CN102059176B - 磷灰岩矿常温泡沫浮选捕收剂及其制备方法 - Google Patents

磷灰岩矿常温泡沫浮选捕收剂及其制备方法 Download PDF

Info

Publication number
CN102059176B
CN102059176B CN201010581679A CN201010581679A CN102059176B CN 102059176 B CN102059176 B CN 102059176B CN 201010581679 A CN201010581679 A CN 201010581679A CN 201010581679 A CN201010581679 A CN 201010581679A CN 102059176 B CN102059176 B CN 102059176B
Authority
CN
China
Prior art keywords
parts
phosphorite
normal
foam flotation
flotation collector
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201010581679A
Other languages
English (en)
Other versions
CN102059176A (zh
Inventor
王仁宗
孙金艳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hubei Fubang New Material Co ltd
Original Assignee
Hubei Forbon Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hubei Forbon Technology Co Ltd filed Critical Hubei Forbon Technology Co Ltd
Priority to CN201010581679A priority Critical patent/CN102059176B/zh
Publication of CN102059176A publication Critical patent/CN102059176A/zh
Application granted granted Critical
Publication of CN102059176B publication Critical patent/CN102059176B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种磷灰岩矿常温泡沫浮选捕收剂,由下述物质组成,各物质按重量份计,油酸15-40份,亚油酸30-65份,氧化石蜡皂20-30份,以油酸、亚油酸、氧化石蜡皂总量为100份计,起泡剂5-10份;制备方法:将15-40份的油酸与30-65份的亚油酸混合,并将混合物加热至100~120℃,加入20-30份的氧化石蜡皂皂化一小时,再以皂化后的混合物为100份计,加入5-10份的起泡剂混合均匀,制得磷灰岩矿常温泡沫浮选捕收剂。本发明的捕收剂可以运用在湖北锦屏、黄麦玲等磷灰岩矿石的常温泡沫浮选上,与传统的常温正浮选捕收剂相比具有捕收能力强、选择性高、用量少、耐常温、选矿成本低较,回收率高的特点。

