CN101367223A - 木材内部微爆破方法 - Google Patents

木材内部微爆破方法 Download PDF

Info

Publication number
CN101367223A
CN101367223A CNA2007101436520A CN200710143652A CN101367223A CN 101367223 A CN101367223 A CN 101367223A CN A2007101436520 A CNA2007101436520 A CN A2007101436520A CN 200710143652 A CN200710143652 A CN 200710143652A CN 101367223 A CN101367223 A CN 101367223A
Authority
CN
China
Prior art keywords
wood
timber
cavity charge
charge containers
blasting method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2007101436520A
Other languages
English (en)
Inventor
王天龙
姜恩来
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Beijing Forestry University
Original Assignee
Beijing Forestry University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Beijing Forestry University filed Critical Beijing Forestry University
Priority to CNA2007101436520A priority Critical patent/CN101367223A/zh
Publication of CN101367223A publication Critical patent/CN101367223A/zh
Pending legal-status Critical Current

Abstract

本发明提供一种在保持木材本身的物理力学性能及外观完整的条件下,使木材内的毛细管全部或部分打开的木材内部微爆破方法,是属于木材加工工艺技术领域;是在压力罐内将木材通过加压,再瞬间释放压力的方法制造出的一类具有良好通透性的木质材料,为木材改性提供基础。本方法具有如下优点和效果:(1)适用于所有木材为原料;(2)方法具有方法简单、可操作性强、且安全可靠的优点;(3)可较好地实现改善木材的通透性的目的;(4)利用木材内部微爆破方法改良木材的通透性,为木材的功能性改性提供技术保障;(5)具有无污染,为绿色环保型生产方法;(6)可以制造出具有通透性良好的木材,增加木材的比表面积,提高木材的绿色环保的功效。

Description

木材内部微爆破方法
技术领域
本发明涉及一种在保持木材本身的物理力学性能及外观完整的条件下,使木材内部被阻塞的组织、细胞和纹孔对全部或部分打开的木材内部微爆破方法,属于木材科学与技术领域。
技术背景
目前,所提供的木材主要是速生树种木材。由于其密度低、材质软、强度及硬度较差,需要对其进行改性处理,以扩大其使用范围,可极大程度地缓解我国木材供需矛盾。向木材内浸注不同性能的改性剂,已获得具有不同功能的改性木材,是通常采用的方法之一。但是,由于木材本身存在着固有的通透性较差等问题,致使木材的改性处理困难。现有的处理技术还存在着生产周期长,效果差,成本较高的缺点,急待开发新的木材改性处理方法。
在传统的改良木材通透性方法中,通常采用冷热水浸泡、水煮、汽蒸、有机溶剂抽提等方法进行木材通透性的改良,效果相对较差和运行成本高的缺点。中国专利:02115318.3、03126182.5、01120932.1、02115319.1、96212421.4、200410026975.8、200510104295.8等,其爆破主要是针对木材、秸秆、草类、工业废纸板和废纸纤维等原料进行的爆破制浆,即将原料爆破成纤维状态,为造纸制造原料。本发明专利是在保持木材本身的物理力学性能及外观完整的条件下,在压力罐内对木材进行加压,使木材内部充满具有一定压力的气体,之后瞬间释放木材内部压力,木材内部压缩气体和水分瞬间膨胀,使木材内部被阻塞的毛细管全部或部分打开的方法。本发明涉及的木材内部微爆破方法使用方便,且安全可靠。经有关文献、资料检索,未发现相近似的专利生产方法内容。
发明内容
本发明的目的,是为了克服上述改良木材通透性方法的不足之处,在保持木材本身的物理力学性能及外观完整的条件下,利用木材内部微爆破的方法,使木材内部被阻塞的组织、细胞和纹孔对全部或部分打开的方法,可以充分地改良木材的通透性能,为实现木材高性能化和多功能化改性创造基础条件。
本发明的目的是这样实现的
涉及一种利用木材内部微爆破方法改良木材通透性的方法,它是将原木材料经圆锯或带锯锯解成板材,其厚度在0.5毫米~200毫米范围;其长度在5毫米~5000毫米范围,其宽度在5毫米~500毫米范围;可不调整木材的含水率或将木材的含水率调整到10%~200%范围内,可在爆破罐内进行木材含水率调整,也可在爆破罐外进行木材含水率调整;将锯解的板材放入特制的爆破罐内,关闭进出料装置;在爆破罐内可以利用电加热和通入蒸汽的方式对木材进行加热,也可以不进行加热;通过蒸汽或加压泵使爆破罐增压,爆破罐内的压力在0.1MPa~2.0MPa范围内;保持要求的压力1分钟~120分钟;然后迅速打开喷放阀,使爆破罐内的压力瞬间降至常压;上述加压—瞬间降压过程可重复1次~15次;完成木材爆破处理后,打开进出料装置,取出木材即完成木材内部微爆破的方案。
本发明创造有如下优点和效果
1.它涉及的木材内部微爆破方法,适用于所有木材为原料;
2.它涉及的木材内部微爆破方法,其方法具有方法简单、可操作性强、且安全可靠的优点;
3.利用木材内部微爆破方法,可较好地实现改善木材的通透性的目的;
4.利用木材内部微爆破方法改良木材的通透性,为木材的功能性改性提供技术保障;
5.木材内部微爆破方法,具有无污染,为绿色环保型生产方法;
6.利用木材内部微爆破方法,可以制造出具有多孔状的类似海绵状的木质材料,增加了木材的比表面积,大大提高木质材料的绿色环保的功效。
具体实施方案:
实施例  制作一种具有通透性良好的木材,原料采用桦木,用带锯或圆锯将其锯解成厚度为5~8毫米,长度为20~1000毫米和宽度为10~30毫米的板材;在爆破关内调整木材的含水率到30%~100%范围内;关闭进出料装置;通过加压泵使爆破罐增压至0.5MPa~0.8MPa范围内;保持要求的压力5分钟~20分钟;然后迅速打开喷放阀,使爆破罐内的压力瞬间降至常压;上述加压—瞬间降压过程可重复1次~10次;完成木材爆破处理后,打开进出料装置,取出木材即完成利用爆破技术生产具有环保和保健功能木质材料的方案。

