Prior art keywords
bracing ply
tire
cord
steel
belted layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201010575573
Other languages
English (en)
Inventor
刘永华
李振波
隋学智
刘永祥
隋家兴
鲍建德
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG YINBAO TYPE GROUP CO Ltd
Original Assignee
SHANDONG YINBAO TYPE GROUP CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG YINBAO TYPE GROUP CO Ltd filed Critical SHANDONG YINBAO TYPE GROUP CO Ltd
Priority to CN 201010575573 priority Critical patent/CN102059922A/zh
Publication of CN102059922A publication Critical patent/CN102059922A/zh
Pending legal-status Critical Current

Links

Images

Landscapes

  • Tires In General (AREA)

Abstract

本发明公开了一种全钢轻型载重子午线轮胎,该轮胎包括胎面部、胎侧部、胎圈部、帘布层、带束层,带束层包括1#带束层、2#带束层、3#带束层、4#带束层,3#带束层与2#带束层之间设有具有防水功能的增粘、增强胶片,本发明由于多使用一层带束层及一层增粘、增强胶片,轮胎的冠部刚性增大,轮胎在行驶时,周向变形减小,行驶平稳、滚动阻力小,在苛刻的多岩石环境抗刺扎性能大幅提高;在雨季作业时,轮胎被刺伤,具有防水功能的增粘、增强胶片会有效的保护胎体免受雨水锈蚀,使用寿命延长1~3倍,降低了运行成本。

Description

全钢轻型载重子午线轮胎
技术领域
本发明涉及一种子午线轮胎,具体的说涉及一种全钢轻型载重子午线轮胎。
背景技术
目前国内诸多轮胎企业广泛采用的全钢轻型载重子午线轮胎截面结构,如图1所示,包括胎面部1、胎侧部2、胎圈部、帘布层3、带束层4,带束层4由3层带束层组成,即1#带束层、2#带束层、3#带束层。全钢轻型载重子午线轮胎的应用范围越来越广,在采石场等恶略的使用条件下作业时,轮胎冠部极易被刺伤,严重的甚至被刺爆,很多轮胎企业通过加深花纹、改进胎面胶配方等方法提高轮胎的抗刺扎性能,有一定的效果。但是雨天作业时,轮胎被刺伤,胎体易受雨水锈蚀,如不及时修补,轮胎将报废或发生爆胎。
发明内容
本发明所要解决的问题是克服上述技术的不足,提供一种具有防水、抗刺扎带束层结构的全钢轻型载重子午线轮胎。
为了解决上述问题,本发明轮胎采用以下技术方案:
一种全钢轻型载重子午线轮胎,该轮胎包括胎面部、胎侧部、胎圈部、帘布层、带束层,其特征在于:带束层包括1#带束层、2#带束层、3#带束层、4#带束层,3#带束层与2#带束层之间设有具有防水功能的增粘、增强胶片。
以下为对上述技术方案所做的进一步改进:
增粘、增强胶片的宽度大于2#带束层的宽度4~16mm,增粘、增强胶片的厚度为2mm~4mm。
进一步改进;
所述1#带束层、2#带束层、3#带束层、4#带束层各层带束层之间帘线相互交叉成网状,带束层帘线与胎冠面中心线的夹角小于90°。
进一步改进;
1#带束层的帘线与胎冠面中心线的夹角为24°,2#带束层、3#带束层、4#带束层的帘线与胎冠面中心线的夹角为15°。
进一步改进;
4#带束层的宽度小于3#带束层的宽度4mm~12mm。
进一步改进;
所述1#带束层、2#带束层、3#带束层的帘线为高强度钢丝帘线。
进一步改进;
所述4#带束层的帘线为高伸长钢丝帘线。
本发明由于多使用一层带束层及一层增粘、增强胶片,轮胎的冠部刚性增大,轮胎在行驶时,周向变形减小,行驶平稳、滚动阻力小,在苛刻的多岩石环境抗刺扎性能大幅提高;在雨季作业时,轮胎被刺伤,具有防水功能的增粘、增强胶片会有效的保护胎体免受雨水锈蚀,使用寿命延长1~3倍,降低了运行成本。
下面结合附图和实施例对本发明作进一步说明:
附图说明
附图1为本发明背景技术中现有采用的全钢轻型载重子午线轮胎的结构示意图;
附图2为本发明实施例中的全钢轻型载重子午线轮胎具有防水、抗刺扎的结构示意图。
图中:图中:1-胎面部;2-胎侧部;3-帘布层;4-带束层;5-增粘、强胶片;41-1#带束层;42-2#带束层;43-3#带束层;44-4#带束层。
具体实施方式
实施例1,如附图2所示,一种具有防水、抗刺扎带束层结构的全钢轻型载重子午线轮胎,该轮胎包括胎面部1、胎侧部2、胎圈部、帘布层3、带束层4,带束层4包括1#带束层41、2#带束层42、3#带束层43、4#带束层44,3#带束层43与2#带束层43之间设有增粘、增强胶片5,增粘、增强胶片宽度大于2#带束层4mm,增粘、增强胶片的厚度为2mm。
1#带束层41、2#带束层42、3#带束层43、4#带束层44各层带束层之间帘线相互交叉成网状,1#带束层41帘线与胎冠面中心线的夹角为24°,所述2#带束层42、3#带束层43、4#带束层44帘线与胎冠面中心线的夹角为15°。
4#带束层44宽度小于3#带束层43的宽度4mm。
1#带束层41、2#带束层42、3#带束层43使用高强度钢丝帘线。
4#带束层44使用高伸长钢丝帘线。
实施例2、如附图2所示,一种具有防水、抗刺扎带束层结构的全钢轻型载重子午线轮胎,该轮胎包括胎面部1、胎侧部2、胎圈部、帘布层3、带束层4,带束层4包括1#带束层41、2#带束层42、3#带束层43、4#带束层44。
3#带束层43与2#带束层42之间设有增粘、增强胶片5,增粘、增强胶片宽度大于2#带束层16mm,增粘、增强胶片的厚度为4mm。
1#带束层41、2#带束层42、3#带束层43、4#带束层44各层带束层之间帘线相互交叉成网状,1#带束层41帘线与胎冠面中心线的夹角为24°,所述2#带束层42、3#带束层43、4#带束层44帘线与胎冠面中心线的夹角为15°。
4#带束层44宽度小于3#带束层43的宽度12mm。
1#带束层41、2#带束层42、3#带束层43使用高强度钢丝帘线。
4#带束层44使用高伸长钢丝帘线。

