CN102154579B - 空气凝汽器焊片 - Google Patents
空气凝汽器焊片 Download PDFInfo
- Publication number
- CN102154579B CN102154579B CN2011100508759A CN201110050875A CN102154579B CN 102154579 B CN102154579 B CN 102154579B CN 2011100508759 A CN2011100508759 A CN 2011100508759A CN 201110050875 A CN201110050875 A CN 201110050875A CN 102154579 B CN102154579 B CN 102154579B
- Authority
- CN
- China
- Prior art keywords
- weld tabs
- air condenser
- percent
- condenser
- soldering terminal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明公开了一种空气凝汽器焊片,焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:8~10%,Zn:20~30%,Mg:0.1~0.2%,Sr:0.04~0.08%,Cu:0.1~0.3%,余量为Al。本发明具有熔化温度低,降低电能消耗,节约能源的优点。
Description
技术领域
本发明涉及一种铝合金材料,特别是一种空气凝汽器焊片。
背景技术
凝汽器一般用于汽轮机动力装置中,也可用于汽车的散热器,分为水冷凝汽器和空气凝汽器两种,凝汽器除将汽轮机的排汽冷凝成水供锅炉重新使用外,还能在汽轮机排汽处建立真空和维持真空,凝汽器真空是影响机组安全、经济运行的一个重要指标,机组运行参数的变化会对凝汽器真空产生影响,而空冷凝汽器有庞大的真空体,在其运行过程中不可避免的要漏入空气,因此在空气凝汽器真空的影响因素中不能忽视漏入空气因素,为保证空气凝汽器的密封性,现有的空气凝汽器焊片一般在635℃温度时,才能熔化进行焊接,这样不仅提高了电能的消耗,且浪费能源。
发明内容
本发明的目的是为了克服以上的不足,提供一种熔化温度低,降低电能消耗,节约能源的空气凝汽器焊片。
本发明的目的通过以下技术方案来实现:一种空气凝汽器焊片,焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:8~10%,Zn:20~30%,Mg:0.1~0.2%,Sr:0.04~0.08%,Cu:0.1~0.3%,余量为Al。
本发明的进一步改进在于:所述焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:8%,Zn:25%,Mg:0.1%,Sr:0.06%,Cu:0.1%,Al:66.74%。
本发明的进一步改进在于:所述焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:9%,Zn:23%,Mg:0.2%,Sr:0.04%,Cu:0.2%,Al:67.56%。
本发明的进一步改进在于:所述焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:10%,Zn:25%,Mg:0.2%,Sr:0.06%,Cu:0.2%,Al:64.54%。
本发明与现有技术相比具有以下优点:熔化温度为550~570℃,这样较原先635℃的熔化温度相比,不仅降低了电能的消耗,且节约了能源。
具体实施方式:
为了加深对本发明的理解,下面将结合实施例对本发明作进一步详述,该实施例仅用于解释本发明,并不构成对本发明保护范围的限定。
本发明示出了空气凝汽器焊片的一种具体实施方式,焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:8~10%,Zn:20~30%,Mg:0.1~0.2%,Sr:0.04~0.08%,Cu:0.1~0.3%,Al:61.42~69.76%,本发明所述的焊片熔化温度为550~570℃,不仅降低了电能的消耗,且节约了能源。
实施例一:空气凝汽器焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:8%,Zn:25%,Mg:0.1%,Sr:0.06%,Cu:0.1%,Al:66.74%,这样通过上述各成份配制后,焊片的熔化温度为563℃,不仅降低了电能的消耗,且节约了能源。
实施例二:空气凝汽器焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:9%,Zn:23%,Mg:0.2%,Sr:0.04%,Cu:0.2%,Al:67.56%。这样通过上述各成份配制后,焊片的熔化温度为558℃,不仅降低了电能的消耗,且节约了能源。
实施例三:空气凝汽器焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:10%,Zn:25%,Mg:0.2%,Sr:0.06%,Cu:0.2%,Al:64.54%,这样通过上述各成份配制后,焊片的熔化温度为552℃,不仅降低了电能的消耗,且节约了能源。
Claims (4)
1.一种空气凝汽器焊片,其特征在于:所述焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:8~10%,Zn:20~30%,Mg:0.1~0.2%,Sr:0.04~0.08%,Cu:0.1~0.3%,余量为Al。
2.根据权利要求1所述空气凝汽器焊片,其特征在于,所述焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:8%,Zn:25%,Mg:0.1%,Sr:0.06%,Cu:0.1%,Al:66.74%。
3.根据权利要求1所述空气凝汽器焊片,其特征在于,所述焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:9%,Zn:23%,Mg:0.2%,Sr:0.04%,Cu:0.2%,Al:67.56%。
4.根据权利要求1所述空气凝汽器焊片,其特征在于,所述焊片包括Si、Zn、Mg、Sr、Cu和Al,其中各成分的质量比为:Si:10%,Zn:25%,Mg:0.2%,Sr:0.06%,Cu:0.2%,Al:64.54%。