CN101928802A - 用于球化包的聚渣方法 - Google Patents

用于球化包的聚渣方法 Download PDF

Info

Publication number
CN101928802A
CN101928802A CN 201010247481 CN201010247481A CN101928802A CN 101928802 A CN101928802 A CN 101928802A CN 201010247481 CN201010247481 CN 201010247481 CN 201010247481 A CN201010247481 A CN 201010247481A CN 101928802 A CN101928802 A CN 101928802A
Authority
CN
China
Prior art keywords
slag
poly
iron
nodularization bag
nodulizing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201010247481
Other languages
English (en)
Inventor
葛华光
田建军
朱传斌
李海顺
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hebei Xinxing Ductile Iron Pipes Co.,Ltd.
Original Assignee
Xinxing Ductile Iron Pipes Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xinxing Ductile Iron Pipes Co Ltd filed Critical Xinxing Ductile Iron Pipes Co Ltd
Priority to CN 201010247481 priority Critical patent/CN101928802A/zh
Publication of CN101928802A publication Critical patent/CN101928802A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种用于球化包的聚渣方法,该方法的步骤为:先将JF-2型聚渣剂加入球化包底部,加入量为球化包中铁水重量的1.5~2.5‰;然后兑铁,并搅拌进行球化处理。采用该方法可以有效防止球化包内壁夹渣,减少铁水氧化,使铁水更加纯净。

Description

用于球化包的聚渣方法
技术领域
本发明涉及一种用于球化包的聚渣方法。
背景技术
目前,铁液经过熔炼球化处理后,经常存在以下不足:1)铁水温度低时造成渣上浮不充分或拔渣不干净,这样使渣残留在铁水中;2)所加稀土在铁水中反应所产生的渣的比重与铁液比重相近,较难从铁液中上浮;3)铁液经镁处理后,铁液表面容易形成一层氧化膜。上述这些因素的存在,使球磨铸铁管在生产过程中容易造成内壁夹渣,影响球磨铸铁管的内在质量。
发明内容
本发明要解决的技术问题是提供一种用于球化包的聚渣方法,该方法可以减少球化包内壁夹渣,防止铁水氧化,使铁水纯净。
为解决上述技术问题,本发明所采取的技术方案是:用于球化包的聚渣方法,所述方法的步骤为:
1)将JF-2型聚渣覆盖剂加入球化包底部,加入量为球化包中铁水重量的1.5~2.5‰;
2)兑铁,并搅拌进行球化处理。
优选的,上述JF-2型聚渣覆盖剂加入量为球化包中铁水重量的2‰;
优选的,上述JF-2型聚渣覆盖剂各组份的重量份数为:SiO2 62~65,Al2O312~15,Fe2O3 2.3,FeO 0.5,NaO 1.5,K2O 1.3。
采用上述技术方案所产生的有益效果在于:1、本方法操作简单,操作性强;
2、加入本聚渣剂后,进行球化处理时进行搅拌,使聚渣剂与铁液中的渣结合,由于聚渣剂比重比铁液比重小,这样可使与聚渣剂结合后的渣上浮,从而在铁液表面形成20~30mm厚的渣层,使铁液表面与空气隔绝,不仅可效防止铁水氧化,还可使铁水更加纯净。
具体实施方式
下面结合具体实施方式对本发明作进一步详细的说明。
一般使用的球化包可装6吨铁水,在往球化包兑铁之前,将称量好的JF-2型聚渣覆盖剂加入球化包包底,加入量为12kg(9kg或15kg也可以),然后兑铁,进行球化处理,同时进行不断的搅拌。加入本聚渣剂后经过球化处理时的搅拌作用使聚渣剂与铁液中的渣结合,由于聚渣剂的比重为1.2-1.4,比铁液的比重轻,这样就可以使与聚渣剂结合后的渣上浮,从而在铁液表面形成20~30mm厚的渣层,使铁液表面与空气隔绝,防止铁水氧化。

Claims (3)

1.用于球化包的聚渣方法,其特征在于:所述方法的步骤为:
1)将JF-2型聚渣覆盖剂加入球化包底部,加入量为球化包中铁水重量的1.5~2.5‰;
2)兑铁,并搅拌进行球化处理。
2.根据权利要求1所述的用于球化包的聚渣方法,其特征在于:JF-2型聚渣覆盖剂加入量为球化包中铁水重量的2‰。
3.根据权利要求1或2所述的用于球化包的聚渣方法,其特征在于:所述JF-2型聚渣覆盖剂各组份的重量份数为:SiO2 62~65,Al2O3 12~15,Fe2O3 2.3,FeO 0.5,NaO 1.5,K2O 1.3。 
CN 201010247481 2010-08-09 2010-08-09 用于球化包的聚渣方法 Pending CN101928802A (zh)