Claims (7)

1.一种全钢轻型载重子午线轮胎,该轮胎包括胎面部(1)、胎侧部(2)、胎圈部、帘布层(3)、带束层(4),其特征在于:带束层(4)包括1#带束层(41)、2#带束层(42)、3#带束层(43)、4#带束层(44),3#带束层(43)与2#带束层(42)之间设有增粘、增强胶片(5)。
2.如权利要求1所述的全钢轻型载重子午线轮胎,其特征是:增粘、增强胶片(5)的宽度大于2#带束层的宽度4~16mm,增粘、增强胶片的厚度为2mm~4mm。
3.如权利要求1所述的全钢轻型载重子午线轮胎,其特征是:所述1#带束层(41)、2#带束层(42)、3#带束层(43)、4#带束层(44)各层带束层之间帘线相互交叉成网状,带束层帘线与胎冠面中心线的夹角小于90°。
4.如权利要求1所述的全钢轻型载重子午线轮胎,其特征是:1#带束层(41)的帘线与胎冠面中心线的夹角为24°,2#带束层(42)、3#带束层(43)、4#带束层(44)的帘线与胎冠面中心线的夹角为15°。
5.如权利要求2或4所述的全钢轻型载重子午线轮胎,其特征是:4#带束层(44)的宽度小于3#带束层(43)的宽度4mm~12mm。
6.如权利要求3所述的全钢轻型载重子午线轮胎,其特征是:所述1#带束层(41)、2#带束层(42)、3#带束层(43)的帘线为高强度钢丝帘线。
7.如权利要求3所述的全钢轻型载重子午线轮胎,其特征是:所述4#带束层(44)的帘线为高伸长钢丝帘线。
CN 201010575573 2010-12-06 2010-12-06 全钢轻型载重子午线轮胎 Pending CN102059922A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201010575573 CN102059922A (zh) 2010-12-06 2010-12-06 全钢轻型载重子午线轮胎

