CN101217265A - 节能环保型铁壳滤波器及其制造方法 - Google Patents
节能环保型铁壳滤波器及其制造方法 Download PDFInfo
- Publication number
- CN101217265A CN101217265A CNA2008100324452A CN200810032445A CN101217265A CN 101217265 A CN101217265 A CN 101217265A CN A2008100324452 A CNA2008100324452 A CN A2008100324452A CN 200810032445 A CN200810032445 A CN 200810032445A CN 101217265 A CN101217265 A CN 101217265A
- Authority
- CN
- China
- Prior art keywords
- iron
- clad
- iron shell
- filter
- wax
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种节能环保型铁壳滤波器及其制造方法,铁壳滤波器由铁壳、内部电子元器件及充填物构成,内部充填物由导热蜡充任,是通过将熔化为纯液态的导热蜡灌注入已经安装设置有电子元器件的铁壳腔内、然后自然冷却,将电子元器件与铁壳固化成一体实现的。由于导热蜡是物理固化型材料,具有良好导热性,熔点低,在熔解状态下呈非稠性纯液态,固化时间短,浇注方便,有利于简化工艺、确保电气分布参数的稳定性和提高工作效率,导热蜡价格低且可以重复利用,符合节能、环保和高效要求,与现有的采用环氧材料作为充填物的铁壳滤波器相比,更具质量和价格优势。
Description
技术领域
本发明涉及低压电子器件制造技术领域,特别是一种有利于简化制造工艺、降低生产成本和提高工作参数稳定性的节能环保型铁壳滤波器及其制造方法。
背景技术
滤波器是一种具有阻断干扰源、有助于提高电气工作电路抗干扰能力的电子器件,通常由包含有电容器和电感线圈的电子元器件组成。对于自身有屏蔽要求的抗干扰滤波器,一般均安装设置在铁壳内,且采用在铁壳腔内设置电子元器件后的空隙中充填固化物的方法固定各电子元器件间的相对位置,以免发生由外界振动等因素引发电子元器件变形性位移、造成内部电气分布参数的变化,从导致影响额定工作参数的稳定性。此外,由于滤波器的电子元器件在工作过程中会产生热量,因而对所充填的固化物还有一个迅速传递、散发热量的要求。所以在抗干扰滤波器的制造中,对于充填物的例行选择相当重要。在现有技术的滤波器制造中,习惯于采用环氧材料作为充填物。但在实践中逐渐发现:由于环氧材料是一种有机化合物,具有相对较高的熔点,且熔化后的液态环氧材料相对比较稠,所以在执行充填作业时必须谨慎小心地进行液位渐升式灌装,否则会因影响电感线圈的内部间距,影响工作电路的电气分布参数,从而导致影响总体工作参数;环氧材料的固化时间较长,在静止状态下至少需要24小时才能充分固化,不利于生产效率的提高;环氧材料的导热性能一般,且只宜作为一次性封装材料(化学固化)使用,滤波器报废后的环氧材料只能作为垃圾处理。由上可见,利用环氧材料充填滤波器总体上存在充填时工序繁琐、工艺复杂、操作难度较高、生产成本较高电气工作参数较难控制等诸多弊端,不符合节能、环保、高效的要求,所以无论从经济性和实用性角度考虑,均欠理想。
发明内容
本发明的目的是要提供一种可以达到节能、环保、高效要求,有利于降低生产成本的节能环保型铁壳滤波器及其制造方法。
本发明的节能环保型铁壳滤波器主体由外带电气引出脚的铁壳、内部电子元器件及充填物构成,特征在于所述的内部充填物由导热蜡构成。
制造本发明的节能环保型铁壳滤波器时,先按常规方法在铁壳上固定设置电气引出脚,在铁壳腔内安装设置包含有电容器和电感线圈的电子元器件,然后将熔化为纯液态的导热蜡灌注入已经安装设置有电子元器件的铁壳腔内,使电子元器件与铁壳内表面完全深浸于其中,最后自然冷却,于是电子元器件与铁壳由导热蜡固化成一体,制成本发明的节能环保型铁壳滤波器。
基于上述构思的本发明节能环保型铁壳滤波器及其制造方法,由于在铁壳内部设置电子元器件后的所有空隙内均由导热蜡作为充填物加以充填,而导热蜡本身是一种物理固化型物质,除导热性能良好,能满足内部电子元器件工作时的散热要求外,还具有:在熔解状态下呈非稠性的纯液体状态,充填时内部元器件不会对它产生任何阻力,故不会导致影响内部分布参数,便于生产过程中快速浇灌充填,有效缩短浇灌充填的时间,有利于提高工作效率和确保滤波器工作参数的稳定性;导热蜡熔点低、具有冷却即凝固的特点,可有效缩短充填后的固化时间,有利于提高生产效率;导热蜡在滤波器报废后仍可以回收、重复利用,符合节能、环保要求要求。综上所述,利用本发明方法生产的本发明的节能环保型铁壳滤波器与采用传统的用环氧材料作为充填物的同类铁壳滤波器相比,具有明显的工艺简单、加工方便、生产效率高,产品性能可靠、工作稳定性好,生产成本更低,完全符合节能、环保和高效的要求,方法可靠,结构科学、选料合理、具有很强的可操作性和实用性,值得在铁壳滤波器制造行业中推广应用。
附图说明
附图是本发明实施例中一个典型普通滤波器的基本结构示意图。
图中:
1.铁壳 2.电子元器件 3.充填物 4.电气引出脚
具体实施方式
下面结合附图及典型实施例对本发明作进一步说明。
在附图中,本发明的节能环保型铁壳滤波器主体由铁壳1、内部电子元器件2及充填物3构成,铁壳1上设置有电气引出脚4,铁壳1腔内设置有电子元器件2及由导热蜡充任的充填物3。
Claims (2)
1.一种节能环保型铁壳滤波器,由铁壳(1)、内部电子元器件(2)及充填物(3)构成,铁壳(1)上设置有电气引出脚(4),其特征在于所述的充填物(3)由导热蜡构成。
2.一种节能环保型铁壳滤波器的制造方法,特征在于先按常规方法在铁壳上固定设置电气引出脚,在铁壳腔内安装设置包含有电容器和电感线圈的电子元器件,然后将熔化为纯液态的导热蜡灌注入已经安装设置有电子元器件的铁壳腔内,使电子元器件与铁壳内表面完全深浸于其中,最后自然冷却,将电子元器件与铁壳固化成一体,制成节能环保型铁壳滤波器。