Claims (9)

1.利用所有的木质材料通过木材内部微爆破方法。其特征是:将原木材料经圆锯或带锯锯解成板材,其厚度在0.5毫米~200毫米范围;其长度在5毫米~5000毫米范围,其宽度在5毫米~500毫米范围;可不调整木材的含水率或将木材的含水率调整到10%~200%范围内,可在爆破罐内进行木材含水率调整,也可在爆破罐外进行木材含水率调整;将锯解的板材放入特制的高压爆破罐内,关闭进出料装置;在爆破罐内可以利用电加热和通入蒸汽的方式对木材进行加热,也可以不进行加热;通过蒸汽或加压泵使爆破罐增压,爆破罐内的压力在0.1MPa~2.0MPa范围内;保持要求的压力1分钟~120分钟;然后迅速打开喷放阀,使爆破罐内的压力瞬间降至常压;上述加压一瞬间降压过程可重复1次~10次;完成木材爆破处理后,打开进出料装置,即完成木材内部微爆破方法。
2.根据权利要求1所述的木材内部微爆破方法,其特征是:生产具有良好通透性的原料是所有的材种的木材。
3.根据权利要求1所述的木材内部微爆破方法,其特征是:锯解成板材的厚度在0.5~200毫米范围,长度在5毫米~5000毫米范围,宽度在5毫米~500毫米范围。
4.根据权利要求1所述的木材内部微爆破方法,其特征是:可不调整木材的含水率,也可在爆破罐内或爆破罐外进行木材含水率调整。
5.根据权利要求4所述的木材含水率的调整,其特征是:其值在10%~200%范围内。
6.根据权利要求1所述的木材内部微爆破方法,其特征是:通过蒸汽或加压泵使爆破罐增压,爆破罐内的压力在0.1MPa~2.0MPa范围内。
7.根据权利要求1所述的木材内部微爆破方法,其特征是:保持要求的压力1分钟~120分钟;然后迅速打开喷放阀,使爆破罐内的压力瞬间降至常压。
8.根据权利要求1所述的木材内部微爆破方法,其特征是:加压和瞬间降压可重复进行。
9.根据权利要求8所述的加压和瞬间降压可重复进行,其特征是:加压和瞬间降压过程可重复1次~15次。
CNA2007101436520A 2007-08-17 2007-08-17 木材内部微爆破方法 Pending CN101367223A (zh)