CN102018273A - Method for reducing carbon monoxide release amount of papermaking reconstituted tobacco - Google Patents
Method for reducing carbon monoxide release amount of papermaking reconstituted tobacco Download PDFInfo
- Publication number
- CN102018273A CN102018273A CN 201010524106 CN201010524106A CN102018273A CN 102018273 A CN102018273 A CN 102018273A CN 201010524106 CN201010524106 CN 201010524106 CN 201010524106 A CN201010524106 A CN 201010524106A CN 102018273 A CN102018273 A CN 102018273A
- Authority
- CN
- China
- Prior art keywords
- papermaking
- carbon monoxide
- reconstituted tobaccos
- method reconstituted
- reconstituted tobacco
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a method for reducing the carbon monoxide release amount of papermaking reconstituted tobacco, and belongs to the technical field of harm reduction of reconstituted tobacco in the tobacco industry. The method has the main technical characteristic that: specific alkali metal inorganic acid salt is added in the coating or flavoring or filler adding process during the production of the papermaking reconstituted tobacco, so that the carbon monoxide release amount of the papermaking reconstituted tobacco can be effectively reduced, and the smoking quality of a product is not obviously changed, wherein the alkali metal inorganic acid salt is formed by compounding one or more of Li2SO4, Na2SO4, K2SO4, Na2CO3, K2CO3, NaCl and KCl and is added in an amount which is 0.1 to 4 percent based on the mass of the papermaking reconstituted tobacco product.
Description
Technical field
The present invention relates to a kind of method that reduces papermaking-method reconstituted tobaccos carbon monoxide burst size, belong to the reconstituted tobacco harm reduction technical field of tobacco industry.
Background technology
Papermaking-method reconstituted tobaccos is to be raw material with tobacco dead meal and tobacco byproduct, a kind of " artificial tobacco leaf " that paper technology after adopting modern extraction and separation technology and improving processes, it is little that this product has density, the filling rate height, flammability is good, it is good to inhale flavor, multiple good characteristics such as releasing content of coke tar is low, it is mixed be assigned in cigarette composition and can play good Jiao that falls, consumption reduction, the regulation and control tobacco inhales the effect of flavor and chemical composition, thereby papermaking-method reconstituted tobaccos still is the functional material of a kind of unique tobacco resource regeneration and reducing cigarette tar and reducing consumption reduction double effects, just progressively is subjected to the favor of Chinese style cigarette composition at present.But research also shows (Yunnan University's journal-natural science edition simultaneously, 2010, S1:130-133): because the cellulose family component content of self is higher, the carbon monoxide of papermaking-method reconstituted tobaccos (CO) burst size is often higher, though thereby in cigarette composition if use this product can play the good burnt consumption reduction effect of falling too much, also may cause the whole limit standard that raises and surpass product of carbon monoxide burst size of cigarette simultaneously.Carbon monoxide is a kind of pest (Hoffman inventory hazardous compound) that mainly contains in the cigarette mainstream flue gas after all, it all can produce bigger damaging effect to breathing, blood, the nervous system of human body, simultaneously, carbon monoxide still is a kind of nonvolatil gas, adopts general method to be difficult to realization its adsorbing and trapping or conversion are removed.Therefore, the carbon monoxide burst size that how effectively to reduce the papermaking-method reconstituted tobaccos product is not only a urgent task of current tobacco industry, also is a technical barrier during reconstituted tobacco is produced.
The Chinese invention patent of application number 200910218320.3 once disclosed a kind of " applying nano materials reduces the method for carbon monoxide in flue gas of papermaking-method reconstituted tobaccos ", though patent adopts the method for adding nano material in reconstructed tobacco leaf slurry or dip-coating prepared opium paste can reach the purpose that reduces papermaking-method reconstituted tobaccos carbon monoxide burst size, but because the material that is added is the special rare nano-metal-oxide of a class, reduce effect but also need the higher amounts ratio can obtain certain carbon monoxide, therefore, this patent of invention will exist cost too high in actual production, apply difficult problem.
