CN101624264A - 玻璃或陶瓷酒瓶防伪方法 - Google Patents

玻璃或陶瓷酒瓶防伪方法 Download PDF

Info

Publication number
CN101624264A
CN101624264A CN200810126199A CN200810126199A CN101624264A CN 101624264 A CN101624264 A CN 101624264A CN 200810126199 A CN200810126199 A CN 200810126199A CN 200810126199 A CN200810126199 A CN 200810126199A CN 101624264 A CN101624264 A CN 101624264A
Authority
CN
China
Prior art keywords
parts
glaze
glass
counterfeit
oxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN200810126199A
Other languages
English (en)
Other versions
CN101624264B (zh
Inventor
黄杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Cui Can
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2008101261997A priority Critical patent/CN101624264B/zh
Publication of CN101624264A publication Critical patent/CN101624264A/zh
Application granted granted Critical
Publication of CN101624264B publication Critical patent/CN101624264B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种玻璃或陶瓷酒瓶防伪方法,所述方法为使用多层釉料在水转印纸上做多层丝网印刷制作成防伪标识,利用一次烧结技术把水转印纸防伪标识烧结在玻璃或陶瓷表面;烧结温度为400-600℃,烧结时间为1.5-4小时;其中,至少一层釉料为夜光釉料,底层釉料在高温下可以和玻璃或陶瓷表面完全结合,中层釉料和底层釉料在高温下结合在一起,中层印刷防伪标识,表层为夜光釉料烧结后可以剥离,剥离后可以看到中层图案和数字,且剥离后不可以原样复原。本发明使使用过的酒瓶不容易被重复回收利用,从而达到打假防假的目的。

Description

玻璃或陶瓷酒瓶防伪方法
技术领域
本发明涉及一种玻璃或陶瓷酒瓶防伪方法。
背景技术
目前在酒的销售市场上有很多假酒,尤其是一些假高档白酒,令白酒制造厂家防不胜防。高档白酒都是玻璃或陶瓷酒瓶包装,一些不法分子利用回收的玻璃或陶瓷酒瓶来制作假酒,达到了以假乱真的程度,令白酒厂家很头疼。怎样控制玻璃或陶瓷酒瓶不能轻易地被回收利用,是白酒厂家急切盼望解决的问题。
发明内容
本发明需要解决的技术问题就在于克服现有玻璃或陶瓷酒瓶易被回收利用、制造假酒的缺陷,提供一种玻璃或陶瓷酒瓶防伪方法,它在玻璃或陶瓷酒瓶上使用玻璃釉料做多层印刷,利用烧结技术把防伪标识烧结在玻璃或陶瓷表面,利用表层可剥离,剥离后不能复原的特点,使使用过的酒瓶不容易被重复回收利用,从而达到打假防假的目的。
为解决上述问题,本发明采用如下技术方案:
本发明一种玻璃或陶瓷酒瓶防伪方法,所述方法为使用多层釉料在水转印纸上做多层丝网印刷制作成防伪标识,利用一次烧结技术把水转印纸防伪标识烧结在玻璃或陶瓷表面;烧结温度为400-600℃,烧结时间为1.5-4小时;其中,底层釉料在高温下可以和玻璃或陶瓷表面完全结合,中层釉料和底层釉料在高温下结合在一起,中层印刷防伪标识,表层使用夜光釉料烧结后可以剥离,剥离后可以看到中层图案和数字,且剥离后不可以原样复原。
所述底层釉料重量份配方为:氧化钠8.57份,三氧化二铝0.9份,二氧化硅5.03份,氧化钾5.58份,氧化锌32.9份,氧化钡0.93份,氧化锡4.28份,氧化钙33.50份和碳酸镁15.00份。
所述中层釉料重量份配方为:氧化钠0.2份,三氧化二铝1.04份,二氧化硅17.6份,三氧化二硫4.21份,氧化锌1.28份,氧化锡2.25份和氧化钙15.20份。
所述表层釉料重量份配方为:氧化钠2份,三氧化二铝1份,二氧化硅3份,氧化锌3.35份,氧化锡1.33份,氧化钙55份和夜光粉30份。
本发明的特点为:
本发明使用多层玻璃或陶瓷环保釉面材料,采取三层丝网印刷技术。其中底层在高温下,釉料可以和玻璃表面完全结合,中层和底层结合在一起,中层可以印刷图案和数字,表层可以剥离,剥离后可以看到中层图案和数字,且剥离后不可以原样复原,利用这一特点,客户可以查询产品的真伪,也可做为鼓励促销,在中层印刷获奖信息等。
具体实施方式
本发明一种玻璃或陶瓷酒瓶防伪方法,所述方法为使用三层釉料在水转印纸上做三层丝网印刷制作成防伪标识,印刷后的水转印纸放在干燥环境内,在使用前必须把玻璃或陶瓷酒瓶准备贴标识的表面处理干净,将水转印纸贴上,利用一次烧结技术把水转印纸防伪标识烧结在玻璃或陶瓷表面;烧结温度为400-600℃,烧结时间为1.5-4小时;其中,底层釉料在高温下可以和玻璃或陶瓷表面完全结合,中层釉料和底层釉料在高温下结合在一起,中层印刷防伪标识,表层使用夜光釉料烧结后可以剥离,剥离后可以看到中层图案和数字,且剥离后不可以原样复原。
所述底层釉料重量份配方为:氧化钠8.57份,三氧化二铝0.9份,二氧化硅5.03份,氧化钾5.58份,氧化锌32.9份,氧化钡0.93份,氧化锡4.28份,氧化钙33.50份和碳酸镁15.00份。
所述中层釉料重量份配方为:氧化钠0.2份,三氧化二铝1.04份,二氧化硅17.6份,三氧化二硫4.21份,氧化锌1.28份,氧化锡2.25份和氧化钙15.20份。
所述表层釉料重量份配方为:氧化钠2份,三氧化二铝1份,二氧化硅3份,氧化锌3.35份,氧化锡1.33份,氧化钙55份和夜光粉30份。
本发明利用底层和中层不能被破坏,表层不能被复制的特点来阻止造假商贩对酒瓶的回收,从而起到打假防假的作用。
本发明使用的所有釉料都是环保无铅产品,适用于食品玻璃包装材料,不溶于水和酒精或其它溶剂。当表层剥离后,很难进行完全复原,从而使酒瓶不容易被重复使用,从而制止造假者回收,达到打假防假的目的。
最后应说明的是:以上实施例仅用以说明本发明而并非限制本发明所描述的技术方案;因此,尽管本说明书参照上述的各个实施例对本发明已进行了详细的说明,但是,本领域的普通技术人员应当理解,仍然可以对本发明进行修改或等同替换;而一切不脱离本发明的精神和范围的技术方案及其改进,均应涵盖在本发明的权利要求范围中。

