一种治理膨胀土滑坡的改良剂 Download PDFInfo
- Publication number
- CN101235291A CN101235291A CN 200810006959 CN200810006959A CN101235291A CN 101235291 A CN101235291 A CN 101235291A CN 200810006959 CN200810006959 CN 200810006959 CN 200810006959 A CN200810006959 A CN 200810006959A CN 101235291 A CN101235291 A CN 101235291A
- Authority
- CN
- China
- Prior art keywords
- modifying agent
- ground
- water
- swelled
- slope
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (2)