CN101507990A CNA2009100299614A CN200910029961A CN101507990A CN 101507990 A CN101507990 A CN 101507990A CN A2009100299614 A CNA2009100299614 A CN A2009100299614A CN 200910029961 A CN200910029961 A CN 200910029961A CN 101507990 A CN101507990 A CN 101507990A
Authority
CN
China
Prior art keywords
straightening
steel pipe
steel tubes
aligning
bending section
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2009100299614A
Other languages
English (en)
Inventor
张铮
陈忠
苏俊
朱茂荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU CHENGDE STEELPIPE CO Ltd
Original Assignee
JIANGSU CHENGDE STEELPIPE CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU CHENGDE STEELPIPE CO Ltd filed Critical JIANGSU CHENGDE STEELPIPE CO Ltd
Priority to CNA2009100299614A priority Critical patent/CN101507990A/zh
Publication of CN101507990A publication Critical patent/CN101507990A/zh
Pending legal-status Critical Current

Links

Abstract

一种端部加厚钢管的矫直方法,涉及冶金工业中金属管材的加工技术领域。本发明将钢管自由支撑在托辊上,在弯曲段的两端分别设置两个支撑点,在弯曲段的最大弯曲面的外侧向钢管中轴施加压力。本发明在整个压力矫直过程中,加厚油管两端处于自由状态,没有任何轴向的约束,因此油管会发生明显的轴向拉伸现象。满足了下道工序车丝扣的要求,克服了过去人工压力矫直机劳动强度大,效率低,质量差,偏差大的缺点,本发明具有投资少、操作简单、效率高、矫直精度高等特点。

Description

一种端部加厚钢管的矫直方法
技术领域
本发明涉及冶金工业中金属管材的加工技术领域。
背景技术
随着世界工业的发展,特别是采油工业的发展,油井管制造行业也得到了迅猛的发展。但随着油井开采难度的不断加大,地质条件的不断恶劣。由于高钢级加厚油管具有优良的密封性、可靠的连接性、简易的操作性等优点,因此高钢级加厚油管的市场迅速发展状大起来。所谓加厚油管即在钢管生产加工过程中需要将钢管两端加厚,形成两头粗、中间细的哑铃状,这样使得加厚油管在通常矫直机上进行矫直时会存在不可避免的两端矫直盲区。因此,为了保证加厚油管全长直线度满足API 5CT规定要求,钢管在通常矫直后还必须进行管端盲区的局部矫直。但加厚油管端部的矫直一直是个难以解决问题。
现有技术的钢管矫直机一般采用斜辊矫直机,由于矫直辊倾斜布置,故钢管在矫直过程中始终作螺旋线运动,钢管在矫直辊间进行多次反复弯曲,来完成钢管的矫直。但对于加厚油管端部的矫直,斜辊矫直机也无能为力。国外也有研究机构,利用光电传感器技术,在钢管的矫直过程中,随着管径的变化,利用传感器来实现矫直机上下辊的距离的调整,端部通过时,将上下辊距离加大,让头部通过,通过后再压下矫直辊。但这种情况实际上末能达到精整钢管端部的目的,只能矫直管体部分。因此加厚油管的端部矫直问题,一直是个技术难题。
发明内容
本发明目的在于提供针对两端外径与管体外径不等的钢管的矫直方法。
本发明将钢管自由支撑在托辊上,在弯曲段的两端分别设置两个支撑点,在弯曲段的最大弯曲面的外侧向钢管中轴施加压力。
所述两个支撑点之间的间距可调。
将需要精整矫直的钢管通过上料机构进入到托辊上,通过旋转找到钢管弯曲部位,通过电控使托辊转动带动钢管在托辊上前后移动。根据弯曲的长度,任意调整两个支撑点之间的距离,固定后,再使弯曲段的最大弯曲面的外侧与外力相对,通过施加压力达到矫直钢管的目的。在整个压力矫直过程中,加厚油管两端处于自由状态,没有任何轴向的约束,因此油管会发生明显的轴向拉伸现象。满足了下道工序车丝扣的要求,克服了过去人工压力矫直机劳动强度大,效率低,质量差,偏差大的缺点,本发明具有投资少、操作简单、效率高、矫直精度高等特点。
具体实施方式
将钢管自由支撑在托辊上,在弯曲段的两端分别设置间距可调的两个支撑点,在弯曲段的最大弯曲面的外侧向施加径向压力。
其矫直原理及力学依据:
将钢管的弯曲部份放在两个固定的支点上,当向钢管施加径向外力时,钢管弯曲部分就产生适量的弹塑性变形而得到矫直。
矫直时顶头对弯曲钢管施加的矫直力应符合力学公式(1):
P/2×L/2>σS×S
P>4σS×S/L(N)      (1)
式中:σS-被矫钢管的屈服强度(Pa)
S—被矫钢管的塑性断面系数(m3)
L—同侧两固定支点之间的距离(m)
钢管矫直的力学参数的计算:
被矫直钢管在液压缸的顶头和两支点间施加的矫直力作用下,使被矫钢管成为一受力简支梁,由于受迫弯曲产生的最大正应力位于最大弯矩所在截面上距中性轴最远的地方。
要使钢管发生塑性变形而被矫直,且钢管不被折断,由弯距M在整个截面上形成的正应力P,必须全部或大部份处于材料的塑性变形范围,达到塑性变形条件。
即:
σS×S<M<σb×S               (1)
S×S/L<P<4σb×S/L     (2)
S×S/L<P<4σS×S/L     (3)
式中:
S—钢管的塑性断面系数
对于圆管:S=4/3(R3-r3)(D0和d0分别为钢管的内外半径)
对于方管:S=1/4(A3-a3)(A和a分别为方管的外内边长)
L—同侧两受力点间的距离
在矫直设备的设计或对设备能力参数的计算中应按钢管断面上的正应力全部达到塑性变形的角度考虑,结合以上公式(2)和(3),矫直机矫直力P应为
对于圆管
16σS(R3-r3)/3L<P<16σb(R3-r3)/3L
对于方管
σS(A3-a3)/L<P<σb(A3-a3)/L

