CN101768646B - 鹅绒皮的制备方法 - Google Patents
鹅绒皮的制备方法 Download PDFInfo
- Publication number
- CN101768646B CN101768646B CN 201010102475 CN201010102475A CN101768646B CN 101768646 B CN101768646 B CN 101768646B CN 201010102475 CN201010102475 CN 201010102475 CN 201010102475 A CN201010102475 A CN 201010102475A CN 101768646 B CN101768646 B CN 101768646B
- Authority
- CN
- China
- Prior art keywords
- goose down
- down fur
- fur
- dehydration
- clean
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明涉及一种制备鹅绒皮的方法和设备,通过专用设备完成鹅绒皮的机械处理和化学处理,包括搅拌清洗、挤压脱脂、鞣制、烘干等步骤,使用本发明制备的鹅绒皮板柔软且抗拉强度好、绒毛致密、丰满、不怕水、不脱毛、色泽光亮洁白。
Description
技术领域:
本发明属原皮的机械处理和化学处理及所用设备,特别涉及一种鹅绒皮的制备工艺方法。所用设备及用该方法,设备生产出的鹅绒皮。
背景技术:
当前,随着人们生活水平的提高,裘皮服装以它保暖性能好的特点,穿着华贵高雅的仪态越来越受到人们的青睐,在国内外裘皮服装多采用动物皮革制作,用禽类皮革制作的服装很少见,尤其是鹅绒皮的更是绝无仅有。鹅绒皮轻而柔,保暖性强,不怕水,光亮洁白,在国际市场上用本发明制备的鹅绒皮样品成为抢手货。
传统的制备动物皮革的技术通常能制得原皮较厚,较坚硬的皮革,但不能制得原皮较薄,绒毛致密且强度好的鹅绒皮。
由于特殊制备鹅绒皮的工艺方法决定了所用设备与制备动物皮革设备的不同,必须设计一条专线设备,才能完成鹅绒皮的制备。
本发明的目的在于提供一种制备柔软易揉而又具有高强度的鹅绒皮的方法。
本发明的另一个目的在于设计一种能够对鹅原皮进行机械处理和化学处理并缩短制备周期的专用设备。
本发明的目的也涉及通过使用该设备方法及设备得到的鹅绒皮。
发明内容:
本发明的技术解决方案是:
制备方法的特征在于:
(a)清洗:将剥下的鹅绒皮放入清洗机(1)内,注入适量清水,加入适量清洗剂,搅拌清洗
(b)脱水:清洗后的鹅绒皮置于脱水机(2)中,脱水处理。
(c)脱脂:脱水后的鹅绒皮放在脱脂机(3)中,加热30-40℃,脱脂。
(d)清洗:脱脂后的鹅绒皮放入清洗机(1)中,注入适量清水,加入适量清洗剂,搅拌清洗
(e)脱水:将清洗后的鹅绒皮置于脱水机(2)中,脱水处理
(f)鞣制:将脱水后的鹅绒皮平铺在处理台(4)上,用喷雾将已配好的化学原料均匀地喷在鹅绒皮上,静置2-3小时
(g)清洗:鞣制后的鹅绒皮放入清洗机(1)中,注入适量清水,加入适量清洗剂及强碱,搅拌清洗
(h)脱水:洗涤后的鹅绒皮置于脱水机中,脱水处理
(i)烘干:脱水后的鹅绒皮平整码放在烘干机(5)内,在温度60-80℃下,历时4-5小时取出
附图说明:
图1、本发明的制备工艺流程图
图2、本发明所用设备排列示意图
(1)清洗机
(2)脱水机
(3)脱脂机
(4)处理台
(5)烘干机
具体实施方式:
根据本发明的一个优选实施例,在步骤(f)中的化学溶液配比(按每一平方英尺计算),食盐0.5-1.2g,盐酸0.2-0.3,草酸0.8-1.2g,硝酸钠0.4-0.55g,柴油0.4-0.8g。
使用上述方法制备鹅绒皮所用设备的特征在于它包括清洗机、脱水机、脱脂机、处理台、烘干机。
使用上述方法和设备制备的鹅绒皮
实施例:
图1为本发明的制备方法步骤如下:
(a)清洗:将剥下的鹅绒皮放入清洗机内(按每平方英尺计算),注入1300-1500g,温度为55℃,加入0.2-0.4g清洗剂,进行搅拌洗涤,清除鹅原皮表面的杂质,脏物。清洗机内可一次洗涤40平方英尺,洗涤时间为15分钟。
(b)脱水:将洗涤干净的鹅绒皮置于脱水机中,进行脱水处理,一次可处理 15平方英尺,脱水时间为6分钟。
(c)脱脂:将脱水后的鹅绒皮放入脱脂机中进行脱脂处理,20分钟可脱脂30平方英尺的鹅绒皮。
(d)清洗:经脱脂后的鹅绒皮放入清洗机中,(按每平方英尺计算)注入1700-2000g温度为40℃的清水,加入0.5-0.6g清洗剂,清除鹅绒皮上剩余的脏物和残留在表皮的油脂。一次可清洗40平方英尺,洗涤时间为10分钟。
(e)脱水:将洗涤干净的鹅绒皮置于脱水机内,进行脱水处理。一次可处理20平方英尺,脱水时间为8分钟。
(f)鞣制:将脱水后的鹅绒皮平铺在处理台上,一次可处理260平方英尺,用喷雾器将配方(按每平方英尺计算)食盐0.5-1.2g,盐酸0.2-0.3,草酸0.8-1.2g,硝酸钠0.4-0.55g,柴油0.4-0.8g的溶液均匀地喷在鹅绒皮的内外皮表面,静置2-3小时。可以得到既柔软又足够致密的且强度高的鹅绒皮。
(g)清洗:将鞣制后的鹅绒皮放入清洗机中,按(每平方英尺)注入1700-2000g温度为20℃,的清水中,加入清洗剂0.2-0.4g,强碱0.2-0.3g洗涤,目的是将鞣制熟化期的鹅绒皮进行除酸清洗,一次可清洗40平方英尺,洗涤时间为10分钟。
(h)脱水:将除酸洗涤后的鹅绒皮放在烘干机中,一次可烘干400平方英尺,烘干温度为50-60℃,历时4-5小时取出。
图2为本发明所用设备排列示意图,根据鹅绒皮的制备工艺流程设计清洗机,脱水机、脱脂机、处理台、烘干机五种专用设备。
按照上述方法和设备制备出的鹅绒皮一平方英寸拉力可达25公斤,可以制作各式裘皮服装、帽子、围脖、手套等。
本发明具有如下优点:
1、可缩短制备周期,由原来的七天缩短八小时,即可出产品,提高了经济效益。
2、本发明制备的鹅绒皮柔软且抗拉强度好,绒毛致密,丰满、不脱毛。厚度可达2公分,保暖性能好。
3、鹅绒皮不怕水,绒毛手感细腻,色泽光亮。洁白可与狐狸皮、貂皮相媲美。
Claims (1)
1.一种制备鹅绒皮的方法,其特征在于:
(a)清洗:将剥下的鹅绒皮放入清洗机(1)内,注入适量清水,加入适量清洗剂,搅拌清洗;
(b)脱水:脱水后的鹅绒皮置于脱水机(2)中,脱水处理;
(c)脱脂:脱水后的鹅绒皮放在脱脂机(3)中,加热30-40℃,脱脂;
(d)清洗:脱脂后的鹅绒皮放入清洗机(1)中,注入适量清水,加入适量清洗剂,搅拌清洗;
(e)脱水:脱水后的鹅绒皮置于脱水机(2)中,脱水处理;
(f)鞣制:将脱水后的鹅绒皮平铺在处理台(4)上,用喷雾将已配好的化学溶液均匀地喷在鹅绒皮上,静置2-3小时;
(g)清洗:鞣制后的鹅绒皮放入清洗机(1)中,注入适量清水,加入适量清洗剂及强碱,搅拌清洗;
(h)脱水:洗涤后的鹅绒皮置于脱水机中,脱水处理;
(i)烘干:脱水后的鹅绒皮平整码放在烘干机(5)内,在温度60—80℃下,历时4—5小时取出;
其中,步骤(f)中的化学溶液配比:食盐0.5-1.2g,盐酸0.2-0.3 g,草酸0.8-1.2g,硝酸钠0.4-0.55g,柴油0.4-0.8g。