drawings
Fig. 1 is the schematic diagram of attapulgite environmental-friendly ashtray crude green body, Fig. 2 be the A of Fig. 1 to view, Fig. 3 is that the B-B of Fig. 1 is to view.
As shown in the figure: the 1st, crude green body, the 2nd, hemispherical object, the 3rd, extinguishing hole, the 4th, the column of smoke that goes out, the 5th, semi arch groove, the 6th, ashtray inside, the 7th, semi arch groove, the 8th, cigarette, the 9th, semi arch groove, the 10th, stainless steel steel wire, the 11st, bowl-shape object, the 12nd, circular groove, the 13rd, cigarette, the 14th, cigarette after extinguishing and cigarette ash, the 15th, base plate, the 16th, centre bore.
The specific embodiment
The invention will be further described below in conjunction with embodiment:
1, the preparation method of attapulgite environmental-friendly ashtray crude green body: (1) is made into attapulgite environmental-friendly ashtray crude green body 1 with the concavo-convex excellent pottery mud with air purification function, the bottom of crude green body 1 is a bowl-shape object 11, the upper diameter of bowl-shape object 11 is controlled at 100 millimeters, highly be controlled at 45 millimeters, the base plate 15 of a sealing is arranged at the bottom in the bowl-shape object 11, the diameter of base plate 15 is controlled at 42 millimeters, design has two columns of smoke 4 that go out on base plate 15 horizontal center lines, going out, the diameter on plane is controlled at 16 millimeters on the column of smoke 4, the diameter of the column of smoke 4 lower planes of going out is controlled at 20 millimeters, there is an extinguishing hole 3 at the column of smoke 4 centers of going out, the diameter of extinguishing hole 3 is controlled at 7.5 millimeters, design respectively on the last horizontal edge of bowl-shape object 11 3 semi arch grooves 5 are arranged, 7 and 9, the diameter of semi arch groove is controlled at 10 millimeters; The top of crude green body 1 is a hollow hemispherical object 2, and the diameter of hemispherical object 2 is identical with the upper diameter of bowl-shape object, and the front of hemispherical object is designed to a unlimited circular groove, and the radius of circular groove is controlled at 35 millimeters;
The air dry of attapulgite environmental-friendly ashtray crude green body process, slow oven dry, middle temperature are burnt till, middle high temperature burns till, cools off, polishes and place stainless steel steel wire 10 backs is the attapulgite environmental-friendly ashtray.
Using method: after smoker's smoking, cigarette 13 can be placed directly in the semi arch groove 7, the centre bore 16 of one end of cigarette 13 burning stainless steel steel wire 13 in the attapulgite environmental-friendly ashtray, the cigarette ash that produces from an end of cigarette 13 burnings can directly fall into below the attapulgite environmental-friendly ashtray stainless steel steel wire 13; After the smoker sucked cigarette, the end with cigarette 8 burnings directly inserted in the extinguishing hole 3 of attapulgite environmental-friendly ashtray earlier, and the back cigarette 8 that will extinguish again takes out, and puts into attapulgite environmental-friendly ashtray inside 6 from stainless steel steel wire centre bore 16; During cleaning attapulgite environmental-friendly ashtray, elder generation takes out stainless steel steel wire 13, and pours out cigarette and cigarette ash 14 after extinguishing, again with standby behind the attapulgite environmental-friendly ashtray scrub.