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201010575573 CN102059922A (zh) 2010-12-06 2010-12-06 全钢轻型载重子午线轮胎

Publications (1)

Publication Number Publication Date
CN102059922A true CN102059922A (zh) 2011-05-18

Family

ID=43995512

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201010575573 Pending CN102059922A (zh) 2010-12-06 2010-12-06 全钢轻型载重子午线轮胎

Country Status (1)

Country Link
CN (1) CN102059922A (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104228466A (zh) * 2014-08-27 2014-12-24 德轮橡胶股份有限公司 一种全钢轻型载重子午线轮胎
CN104369623A (zh) * 2014-08-27 2015-02-25 德轮橡胶股份有限公司 一种全钢载重子午线轮胎
CN110001294A (zh) * 2019-05-07 2019-07-12 江苏通用科技股份有限公司 全钢子午线轮胎胎冠结构

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1671564A (zh) * 2002-06-28 2005-09-21 株式会社普利司通 充气轮胎
CN101428533A (zh) * 2007-11-08 2009-05-13 韩国轮胎株式会社 载重汽车用轮胎

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1671564A (zh) * 2002-06-28 2005-09-21 株式会社普利司通 充气轮胎
CN101428533A (zh) * 2007-11-08 2009-05-13 韩国轮胎株式会社 载重汽车用轮胎

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104228466A (zh) * 2014-08-27 2014-12-24 德轮橡胶股份有限公司 一种全钢轻型载重子午线轮胎
CN104369623A (zh) * 2014-08-27 2015-02-25 德轮橡胶股份有限公司 一种全钢载重子午线轮胎
CN110001294A (zh) * 2019-05-07 2019-07-12 江苏通用科技股份有限公司 全钢子午线轮胎胎冠结构

Similar Documents

Publication Publication Date Title
CN201895538U (zh) 一种全钢载重子午线轮胎
EP2261059A3 (en) Pneumatic tire with an overlay reinforcement
CN1671564A (zh) 充气轮胎
CN201998750U (zh) 一种全钢轻型载重子午线轮胎
CN102059922A (zh) 全钢轻型载重子午线轮胎
CN201633479U (zh) 聚氨酯胎侧增强型填充轮胎
ATE477940T1 (de) Reifen für schwerfahrzeuge
CN102029863A (zh) 全钢载重子午线轮胎
CN104369623A (zh) 一种全钢载重子午线轮胎
CN204236145U (zh) 一种全钢载重子午线轮胎
CN201525246U (zh) 分体式汽车轮胎
CN103568733A (zh) 耐刺扎型载重汽车轮胎
CN207772793U (zh) 外层带束层与零度带束层分离式结构的全钢子午线轮胎
CN205381098U (zh) 一种新型胎冠结构的农用车胎
CN202727889U (zh) 耐刺扎型载重汽车轮胎
CN201534469U (zh) 带骨架高弹性实心轮胎
CN104228466A (zh) 一种全钢轻型载重子午线轮胎
CN203864341U (zh) 使用缠绕带束层补强结构的全钢丝载重子午线轮胎
CN204236146U (zh) 一种全钢轻型载重子午线轮胎
CN206884616U (zh) 一种充气轮胎
CN218661184U (zh) 一种防刺扎型电动车轮胎
KR20150138894A (ko) 개선된 보강벨트를 가지는 공기입 타이어
CN201261359Y (zh) 一种深花纹高耐刺扎耐切割斜交巨型工程轮胎
CN213892064U (zh) 一种免充气手推车轮胎
CN201009677Y (zh) 带有过渡加强层的全钢子午工程轮胎

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20110518