CN101408382A - 金属化球团矿冷却输送机 - Google Patents
金属化球团矿冷却输送机 Download PDFInfo
- Publication number
- CN101408382A CN101408382A CNA2007101513724A CN200710151372A CN101408382A CN 101408382 A CN101408382 A CN 101408382A CN A2007101513724 A CNA2007101513724 A CN A2007101513724A CN 200710151372 A CN200710151372 A CN 200710151372A CN 101408382 A CN101408382 A CN 101408382A
- Authority
- CN
- China
- Prior art keywords
- cooling
- water
- pellet cooling
- conveyer
- metalized
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种供转底炉炼铁新工艺应用的金属化球团矿冷却输送机,在振动输送机的基础上,四壁用钢板焊成双层,中间通水,靠辐射与传导传热,辅之以喷淋水的方法,在空气中把金属化球团矿在运输过程中冷却到常温。这种设备结构和制造简单,成本低廉。
Description
所属技术领域
本发明涉及一种转底炉炼铁工艺,它是转底炉的专用设备,其作用是将高温的金属化球团矿冷却到常温,并输送至储矿槽。
背景技术
金属化球团矿的冷却是一项专门的技术,它既要把高温的球团矿冷却到常温,又要防止金属化球团矿的再氧化,传统的冷却方法是用煤气冷却,或将冷却对象放在密闭的回转筒中,从外部喷淋水,间接冷却。本发明是在振动输送机的基础上,四壁用钢板焊成双层,中间通水,靠辐射与传导传热,在空气中把金属化球团矿冷却到常温。
发明内容:
1、金属化球团矿冷却输送机由机体(1)、振动电机(2)、支撑弹簧(3)、冷却水进口(4)和出水口(5)组成,如附图1。设备的总长为4~10m。
2、金属化球团矿冷却输送机的冷却壁结构见附图1,通水间隙(6)8~16mm,水流速度在1-4m/s之间。
3、金属化球团矿冷却输送机内部上方有一个喷淋水管(7),必要时喷水,作为冷却的补充手段。
4、为防止金属化球团矿冷却输送机的通水间隙中有气体滞留,进水口设在机体的下方,出水口设在机体的上方。如图1所示。
附图说明:
附图1是金属化球团矿冷却输送机结构简图。其中:
1-机体,2-振动电机,3-支撑弹簧,4-进水口,
5-出水口,6-冷却水通道,7-喷淋水管。
Claims (3)
1、一种供转底炉炼铁新工艺应用的金属化球团矿冷却输送机,它具有冷却和输送产品的双重功能。长4-10m。
2、如权利1所述的金属化球团矿冷却输送机,它的四壁用普通碳素钢板焊成双层结构,中间通水冷却,通水间隙8-16mm,水流速度在1-4m/s之间。
3、如权利1、2所述的金属化球团矿冷却输送机,在机内上方设有喷淋水管,可以喷水作为加强冷却的补充手段。