Claims (5)

1、一种玻璃或陶瓷酒瓶防伪方法,其特征在于:所述方法为使用多层釉料在水转印纸上做多层丝网印刷制作成防伪标识,利用一次烧结技术把水转印纸防伪标识烧结在玻璃或陶瓷表面;烧结温度为400-600℃,烧结时间为1.5-4小时;其中至少一层釉料为夜光釉料。
2、如权利要求1所述的玻璃或陶瓷酒瓶防伪方法,其特征在于:多层釉料为三层釉料;其中,底层釉料在高温下可以和玻璃或陶瓷表面完全结合,中层釉料和底层釉料在高温下结合在一起,中层印刷防伪标识,表层使用夜光釉料,烧结后可以剥离,剥离后可以看到中层图案和数字,且剥离后不可以原样复原。
3、如权利要求2所述的玻璃或陶瓷酒瓶防伪方法,其特征在于:所述底层釉料重量份配方为:氧化钠8.57份,三氧化二铝0.9份,二氧化硅5.03份,氧化钾5.58份,氧化锌32.9份,氧化钡0.93份,氧化锡4.28份,氧化钙33.50份和碳酸镁15.00份。
4、如权利要求3所述的玻璃或陶瓷酒瓶防伪方法,其特征在于:所述中层釉料重量份配方为:氧化钠0.2份,三氧化二铝1.04份,二氧化硅17.6份,三氧化二硫4.21份,氧化锌1.28份,氧化锡2.25份和氧化钙15.20份。
5、如权利要求4所述的玻璃或陶瓷酒瓶防伪方法,其特征在于:所述表层釉料重量份配方为:氧化钠2份,三氧化二铝1份,二氧化硅3份,氧化锌3.35份,氧化锡1.33份,氧化钙55份和夜光粉30份。
CN2008101261997A 2008-07-07 2008-07-07 玻璃或陶瓷酒瓶防伪方法 Expired - Fee Related CN101624264B (zh)