CN101716820A - 表面复合层原料节约型中空模头芯棒 - Google Patents
表面复合层原料节约型中空模头芯棒 Download PDFInfo
- Publication number
- CN101716820A CN101716820A CN200910253397A CN200910253397A CN101716820A CN 101716820 A CN101716820 A CN 101716820A CN 200910253397 A CN200910253397 A CN 200910253397A CN 200910253397 A CN200910253397 A CN 200910253397A CN 101716820 A CN101716820 A CN 101716820A
- Authority
- CN
- China
- Prior art keywords
- die head
- core rod
- perpendicular muscle
- filling channel
- composite layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了表面复合层原料节约型中空模头芯棒,芯棒内置在中空模头内,芯棒上具有中空板材竖筋成型部位和物料导流部位,芯棒具有用来预先填充竖筋成型部位的预填充通道,该预填充通道对称设置在芯棒两侧,用以连通挤出模头内的熔体通道和竖筋成型部位,使得预填充通道中的料流先于熔体通道内料流填充竖筋成型部位,使得竖筋中原料大部分来源于预填充通道,表面复合层在中空板材竖筋部位不再凹陷,表面覆盖均匀,表面原料不再多余使用,节约了成本,改善了产品结构。
Description
技术领域
本发明涉及挤出模具领域,具体涉及一种中空模头芯棒。
背景技术
目前,中空板材是通过挤出模具进行挤出后成型,挤出熔体通道里具有两层物料或多层物料,外层为复合层,覆盖在中空板材上下表面,原料层为成型中空板材主体。现有技术中,中空模头芯棒如图1所示,芯棒1′上具有中空板材内竖筋成型部位2′和物料导流部位3′,E方向为料流挤出填充方向。在该结构中,物料导流部位3′顺着E方向看是顺三角形,三角形的顶点在出料方向,在熔体通道里的两层物料经过模头熔体通道由E方向填充竖筋成型部位2′,此时会产生外层复合层往中空板材内的竖筋部位凹陷,挤出后中空板材的截图如图2所示,这个凹陷4′存在会导致外层复合层物料的多余使用,并且从结构上来并不完善,需要解决这个技术问题。
发明内容
本发明的目的在于提供一种表面复合层原料节约型中空模头芯棒,可以解决中空板材外层复合层物料凹陷的技术问题,提高外层复合层物料的使用效率,使得成型后的中空板材结构更加完善。
表面复合层原料节约型中空模头芯棒,芯棒内置在中空模头内,芯棒上具有中空板材竖筋成型部位和物料导流部位,其特征在于:芯棒具有用来预先填充竖筋成型部位的预填充通道,该预填充通道对称设置在芯棒两侧,用以连通挤出模头内的熔体通道和竖筋成型部位,使得预填充通道中的料流先于熔体通道内料流填充竖筋成型部位,使得竖筋中原料大部分来源于预填充通道。
所述的竖筋成型部位包括有预进料部位,其中预进料部位呈三角形,三角形顶点位于进料方向,预进料部位汇集两侧预填充通道内的料流。
所述的物料导流部位为预填充通道和竖筋成型部位的相隔离部分,熔体通道内的内层物料部分先分流进入预填充通道后,熔体通道内的主料流再经过物料导流部位后填充竖筋成型部位。
本发明相比现有技术,具有如下优点:
1、挤出模头熔体通道内的内层物料部分先分流进入预填充通道后,熔体通道内的主料流再经过物料导流部位后填充竖筋成型部位,使得竖筋中原料大部分来源于预填充通道,这样的结构就不会产生外层物料往中空板材内的竖筋部位凹陷,挤出成型后外层物料均匀地覆盖在中空板材表面,使得产品表面均匀,外层物料不被多余使用,产品结构完善。
附图说明
图1为现有技术中空模头芯棒结构示意图;
图2为现有技术挤出成型后产品结构剖面图;
图3为本发明中空模头芯棒结构示意图;
图4为本发明中空模头芯棒另一角度示意图;
图5为本发明芯棒内置在中空模头内的结构示意图;
图6为本发明挤出成型后产品结构剖面图。
具体实施方式
下面结合附图对本发明作进一步说明。
如图1、2所示,为现有技术中空模头芯棒的结构以及挤出产品结构剖面图,芯棒1′上具有中空板材内竖筋成型部位2′和物料导流部位3′,E方向为料流挤出填充方向。在该结构中,物料导流部位3′顺着E方向看是顺三角形,三角形的顶点在出料方向,在熔体通道里的两层物料经过模头熔体通道由E方向填充竖筋成型部位2′,此时会产生外层复合层往中空板材内的竖筋部位凹陷,挤出后中空板材的截图如图2所示,这个凹陷4′存在会导致外层复合层物料的多余使用。
如图3、4、5所示,表面复合层原料节约型中空模头芯棒,芯棒1内置在中空模头8内,芯棒1为中空模头熔体通道9的组成部分,芯棒1根据所需中空板材制作要求设置有多个竖筋成型部位2和物料导流部位3,在芯棒1两侧对称设置有用来预先填充竖筋成型部位2的预填充通道4,该预填充通道4用以连通挤出模头内的熔体通道9和竖筋成型部位2。竖筋成型部位2包括有预进料部位21,其中预进料部位21呈三角形,三角形顶点位于进料方向,预进料部位21汇集两侧预填充通道4内的料流。当熔体通道内的物料挤出时,预填充通道4中的料流先于熔体通道9内料流汇集填充竖筋成型部位2,使得中空板材竖筋中原料大部分来源于预填充通道4。
如图5所示,所述的物料导流部位3为预填充通道6和竖筋成型部位2相隔离部分,熔体通道9内的内层物料部分B先分流进入预填充通道4后,熔体通道9内的主料流再经过物料导流部位3后填充竖筋成型部位2,此时挤出产品剖面如图6所示,A所指为复合层,A均匀地覆盖在B表面,在中空板材竖筋部位不再凹陷,表面复合层原料不再多余使用,节约了成本,改善了产品结构。
Claims (3)
1.表面复合层原料节约型中空模头芯棒,芯棒内置在中空模头内,芯棒上具有中空板材竖筋成型部位和物料导流部位,其特征在于:芯棒具有用来预先填充竖筋成型部位的预填充通道,该预填充通道对称设置在芯棒两侧,用以连通挤出模头内的熔体通道和竖筋成型部位,使得预填充通道中的料流先于熔体通道内料流填充竖筋成型部位。
2.如权利要求1所述的表面复合层原料节约型中空模头芯棒,其特征在于:所述的竖筋成型部位包括有预进料部位,其中预进料部位呈三角形,三角形顶点位于进料方向,预进料部位汇集两侧预填充通道内的料流。
3.如权利要求1或2所述的表面复合层原料节约型中空模头芯棒,其特征在于:所述的物料导流部位为预填充通道和竖筋成型部位相隔离部分,熔体通道内的内层物料部分先分流进入预填充通道后,熔体通道内的主料流再经过物料导流部位后填充竖筋成型部位。