CN101879650A - 一种弯管熔透焊接方法 - Google Patents

一种弯管熔透焊接方法 Download PDF

Info

Publication number
CN101879650A
CN101879650A CN2009100507443A CN200910050744A CN101879650A CN 101879650 A CN101879650 A CN 101879650A CN 2009100507443 A CN2009100507443 A CN 2009100507443A CN 200910050744 A CN200910050744 A CN 200910050744A CN 101879650 A CN101879650 A CN 101879650A
Authority
CN
China
Prior art keywords
welding
submerged arc
bend pipe
arc welding
weld
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2009100507443A
Other languages
English (en)
Inventor
贾建波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CMTCC Shanghai Shisanye Construction Co Ltd
Original Assignee
CMTCC Shanghai Shisanye Construction Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CMTCC Shanghai Shisanye Construction Co Ltd filed Critical CMTCC Shanghai Shisanye Construction Co Ltd
Priority to CN2009100507443A priority Critical patent/CN101879650A/zh
Publication of CN101879650A publication Critical patent/CN101879650A/zh
Pending legal-status Critical Current

Abstract

本发明涉及焊接方法,尤其涉及一种弯管焊接方法。一种弯管熔透焊接方法,它包括一埋弧焊机,一套焊接转台,所述埋弧焊机带有行走轮、行走导轮,所述焊接方法包括:将卷制的弯管管件的内外直缝采用埋弧焊焊接并校园步骤;将一套焊接转台按照弯管的夹角放置步骤;将待焊接的管件分别置于焊接转台的转台轮上步骤;将埋弧焊机置于管件上进行环缝焊接步骤。本发明焊接质量稳定,焊接速度快,劳动强度相对较低。

Description

一种弯管熔透焊接方法
技术领域
本发明涉及焊接方法,尤其涉及一种弯管焊接方法。
本发明适用于焊缝质量等级及外观要求较高的板厚6mm以上,管直径大于800mm,角度小于45°的弯管熔透焊接。
背景技术
当前,弯管直缝和环缝焊接全部采用手工电弧焊接和手工气保焊接,焊接质量受人为因素影响较大;而且焊接过程机械化程度较低,焊工劳动强度大;焊接速度较慢,焊缝一次合格率较低。
发明内容
本发明旨在解决上述缺陷,提供一种弯管熔透焊接方法。本发明焊接质量稳定,焊接速度快,劳动强度相对较低。
本发明是这样实现的,
一种弯管熔透焊接方法,它包括一埋弧焊机,一套焊接转台,所述埋弧焊机带有行走轮,所述焊接方法包括:
将卷制的弯管管件的内外直缝采用埋弧焊焊接并校园步骤;
将两个焊接转台按照弯管的夹角放置步骤;
将待焊接的管件分别置于焊接转台的转台轮上步骤;
将埋弧焊机置于管件上进行环缝焊接步骤。
所述的一种弯管熔透焊接方法,所述将埋弧焊机置于管件上进行环缝焊接步骤包括将埋弧焊机放置在一个待焊接的管件之上,转台匀速旋转,埋弧焊机以同等速度与转台旋转相反方向行走进行焊接。
所述的一种弯管熔透焊接方法,所述埋弧焊机还包括一个由连接杆连接的一个导向行走轮。
本发明对于弯管直缝和环缝全部采用埋弧焊接,提高了机械化程度,减小了工人劳动强度,减小了人为因素对焊接质量的影响。提高了焊接速度、质量,提高了焊缝合格率,减少了焊缝返工率,提高了焊接效率,降低了焊接成本,减小了环境污染。
附图说明
下面,结合附图进一步说明发明的具体实施方式:
图1为本发明示意图;
图2为所述埋弧焊机行走轮和行走导轮示意图。
具体实施方式
如图1所示,一种弯管熔透焊接方法,它包括一埋弧焊机1,一套焊接转台2,所述埋弧焊机1带有行走轮3;所述埋弧焊机还包括一个由连接杆连接的一个导向行走轮6(从图2可见),所述焊接方法包括:
将卷制的弯管管件4的内外直缝采用埋弧焊焊接并校园步骤;
将一套焊接转台2按照弯管的夹角放置步骤;
将待焊接的管件4分别置于焊接转台2的转台轮5上步骤;
将埋弧焊机1置于管件4上进行环缝焊接步骤。
所述的一种弯管熔透焊接方法,埋弧焊机的行走轮3和行走导轮6分别放置在一个待焊接的管件4上,行走导轮6放置于管件4的对接焊缝坡口内,坡口作为行走导轮的导轨进行焊接。
焊接时转台匀速旋转,埋弧焊机焊接时行走速度与管道旋转速度相等,方向相反,焊机行走轮在弯管表面行走,行走导轮在弯管对接焊缝坡口之内行走,焊缝坡口作为行走导轮导轨。

Claims (3)

1.一种弯管熔透焊接方法,它包括一台埋弧焊机,一套焊接转台,其特征在于,所述埋弧焊机带有行走轮,所述焊接方法包括:
将卷制的弯管管件的内外直缝采用埋弧焊焊接并校园步骤;
将一套焊接转台按照弯管的夹角放置步骤;
将待焊接的管件分别置于焊接转台的转台轮上步骤;
将埋弧焊机置于管件上进行环缝焊接步骤。
2.根据权利要求1所述的一种弯管熔透焊接方法,其特征在于,所述将埋弧焊机置于管件上进行环缝焊接步骤包括将埋弧焊机放置在一个待焊接的管件之上,转台匀速旋转,埋弧焊机以同等速度与转台旋转相反方向行走进行焊接。
3.根据权利要求1或2所述的一种弯管熔透焊接方法,其特征在于,所述埋弧焊机还包括一个由连接杆连接的一个导向行走轮。
CN2009100507443A 2009-05-07 2009-05-07 一种弯管熔透焊接方法 Pending CN101879650A (zh)