Summary of the invention
The objective of the invention is to problem at the prior art existence, a kind of economy is provided and effectively reduces the method for papermaking-method reconstituted tobaccos carbon monoxide burst size, it is characterized in that, when papermaking-method reconstituted tobaccos is produced, by add specific alkali metal inorganic acid salt in the product to reduce the burst size of papermaking-method reconstituted tobaccos carbon monoxide.
As follows for realizing the technical measures that purpose of the present invention adopts:
Painting process of producing at papermaking-method reconstituted tobaccos or perfuming operation or filler add operation, by 0.1%~4% adding proportion (mass ratio) of required converted products quality, with alkali metal inorganic acid salt Li
2SO
4, Na
2SO
4, K
2SO
4, Na
2CO
3, K
2CO
3, one or more the composite additives that form among NaCl, the KCl add in the papermaking-method reconstituted tobaccos and finally be processed into product.
Compare with the reference product of ordinary production, detect through main flume, the carbon monoxide burst size of the papermaking-method reconstituted tobaccos behind the interpolation alkali metal inorganic acid salt has obvious reduction.
The present invention adds the alkali metal inorganic acid salt in the papermaking-method reconstituted tobaccos product, make full use of the characteristic that the fusion at high temperature of alkali metal inorganic acid salt need absorb a large amount of heats and will influence papermaking-method reconstituted tobaccos fired state and ignition temperature, suppress the generation of part carbon monoxide papermaking-method reconstituted tobaccos when burning main flume from root, thereby reach the purpose of effective reduction papermaking-method reconstituted tobaccos product carbon monoxide burst size.
Compared with prior art, the present invention has following useful benefits:
1, the additive cost is low.The present invention is selected all to be some common and be easy to obtain alkali metal inorganic acid salts on the market, cheap, adding proportion is little, compares the chemical materials such as nano metal of the required interpolation of present reduction papermaking-method reconstituted tobaccos carbon monoxide burst size, and the additive cost is lower.
2, not obvious change product suction quality.The alkali metal inorganic acid salt that the present invention is selected, all be through experiment repeated screening and compliance test result, can be when optionally reducing papermaking-method reconstituted tobaccos carbon monoxide burst size, substantially do not influence the puff number and suction quality of product, add these materials and can not cause that the suction quality of product obviously changes.
3, the interpolation implementation is simple.The alkali metal inorganic acid salt that the present invention is selected, all be some additives that dissolve in painting process in the papermaking-method reconstituted tobaccos production, perfuming operation and filler interpolation operation production feed liquid, thereby as long as before pre-these materials are added in the production feed liquid in the above-mentioned operation by certain dosage and miscible evenly, can be easily the mode of alkali metal inorganic acid salt by ordinary production be joined the papermaking-method reconstituted tobaccos product.In above whole process, do not need to increase any production equipment, can not change existing papermaking-method reconstituted tobaccos production and processing technology yet, technical implementation way is simple.
4, reduction carbon monoxide effect is obvious.The alkali metal inorganic acid salt that the present invention is selected in the scope of the adding proportion 0.1%~4% of claim, can reach the purpose that reduces papermaking-method reconstituted tobaccos carbon monoxide burst size 5%~20%, and the harm reduction effect of product is obvious, selectivity is strong.
The specific embodiment
Below in conjunction with specific embodiment technical scheme of the present invention is described further:
Embodiment 1
The painting process of producing at papermaking-method reconstituted tobaccos, 1% adding proportion by required converted products quality will be dissolved with 2Kg Li in advance
2SO
4The coating feed liquid, evenly coat reconstituted tobacco sheet base and finally be processed into 200Kg papermaking-method reconstituted tobaccos product by the mode of ordinary production.
Embodiment 2
The painting process of producing at papermaking-method reconstituted tobaccos, 1% adding proportion by required converted products quality will be dissolved with 2Kg Na in advance
2SO
4The coating feed liquid, evenly coat reconstituted tobacco sheet base and finally be processed into 200Kg papermaking-method reconstituted tobaccos product by the mode of ordinary production.
Embodiment 3
The painting process of producing at papermaking-method reconstituted tobaccos, 1% adding proportion by required converted products quality will be dissolved with 2Kg K in advance
2SO
4The coating feed liquid, evenly coat reconstituted tobacco sheet base and finally be processed into 200Kg papermaking-method reconstituted tobaccos product by the mode of ordinary production.