Description

磷灰岩矿常温泡沫浮选捕收剂及其制备方法
技术领域
本发明涉及矿石泡沫浮选捕收剂,尤其涉及一种磷灰岩矿常温泡沫浮选捕收剂及其制备方法
背景技术
中国东部自湖北蕲春、黄梅、黄麦岭,经安徽宿松、肥东,至江苏锦屏,分布有一系列中小型沉积变质磷灰石岩矿床,习惯上称之为“海州式磷矿”。矿体形态以层状、似层状为主,少部分呈透镜状、脉状及不规则状。矿石结构主要有花岗变晶结构、磷片变晶结构、磷片花岗变晶结构、淋滤残余结构及碎裂结构。矿石构造主要有片状构造、片麻状构造。根据矿石中脉石矿物成分大致分为磷灰岩、硅质长石质磷灰岩、云母质磷灰岩、硅质磷灰岩、锰质磷灰岩及白云质磷灰岩等。磷灰石分布广泛,矿石矿物为粒状磷灰石金紧密镶嵌,含量在80%-90%,多形成于地表风化带,被淋滤溶蚀空洞发育,空洞中往往有锰土充填,碳酸盐矿物很少。磷灰石多呈六方短柱,晶簇状定向排列,局部常残余有胶磷矿。有关学者对此类磷矿进行研究,综合磷灰石的自然形态、红外光谱及晶体化学式,可以确定矿石矿物有三种类型:硅质及硅酸盐型亚类磷灰岩矿石、碳酸盐型亚类磷灰岩矿石、为混合型亚类磷灰岩矿石,此类磷矿易于浮选。浮选中多使用的是脂肪酸类捕收剂,常温下大多呈胶束形,很少呈浮游活性形,长期以来,在磷矿直接浮选,需将矿浆加温,以使捕收剂保持高度的分散性,获得较理想的分选指标。但矿浆加温费用太高。初步估算,矿浆加温到35℃,每吨原矿所需煤为28.4Kg。因此常温捕收剂的研发成功能起到降低选矿成本的作用。
发明内容
本发明的目的为了克服上述现有技术存在的缺陷和问题,而提供一种磷灰岩矿常温泡沫浮选捕收剂及其制备方法,本发明提供的磷矿常温泡沫浮选捕收剂可以将五氧化二磷含量为8%-15%的原矿提升到五氧化二磷含量为30%以上的精矿,而且精矿回收率高,选矿成本低。
本发明是通过以下技术实现的:
磷灰岩矿常温泡沫浮选捕收剂,其特征在于:由下述物质组成,各物质按重量份计,油酸15-40份,亚油酸30-65份,氧化石蜡皂20-30份,以油酸、亚油酸、氧化石蜡皂总量为100份计,起泡剂5-10份,制备方法:将15-40份的油酸与30-65份的亚油酸混合,并将混合物加热至100~120℃,加入20-30份的氧化石蜡皂皂化一小时,再以皂化后的混合物为100份计,加入5-10份的起泡剂混合均匀,制得磷灰岩矿常温泡沫浮选捕收剂。
所述的起泡剂为从市场上购置的MES。
所述的油酸、亚油酸均从市场购置。
所述的氧化石蜡皂为石蜡与固体氢氧化钠按常规方法皂化所得,也可以从市场购置。
本发明提供的捕收剂具有捕收能力强、选择性高、用量少、常温浮选、选矿成本低和应用广等优点,不仅适用于“海州式”磷矿的选矿生产,也可用于各种磷矿石的选矿生产,而且在浮选温度在20℃左右时,所生产的磷精矿质量仍达到合格要求且回收率很高,这对于我国大量低品位“海州式”磷矿资源的利用有着非常重要的意义。
具体实施方式
下面结合实施例对本发明作进一步说明,但不限定本发明,以下实施例各物质按重量份计。所述的起泡剂为从市场上购置的MES。所述的油酸、亚油酸均从市场购置。所述的氧化石蜡皂为石蜡与固体氢氧化钠按常规方法皂化所得,也可以从市场购置。
实施例1:将45份的亚油酸和35份的油酸原料混合,并将混合物加热至120℃,加入20份的氧化石蜡皂并搅拌皂化一小时左右,以皂化后的混合物为100份加入5份的所购的起泡剂G30得磷灰岩矿常温泡沫浮选捕收剂成品。
将本实施例1制得的磷灰岩矿常温泡沫浮选捕收剂用于湖北黄梅磷矿常温浮选试验:在矿浆自然温度为20℃,原矿P2O5为13.51%时,采用一粗一精一扫闭路流程,每吨浮选磷矿中捕收剂加入量为0.7kg,经过直接浮选可获得精矿P2O5为30.27%,回收率达到82.65%的好指标。
实施例2:将50份的亚油酸和20份的油酸原料混合,并将混合物加热至110℃,加入30份的氧化石蜡皂并搅拌皂化一小时左右,以皂化后的混合物为100份加入8份的所购的起泡剂G30得磷灰岩矿常温泡沫浮选捕收剂成品。
将本实施例2制得的磷灰岩矿常温泡沫浮选捕收剂用于湖北黄梅磷矿常温浮选试验:在矿浆自然温度为20℃,原矿P2O5为13.51%时,采用一粗一精一扫闭路流程,每吨浮选磷矿中捕收剂加入量为0.7kg,经过直接浮选可获得精矿P2O5为30.41%,回收率达到81.63%的好指标。
实施例3:将55份的亚油酸和25份的油酸原料混合,并将混合物加热至100℃,加入20份的氧化石蜡皂并搅拌皂化一小时左右,以皂化后的混合物为100份加入10份的所购的起泡剂G30得磷灰岩矿常温泡沫浮选捕收剂成品。
将本实施例3制得的磷灰岩矿常温泡沫浮选捕收剂用于湖北黄梅磷矿常温浮选试验:在矿浆自然温度为20℃,原矿P2O5为13.51%时,采用一粗一精一扫闭路流程,每吨浮选磷矿中捕收剂加入量为0.7kg,经过直接浮选可获得精矿P2O5为30.94%,回收率达到81.73%的好指标。
实施例4:将30份的亚油酸和40份的油酸原料混合,并将混合物加热至120℃,加入30份的氧化石蜡皂并搅拌皂化一小时左右,以皂化后的混合物为100份加入5份的所购的起泡剂G30得磷灰岩矿常温泡沫浮选捕收剂成品。
将本实施例4制得的磷灰岩矿常温泡沫浮选捕收剂用于湖北黄梅磷矿常温浮选试验:在矿浆自然温度为20℃,原矿P2O5为13.51%时,采用一粗一精一扫闭路流程,每吨浮选磷矿中捕收剂加入量为0.7kg,经过直接浮选可获得精矿P2O5为30.37%,回收率达到81.65%的好指标。
实施例5:将65份的亚油酸和15份的油酸原料混合,并将混合物加热至100℃,加入20份的氧化石蜡皂并搅拌皂化一小时左右,以皂化后的混合物为100份加入10份的所购的起泡剂G30得磷灰岩矿常温泡沫浮选捕收剂成品。
将本实施例5制得的磷灰岩矿常温泡沫浮选捕收剂用于湖北黄梅磷矿常温浮选试验:在矿浆自然温度为20℃,原矿P2O5为13.51%时,采用一粗一精一扫闭路流程,每吨浮选磷矿中捕收剂加入量为0.7kg,经过直接浮选可获得精矿P2O5为30.58%,回收率达到81.98%的好指标。

Claims (2)

1.磷灰岩矿常温泡沫浮选捕收剂,其特征在于:由下述物质组成,各物质按重量份计,油酸15-40份,亚油酸30-65份,氧化石蜡皂20-30份,以油酸、亚油酸、氧化石蜡皂总量为100份计,起泡剂5-10份;将15-40份的油酸与30-65份的亚油酸混合,并将混合物加热至100~120℃,加入20-30份的氧化石蜡皂皂化一小时,再以皂化后的混合物为100份计,加入5-10份的起泡剂混合均匀,制得磷灰岩矿常温泡沫浮选捕收剂。
2.根据权利要求1所述的磷灰岩矿常温泡沫浮选捕收剂的制备方法,其特征在于:将15-40份的油酸与30-65份的亚油酸混合,并将混合物加热至100~120℃,加入20-30份的氧化石蜡皂皂化一小时,再以皂化后的混合物为100份计,加入5-10份的起泡剂混合均匀,制得磷灰岩矿常温泡沫浮选捕收剂。
CN201010581679A 2010-12-03 2010-12-03 磷灰岩矿常温泡沫浮选捕收剂及其制备方法 Expired - Fee Related CN102059176B (zh)