Claims (1)

1. the preparation method of an attapulgite environmental-friendly ashtray crude green body, it is characterized in that, (1) is made into attapulgite environmental-friendly ashtray crude green body with concavo-convex excellent pottery mud with air purification function, the bottom of crude green body is a bowl-shape object, the upper diameter of bowl-shape object is controlled at 80~150 millimeters, highly be controlled at 35~65 millimeters, the base plate of a sealing is arranged at the bottom in the bowl-shape object, the diameter of base plate is controlled at 40~80 millimeters, design has two columns of smoke that go out on the floor level center line, going out, the diameter on plane is controlled at 14~24 millimeters on the column of smoke, the diameter of column of smoke lower plane of going out is controlled at 16~26 millimeters, and there is an extinguishing hole at the column of smoke center of going out, and the diameter of extinguishing hole is controlled at 6~10 millimeters, designing respectively on the last horizontal edge of bowl-shape object has 3 semi arch grooves, and the diameter of semi arch groove is controlled at 8~12 millimeters; The top of crude green body is a hollow hemispherical object, and the diameter of hemispherical object is identical with the upper diameter of bowl-shape object, and the front of hemispherical object is designed to a unlimited circular groove, and the radius of circular groove is controlled at 25~50 millimeters;
Described production method with concavo-convex excellent pottery mud of air purification function is: (1) will have after the batch mixes of concavo-convex excellent pottery mud of air purification function and stir in the input mixer; (2) carry out wet ball grinding in the mixture after being mixed input ball mill, the grain fineness of ball milling disposed slurry is less than 0.044 millimeter; (3) will carry out the old semi-finished product that are treated in the input of the slurry behind the ball milling sedimentation basin, half-finished water content is less than 45%, and the old time was controlled at 3~30 days; (4) semi-finished product are imported in the vacuum-extruder extruding and cut into rectangular block, the thickness of the block thing of rectangle is less than 50 millimeters, for having the concavo-convex excellent pottery mud of air purification function;
Batching with concavo-convex excellent pottery mud of air purification function is made up of following component by weight percentage: paste attapulgite clay 45~75%, attapulite constant humidity amendment 5~30%, natural-minerals adsorptive filter medium 5~15%, cacumen biotae 2~10%, alumina silicate fibre 1~5%, polyacrylamide 0.1~3% and water 1~35%;
The production technology of described paste attapulgite clay: will stir in the concavo-convex excellent ore deposit input mixer, after extruder is squeezed into sheet, import once more in the mixer and stir, natural drying after extruder is squeezed into sheet, the concavo-convex excellent ore deposit of drying is transported in the feed reservoir soaks, dash with air pump and to turn over, post precipitation is emitted immersion water, the sieve decontamination in the input semi-finished product pond, is soaked again, dash with air pump and to turn over, post precipitation is emitted immersion water, and the slurry transportation of post precipitation is arrived in the finished product pond, is paste attapulgite clay;
Described paste attapulgite clay is made up of following component by weight percentage: Concave-convex clay rod 25~60%, water 40~75%;
Rice hulls, quick dissolved sodium silicate and the zeolite powder of described attapulite constant humidity amendment after by Concave-convex clay rod, montmorillonite, acidifying formed; The production method of attapulite constant humidity amendment is: the rice hulls after the acidifying and Concave-convex clay rod and montmorillonite are mixed by batching, extrusion modification slabbing mixture, abrasive dust after airing mixes by batching with quick dissolved sodium silicate and zeolite powder and is attapulite constant humidity amendment;
The batching of attapulite constant humidity amendment is made up of following component by weight percentage: the semi-finished product 55~90% of attapulite constant humidity amendment, quick dissolved sodium silicate 2~8% and zeolite powder 5~40%; The half-finished batching of attapulite constant humidity amendment is made up of following component: the rice hulls 5~15% after the acidifying, Concave-convex clay rod 35~55%, montmorillonite 5~15% and water 35~55% by weight percentage;
Zeolite, Concave-convex clay rod acidifying after, bentonite acidifying after, diatomite acidifying after, volcanic rock and the alumine of the batching of described natural-minerals adsorptive filter medium after by acidifying formed; The preparation method of natural-minerals adsorptive filter medium is: is natural-minerals adsorptive filter medium with the batching of natural-minerals adsorptive filter medium through mixing, pulverize, sieving;
The batching of natural-minerals adsorptive filter medium is made up of following component by weight percentage: the zeolite 15~35% after the acidifying, the Concave-convex clay rod 15~35% after the acidifying, the bentonite 15~25% after the acidifying, the diatomite 10~20% after the acidifying, volcanic rock 5~10% and alumine 5~10%.
CN 201110099868 2011-04-21 2011-04-21 Method for making environment-friendly attapulgite ash tray rough blank Active CN102229178B (en)