Embodiment 4
The painting process of producing at papermaking-method reconstituted tobaccos, 1% adding proportion by required converted products quality will be dissolved with 2Kg Na in advance
2CO
3The coating feed liquid, evenly coat reconstituted tobacco sheet base and finally be processed into 200Kg papermaking-method reconstituted tobaccos product by the mode of ordinary production.
Embodiment 5
The painting process of producing at papermaking-method reconstituted tobaccos, 1% adding proportion by required converted products quality will be dissolved with 2KgK in advance
2CO
3The coating feed liquid, evenly coat reconstituted tobacco sheet base and finally be processed into 200Kg papermaking-method reconstituted tobaccos product by the mode of ordinary production.
Embodiment 6
Painting process in papermaking-method reconstituted tobaccos production, 1% adding proportion by required converted products quality, to be dissolved with the coating feed liquid of 2Kg NaCl in advance, evenly coat reconstituted tobacco sheet base and finally be processed into 200Kg papermaking-method reconstituted tobaccos product by the mode of ordinary production.
Embodiment 7
Painting process in papermaking-method reconstituted tobaccos production, 1% adding proportion by required converted products quality, to be dissolved with the coating feed liquid of 2KgKCl in advance, evenly coat reconstituted tobacco sheet base and finally be processed into 200Kg papermaking-method reconstituted tobaccos product by the mode of ordinary production.
Embodiment 8
The filler of producing at papermaking-method reconstituted tobaccos adds operation, and total adding proportion of 1.4% by required converted products quality will misciblely in advance have Li
2SO
4, Na
2SO
4, K
2SO
4, Na
2CO
3, K
2CO
3, NaCl, each 0.2Kg of KCl the filler feed liquid, by the mode of ordinary production reconstructed tobacco leaf slurry is carried out filler and adds and finally be processed into 100Kg papermaking-method reconstituted tobaccos product.
Embodiment 9
The perfuming operation of producing at papermaking-method reconstituted tobaccos, 0.2% adding proportion by required converted products quality will be dissolved with 0.2KgNa in advance
2SO
4The spices feed liquid, by the mode of ordinary production to the reconstituted tobacco perfuming and finally be processed into 100Kg papermaking-method reconstituted tobaccos product.
Embodiment 10
The perfuming operation of producing at papermaking-method reconstituted tobaccos, 3% adding proportion by required converted products quality will be dissolved with 3Kg Na in advance
2SO
4The spices feed liquid, by the mode of ordinary production to the reconstituted tobacco perfuming and finally be processed into 100Kg papermaking-method reconstituted tobaccos product.
The reference product that the papermaking-method reconstituted tobaccos product and the ordinary production of the foregoing description 1~10 do not added the alkali metal inorganic acid salt carries out respectively that main flume detects and the contrast of suction quality is smoked panel test, and the results are summarized in table 1.As can be seen from Table 1: in papermaking-method reconstituted tobaccos, add the specified alkali metal inorganic acid salt of patent of the present invention, obviously do not change product puff number and suction quality, but all have the selectivity of different amplitudes to reduce the carbon monoxide burst size of papermaking-method reconstituted tobaccos.
The main flume of table 1 embodiment 1~10 papermaking-method reconstituted tobaccos product and reference product detects and suction quality smoking result
Claims (3)
1. reduce the method for papermaking-method reconstituted tobaccos carbon monoxide burst size, it is characterized in that:, add the burst size that the alkali metal inorganic acid salt can reduce the papermaking-method reconstituted tobaccos carbon monoxide in painting process or perfuming operation or the filler interpolation operation that papermaking-method reconstituted tobaccos is produced.
2. the method for reduction papermaking-method reconstituted tobaccos carbon monoxide burst size according to claim 1 is characterized in that the alkali metal inorganic acid salt that is added is Li
2SO
4, Na
2SO
4, K
2SO
4, Na
2CO
3, K
2CO
3, one or more composite the forming among NaCl, the KCl.
3. the method for reduction papermaking-method reconstituted tobaccos carbon monoxide burst size according to claim 1 is characterized in that the adding proportion of alkali metal inorganic acid salt is 0.1~4% of a papermaking-method reconstituted tobaccos product quality.