Claims (2)

1、一种端部加厚钢管的矫直方法,其特征在于将钢管自由支撑在托辊上,在弯曲段的两端分别设置两个支撑点,在弯曲段的最大弯曲面的外侧向钢管施加径向压力。
2、根据权利要求1所述端部加厚钢管的矫直方法,其特征在于所述两个支撑点之间的间距可调。
CNA2009100299614A 2009-03-25 2009-03-25 一种端部加厚钢管的矫直方法 Pending CN101507990A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CNA2009100299614A CN101507990A (zh) 2009-03-25 2009-03-25 一种端部加厚钢管的矫直方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CNA2009100299614A CN101507990A (zh) 2009-03-25 2009-03-25 一种端部加厚钢管的矫直方法

Publications (1)

Publication Number Publication Date
CN101507990A true CN101507990A (zh) 2009-08-19

Family

ID=41000613

Family Applications (1)

Application Number Title Priority Date Filing Date
CNA2009100299614A Pending CN101507990A (zh) 2009-03-25 2009-03-25 一种端部加厚钢管的矫直方法

Country Status (1)

Country Link
CN (1) CN101507990A (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103370149A (zh) * 2011-02-14 2013-10-23 新日铁住金株式会社 弯曲矫正方法
CN111475896A (zh) * 2020-04-14 2020-07-31 太原科技大学 一种棒材矫直应力中性层位置确定方法
CN114798818A (zh) * 2022-04-02 2022-07-29 江苏赐瑞金属制品有限公司 一种镀锌方管自动矫直机及自动矫直方法

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103370149A (zh) * 2011-02-14 2013-10-23 新日铁住金株式会社 弯曲矫正方法
CN111475896A (zh) * 2020-04-14 2020-07-31 太原科技大学 一种棒材矫直应力中性层位置确定方法
CN111475896B (zh) * 2020-04-14 2023-04-21 太原科技大学 一种棒材矫直应力中性层位置确定方法
CN114798818A (zh) * 2022-04-02 2022-07-29 江苏赐瑞金属制品有限公司 一种镀锌方管自动矫直机及自动矫直方法
CN114798818B (zh) * 2022-04-02 2023-09-08 江苏赐瑞金属制品有限公司 一种镀锌方管自动矫直机及自动矫直方法

Similar Documents

Publication Publication Date Title
CN1781655A (zh) 焊管生产工艺
CN104339124A (zh) 一种不锈钢圆筒多曲率成型方法
CN101507990A (zh) 一种端部加厚钢管的矫直方法
CN101507991A (zh) 一种端部加厚钢管矫直机
CN107234440A (zh) 直径和壁厚可调的螺纹管桩生产线
CN104801578A (zh) 一种三辊卷板机的弯卷方法
CN205128608U (zh) 弯曲半径可调的高频焊管成型轧辊装置
CN105268780B (zh) 用于校正金属管的端部的方法和装置
CN104815881A (zh) 三辊卷板机的弯卷方法
CN209597917U (zh) 钢管矫直机构
CN217432663U (zh) 一种椭圆管矫直机构
CN109175011A (zh) 一种高直线度矫直机
CN206276752U (zh) 金属圆管折弯加工的夹紧扳动装置
CN204912366U (zh) 复合型钻杆矫直机
KR101443207B1 (ko) 마그네슘 파이프 교정기
CN206065113U (zh) 一种斜辊矫直机
CN201380218Y (zh) 端部加厚钢管矫直机
CN204182740U (zh) 一种盘管机多模具安装机构
CN210876918U (zh) 一种方管在线冷弯成型辅助装置
RU2614975C1 (ru) Способ гибки труб и станок для осуществления способа
CN110325298A (zh) 芯棒、弯管及其制造方法和制造装置
CN204294657U (zh) 一种冷拔机设备
CN202490857U (zh) 钢管道卷制支架
CN206702710U (zh) 轧辊铣床的金属夹持器
CN2936478Y (zh) 万能四辊矫直机

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Open date: 20090819