CN101177774A - 一种钛及钛合金表面氧碳共渗的设备及方法 - Google Patents
一种钛及钛合金表面氧碳共渗的设备及方法 Download PDFInfo
- Publication number
- CN101177774A CN101177774A CNA2007101885303A CN200710188530A CN101177774A CN 101177774 A CN101177774 A CN 101177774A CN A2007101885303 A CNA2007101885303 A CN A2007101885303A CN 200710188530 A CN200710188530 A CN 200710188530A CN 101177774 A CN101177774 A CN 101177774A
- Authority
- CN
- China
- Prior art keywords
- titanium
- vacuum chamber
- carbon
- cementation
- titanium alloy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (4)