CN101435320A - 一种无试剂地浸采铀工艺流程 - Google Patents

一种无试剂地浸采铀工艺流程 Download PDF

Info

Publication number
CN101435320A
CN101435320A CNA2008102293872A CN200810229387A CN101435320A CN 101435320 A CN101435320 A CN 101435320A CN A2008102293872 A CNA2008102293872 A CN A2008102293872A CN 200810229387 A CN200810229387 A CN 200810229387A CN 101435320 A CN101435320 A CN 101435320A
Authority
CN
China
Prior art keywords
uranium
ion
leaching solution
ore bed
reagent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CNA2008102293872A
Other languages
English (en)
Other versions
CN101435320B (zh
Inventor
付春延
颜明友
李作臣
詹良
张忠华
汪利
郑继伟
孙建华
石建义
刘春华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Liaohe Petroleum Exploration Bureau
Original Assignee
Liaohe Petroleum Exploration Bureau
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Liaohe Petroleum Exploration Bureau filed Critical Liaohe Petroleum Exploration Bureau
Priority to CN2008102293872A priority Critical patent/CN101435320B/zh
Publication of CN101435320A publication Critical patent/CN101435320A/zh
Application granted granted Critical
Publication of CN101435320B publication Critical patent/CN101435320B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种无试剂地浸采铀工艺流程,此种工艺流程是在常规的无试剂地浸采铀工艺流程基础上,在介质进入吸附塔前增加一套由离子交换器、鼓风机、砂滤罐、再生剂罐、废液池组成的离子交换装置。通过注入孔向矿层注入含有氧化剂的溶浸液,使矿层中的铀变成铀酰离子或其它络合离子形式溶于溶浸液地下水中,再通过抽出孔将含有铀组分的浸出液提到地面,进行沉降和离子交换处理、吸附后,将溶浸液重新回注到矿层循环使用,含铀的饱和树脂经过解析、沉淀、压滤等工序生产出重铀酸岩产品。该方法具有投资少、操作技术成熟、防堵效果显著等优点,利用该工艺方法可以保证采铀井及生产系统连续稳定运行,提高生产时率和产品产量。

Description

一种无试剂地浸采铀工艺流程
技术领域:
本发明涉及一种用于砂岩型铀矿床开采生产过程的工艺流程,属铀矿开采技术类。
背景技术:
无试剂地浸采铀是目前铀矿开采处于领先水平的开采方式。在此种方式采铀过程中,抽出液和回注液通常采用简单沉降、砂滤等方式对水质进行净化,一般只能除掉水中机械杂质及部分微生物,但无法去除由金属阳离子产生的化学沉淀物,因而无法消除矿层及生产系统中的化学堵塞。这样,不仅需要经常采取洗井、气举等方法解堵,使得生产成本增大,而且影响铀矿正常开采,降低铀井生产时率和产品产量。
发明内容:
本发明目的在于提供一种防堵效果显著、可以保证采铀井和生产系统正常生产运行、提高生产时率和产品产量的无试剂地浸采铀工艺流程。
本发明目的的技术方案如下。此种工艺流程是在常规的无试剂地浸采铀工艺流程基础上,在介质进入吸附塔前增加一套由离子交换器、鼓风机、砂滤罐、再生剂罐、废液池组成的离子交换装置。采铀生产过程中,通过注入孔向矿层注入含有氧化剂的溶浸液,使矿层中的铀变成铀酰离子或其它络合离子形式溶于溶浸液(地下水)中,再通过抽出孔将含有铀组分的浸出液提到地面,在地面进行沉降、离子交换处理、吸附后,将溶浸液重新回注到矿层循环使用,含铀的饱和树脂经过解析、沉淀、压滤等工序生产出重铀酸岩产品。在离子交换装置中,利用其中的离子交换树脂脱除贵液中易形成沉淀的Ca2+、Mg2+、Fe3+等金属阳离子,从源头上保证流程内物流的清洁,既避免了沉淀的生成,起到防堵作用,又确保了吸附剂不被污染,提高吸附效率,延长使用寿命,同时还可以减少二氧化碳的补充量。吸附饱和的离子交换树脂经再生后可反复使用。
本发明提供的工艺流程将离子交换处理技术集成应用于无试剂地浸采铀工艺流程,具有投资少、单元操作技术成熟、防堵效果显著等优点,利用该工艺方法可以保证采铀井及生产装置系统连续稳定运行,提高生产时率和产品产量,同时可以减少二氧化碳的补充量,延长树脂的使用寿面,提高吸附效率,从而达到降低成本、提高经济效益的目的。
附图说明:
图1为本发明的总体工艺流程示意图。图2为离子交换装置工艺流程图。
具体实施方式:
以下结合附图对本发明的实施加以说明。
如图所示,常规的无试剂地浸采铀工艺流程由矿层、抽液井、贵液池、吸附塔、配液池、注液井等多个环节构成,并经解析沉淀、压滤烘干成产品。本发明是在该工艺流程基础上,在吸附塔前增加一套由离子交换器、砂滤罐、再生剂罐、废液池组成的离子交换装置。

Claims (1)

1、一种无试剂地浸采铀工艺流程,其特征在于,此种工艺流程是在常规的无试剂地浸采铀工艺流程基础上,在介质进入吸附塔前增加一套由离子交换器、鼓风机、砂滤罐、再生剂罐、废液池组成的离子交换装置;采铀生产过程中,通过注入孔向矿层注入含有氧化剂的溶浸液,使矿层中的铀变成铀酰离子或其它络合离子形式溶于溶浸液中,再通过抽出孔将含有铀组分的浸出液提到地面,在地面进行沉降、离子交换处理、吸附后,将溶浸液重新回注到矿层循环使用,含铀的饱和树脂经过解析、沉淀、压滤等工序生产出重铀酸岩产品;在离子交换装置中,利用其中的离子交换树脂脱除贵液中易形成沉淀的Ca2+、Mg2+、Fe3+等金属阳离子,从源头上保证流程内物流的清洁,既避免了沉淀的生成,起到防堵作用,又确保了吸附剂不被污染,提高吸附效率,延长使用寿命,同时还可以减少二氧化碳的补充量。
CN2008102293872A 2008-12-08 2008-12-08 一种无试剂地浸采铀工艺流程 Expired - Fee Related CN101435320B (zh)