CN101654251A - 硅橡胶裂解灰渣的回收处理方法 - Google Patents

硅橡胶裂解灰渣的回收处理方法 Download PDF

Info

Publication number
CN101654251A
CN101654251A CN200910192301A CN200910192301A CN101654251A CN 101654251 A CN101654251 A CN 101654251A CN 200910192301 A CN200910192301 A CN 200910192301A CN 200910192301 A CN200910192301 A CN 200910192301A CN 101654251 A CN101654251 A CN 101654251A
Authority
CN
China
Prior art keywords
silicon rubber
waste residue
cracking waste
rubber cracking
processing method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN200910192301A
Other languages
English (en)
Inventor
吴世维
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN200910192301A priority Critical patent/CN101654251A/zh
Publication of CN101654251A publication Critical patent/CN101654251A/zh
Pending legal-status Critical Current

Abstract

本发明涉及硅橡胶裂解废渣的回收处理方法,其特征是把酸性灰渣中和、干燥后再经500~1200℃煅烧1~5小时,用此方法回收的填料(二氧化硅)具有质量稳定、品质高、颗粒均匀、颜色一致,并具有工艺和设备简单,生产过程无污染等特点。

Description

硅橡胶裂解灰渣的回收处理方法
技术领域
本发明涉及一种化工废料的回收利用,特别是一种硅橡胶裂解灰渣的回收利用处理方法。
背景技术
在现在的化工生产企业中,“三废”的回收和综合利用,关系到企业的生产成本和环境污染问题,甚至关系到企业的存亡问题。硅橡胶是一种优良的材料,广泛用于国防和各行各业的产品上,而使用过程中所产生的大量边角废料,用物理和生化的方法不能解除其对环境的污染,因而,人们利用硅橡胶的边角废料通过化学的裂解方法回收有机硅环体,加以利用。而在这一过程中也产生了大量的酸性粉尘和灰渣,即硅橡胶裂解灰渣,其主要成份为二氧化硅,这些灰渣的酸性很强,不能直接应用。专利号为200610035221.8的“一种硅橡胶裂解渣回收利用方法”则把这种裂解灰渣采用化工生产中的常用方法,即:中和→干燥→粉碎的方法回收“粉体”,以作填料使用。但这样处理和回收的“粉体”,由于技术上的缺陷,导致回收的产品(粉体)质量不稳定、杂质多、颗粒大细不均匀、颜色各异等问题,直接影响填料的应用。
发明内容
本发明的目的是利用化学和物理的处理方法,回收硅橡胶裂解灰渣中的有效成份——二氧化硅,并提高其品质,使其适用于化工、橡胶等行业作为填充剂使用。本发明是以如下的方法实现的:
一种硅橡胶裂解灰渣的回收处理方法,包括把灰渣进行中和、干燥、粉碎和筛分,其特征是把灰渣经中和、干燥后,再经500~1200℃煅烧1~5小时,然后再进行粉碎、筛分。其实际处理过程是把硅橡胶裂解灰渣送入专用的中和槽内,加水进行搅拌,并加入碱进行中和,调节PH值至中性,灰渣经脱水后送到干燥设备中进行干燥,并经煅烧炉在500~1200℃高温煅烧1~5小时,除去杂质,冷却后的灰渣送入特种磨碎机中进行粉碎,再经震动筛筛分成合格的二氧化硅,包装后即可出厂作填料。
本发明具有工艺、设备简单,生产过程无污染,产品质量稳定、品质高、成本低的特点。
以下结合附图对本发明的实施作进一步详细的描述:
附图说明
图1是本发明的灰渣回收处理流程示意图
具体实施方式
如图1所示,一种硅橡胶裂解灰渣的回收处理方法,包括把裂解灰渣进行中和、干燥、粉碎和筛分,其特征是把灰渣经中和、干燥后,再经500~1200℃煅烧,煅烧时间为1~5小时,然后进行粉碎、筛分。
实施例1:
把硅橡胶裂解灰渣送入中和槽内,加水进行搅拌,并加入碱进行中和,调节PH到中性,灰渣经离心机脱水后送至干燥设备中干燥,干燥后的灰渣送入煅烧炉内在700℃高温煅烧3小时,冷却后的灰渣送入磨碎机中粉碎,再经震动筛筛分后包装。
实施例2:
按照实施例1的方法,灰渣在煅烧炉内的煅烧温度为800℃煅烧,煅烧时间3小时。
实施例3:
按照实施1的方法,灰渣在煅烧炉内的煅烧温度为900℃,煅烧时间3小时。

Claims (1)

1.一种硅橡胶裂解灰渣的回收处理方法,包括把裂解灰渣进行中和、干燥、粉碎和筛分,其特征是把灰渣经中和、干燥后,再经500~1200℃煅烧1~5小时,然后进行粉碎、筛分。
CN200910192301A 2009-09-11 2009-09-11 硅橡胶裂解灰渣的回收处理方法 Pending CN101654251A (zh)