CN102102478A - 高分子复合门板的加工方法 - Google Patents
高分子复合门板的加工方法 Download PDFInfo
- Publication number
- CN102102478A CN102102478A CN2009102015496A CN200910201549A CN102102478A CN 102102478 A CN102102478 A CN 102102478A CN 2009102015496 A CN2009102015496 A CN 2009102015496A CN 200910201549 A CN200910201549 A CN 200910201549A CN 102102478 A CN102102478 A CN 102102478A
- Authority
- CN
- China
- Prior art keywords
- coating
- composite door
- pvc
- macromolecular composite
- door panel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种高分子复合门板的加工方法,包括以下步骤:(a)使用PUR胶将PVC或ABS塑料片材粘合在中密度纤维板上,形成半成品;(b)将PET塑料薄膜四边用橡皮筋拉紧撑平固定在膜框架上;(c)在步骤(a)半成品的PVC或ABS塑料的表面涂上UV涂料,将步骤(b)拉紧撑平的PET塑料薄膜连同膜框架罩UV涂料的上面,用滚轮滚涂均匀;(d)采用紫外灯照射使UV涂料固化。本发明的方法加工出的高分子复合门板具有光亮度、平整度高的优点。
Description
技术领域
本发明涉及建筑装饰材料领域,具体涉及一种高分子复合门板的加工方法。
背景技术
随着新材料技术的不断发展和生活水平的提高,人们对建筑装饰材料的要求也越来越高。为了达到更好的装饰效果,人们对门板的颜色、形状挑剔的同时,对门板的光亮度和平整度也有了更高的要求,然而门板的光亮度和平整度的高低直接取决于门板的加工方法。本发明是为满足人们的需求,对门板的加工方法的进一步发展。
发明内容
本发明的目的在于克服现有技术的不足,提供一种光亮度、平整度高的高分子复合门板的加工方法。
本发明的目的是这样实现的:一种高分子复合门板的加工方法,其特征在于:它包括以下步骤:
(a)使用PUR胶将PVC或ABS塑料片材粘合在中密度纤维板上,形成半成品;
(b)将PET塑料薄膜四边用橡皮筋拉紧撑平固定在膜框架上;
(c)在步骤(a)半成品的PVC或ABS塑料的表面涂上UV涂料,将步骤(b)拉紧撑平的PET塑料薄膜连同膜框架罩UV涂料的上面,用滚轮滚涂均匀;
(d)采用紫外灯照射使UV涂料固化。
本发明的优点在于:本发明的方法是在将PET塑料薄膜采用橡皮筋拉紧撑平固定在膜框架上,加上紫外灯照射使UV涂料迅速固化的技术,保证了加工成型门板的平整度,因此加工出的高分子复合门板具有光亮度、平整度高的优点。
具体实施方式
下面对本发明做进一步的说明。
实施例1:一种高分子复合门板的加工方法,它包括以下步骤:(a)使用PUR胶将PVC或ABS塑料片材粘合在中密度纤维板上,形成半成品;(b)将PET塑料薄膜四边用橡皮筋拉紧撑平固定在膜框架上;(c)在步骤(a)半成品的PVC或ABS塑料的表面涂上UV涂料,将步骤(b)拉紧撑平的PET塑料薄膜连同膜框架罩UV涂料的上面,用滚轮滚涂均匀;(d)采用紫外灯照射使UV涂料固化。
Claims (1)
1.一种高分子复合门板的加工方法,其特征在于:它包括以下步骤:
(a)使用PUR胶将PVC或ABS塑料片材粘合在中密度纤维板上,形成半成品;
(b)将PET塑料薄膜四边用橡皮筋拉紧撑平固定在膜框架上;
(c)在步骤(a)半成品的PVC或ABS塑料的表面涂上UV涂料,将步骤(b)拉紧撑平的PET塑料薄膜连同膜框架罩UV涂料的上面,用滚轮滚涂均匀;
(d)采用紫外灯照射使UV涂料固化。