CN101852713B - 一种测量玻璃纸水汽渗透性的方法 - Google Patents

一种测量玻璃纸水汽渗透性的方法 Download PDF

Info

Publication number
CN101852713B
CN101852713B CN2009100203005A CN200910020300A CN101852713B CN 101852713 B CN101852713 B CN 101852713B CN 2009100203005 A CN2009100203005 A CN 2009100203005A CN 200910020300 A CN200910020300 A CN 200910020300A CN 101852713 B CN101852713 B CN 101852713B
Authority
CN
China
Prior art keywords
vapor permeability
sample
paper
viscose paper
screw cover
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2009100203005A
Other languages
English (en)
Other versions
CN101852713A (zh
Inventor
张晓煜
王晓荣
张文文
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG HENGLIAN NEW MATERIALS CO., LTD.
Original Assignee
WEIFANG HENGLIAN CELLOPHANE CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WEIFANG HENGLIAN CELLOPHANE CO Ltd filed Critical WEIFANG HENGLIAN CELLOPHANE CO Ltd
Priority to CN2009100203005A priority Critical patent/CN101852713B/zh
Publication of CN101852713A publication Critical patent/CN101852713A/zh
Application granted granted Critical
Publication of CN101852713B publication Critical patent/CN101852713B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种测量玻璃纸水汽渗透性的方法,其步骤是在一铝盘内放置一定重量的硅胶并置于干燥器内,然后将事先切取好的试样覆盖在铝盘上并拧紧螺钉盖,称量后得重量G1g,然后将上述铝盘放在水汽渗透仪内,在一定条件下放置24小时后取出,称得重量为G2g,用G2-G1然后乘以200(g/m2·24h)即得待测试样的水汽渗透性。本发明所述的测量方法操作简便,所使用的工具、设备简单易得,测量费用低。使用本发明所述的测量方法,可以较为准确的测量出玻璃纸的水汽渗透性。

Description

一种测量玻璃纸水汽渗透性的方法
技术领域
本发明属于一种测量玻璃纸水汽渗透性的方法。
背景技术
玻璃纸具有高透明度以及阻隔、抗热、抗静电、防水、防潮等性能,尤其是其具有的防水、防潮性及强热封性等优点,用其作为包装材料时有利于被包装物品存放寿命的延长,因此,近年来被越来越多地用作包装材料尤其是食品类包装材料。当玻璃纸被用作食品类包装材料尤其是液体类食品以及其他需要较好密封性食品的包装材料时,其水汽渗透性必须符合一定标准,这就需要玻璃纸的生产厂家对玻璃纸的水汽渗透性进行准确的测量。目前尚没有一种规范而又准确的测量玻璃纸水汽渗透性的方法应用于生产实践中。
发明内容
本发明的目的是提供一种可以准确测量玻璃纸水汽渗透性的方法。
为实现上述目的,本发明的技术方案是采取以下步骤:
a、在待测玻璃纸上切取一定大小且具有一定形状的试样若干块;
b、在大小形状与上述试样相应且带有螺钉盖的铝盘内置放一定重量的硅胶,并将该铝盘置于干燥器内,然后将试样覆盖在铝盘上,拧紧螺钉盖;
c、将拧好螺钉盖的铝盘快速称重,得重量G1(g);
d、将上述铝盘放在水汽渗透仪内,在一定条件下,24小时后取出,放在干燥器内,快速称重,得重量G2(g);
e、按照下式计算试样的水汽渗透性:
水汽渗透性=(G2-G1)×200(g/m2·24h)
f、按照上述步骤,计算其他试样的水汽渗透性,然后取其平均值,即为待测玻璃纸的水汽渗透性。
按照上述方法测量玻璃纸的水汽渗透性,a步骤中切取试样时,使用冲床切取2块圆形试样,每块圆形试样的直径为88mm。b步骤中所使用的硅胶为变色硅胶,其重量为10g;拧紧螺钉盖时,要确保试样的纸面平整光滑,纸面与螺钉盖接触的部位无任何缝隙。d步骤中所说的一定条件是指在温度为38℃、相对湿度为85%rh的条件下。
本发明较好的解决了玻璃纸水汽渗透性的规范测量问题。本发明所述的测量方法操作简便,所使用的工具、设备简单易得,测量费用低。使用本发明所述的测量方法,可以较为准确的测量出玻璃纸的水汽渗透性,避免因玻璃纸的水汽渗透性不够而影响产品的质量,可为产品质量的提高提供重要保证。
具体实施方式
实施例1、使用冲床在待测玻璃纸上切取2块直径为88mm的圆形试样;调整QYPT130水汽渗透仪,使其温度为38℃,相对湿度为85%rh;在大小形状与所取试样相应且带有螺钉盖的铝盘内置放10g变色硅胶,并将铝盘置于干燥器内,然后将第一块试样覆盖在铝盘上,拧紧螺钉盖;注意在拧紧螺钉盖时,要确保试样的纸面平整光滑,纸面与螺钉盖接触的部位无任何缝隙;将拧紧螺钉盖的铝盘在电子天平上快速称重,称得重量G1为169.04g;将称重后的铝盘放在水汽渗透仪内,在温度为38℃,相对湿度为85%rh的条件下,放置24小时后取出,放在干燥器内,用电子天平快速称得重量G2为169.14g;按照下式计算试样的水汽渗透性:
水汽渗透性=(G2-G1)×200(g/m2·24h)=20(g/m2·24h)
用同样的方法测得第二块试样的水汽渗透性为24(g/m2·24h);两块试样水汽渗透性的平均值为22(g/m2·24h),即所测玻璃纸的水汽渗透性为22(g/m2·24h)。

Claims (6)

1.一种测量玻璃纸水汽渗透性的方法,其特征是采取以下步骤:
a、在待测玻璃纸上切取一定大小且具有一定形状的试样若干块;
b、在大小形状与上述试样相应且带有螺钉盖的铝盘内置放一定重量的硅胶,并将该铝盘置于干燥器内,然后将试样覆盖在铝盘上,拧紧螺钉盖;拧紧螺钉盖时,要确保试样的纸面平整光滑,纸面与螺钉盖接触的部位无任何缝隙;
c、将拧好螺钉盖的铝盘快速称重,得重量G1(g);
d、将上述铝盘放在水汽渗透仪内,在一定的温度和相对湿度的条件下,24小时后取出,放在干燥器内,快速称重,得重量G2(g);
e、按照下式计算试样的水汽渗透性:
水汽渗透性=(G2-G1)×200(g/m2·24h)
f、按照上述步骤,计算其他试样的水汽渗透性,然后取其平均值,即为待测玻璃纸的水汽渗透性。
2.如权利要求1所述的测量玻璃纸水汽渗透性的方法,其特征是a步骤中切取试样时,使用冲床切取圆形试样。
3.如权利要求2所述的测量玻璃纸水汽渗透性的方法,其特征是圆形试样的直径为88mm。
4.如权利要求1所述的测量玻璃纸水汽渗透性的方法,其特征是a步骤中切取试样的数量为2块。
5.如权利要求1所述的测量玻璃纸水汽渗透性的方法,其特征是b步骤中所使用的硅胶为变色硅胶,其重量为10g。
6.如权利要求1所述的测量玻璃纸水汽渗透性的方法,其特征是d步骤中所说的一定的温度和相对湿度是指在温度为38℃、相对湿度为85%rh。
CN2009100203005A 2009-04-06 2009-04-06 一种测量玻璃纸水汽渗透性的方法 Active CN101852713B (zh)