CN101159182A - 电缆翻新方法 - Google Patents
电缆翻新方法 Download PDFInfo
- Publication number
- CN101159182A CN101159182A CNA2007100259196A CN200710025919A CN101159182A CN 101159182 A CN101159182 A CN 101159182A CN A2007100259196 A CNA2007100259196 A CN A2007100259196A CN 200710025919 A CN200710025919 A CN 200710025919A CN 101159182 A CN101159182 A CN 101159182A
- Authority
- CN
- China
- Prior art keywords
- cable
- core
- afterwards
- retreading
- cable core
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开一种电缆翻新方法。具体说,是将旧电缆翻新成可用电缆的电缆翻新方法,尤其适用于通信电缆的翻新。它包括以下步骤:对需拆旧的电缆进行检测,判断其可修复程度;对可以修复的电缆进行外护套开剥;将大对数电缆拆分成多根小对数电缆;对小对数电缆的缆芯进行加固,防止原电缆芯线的结构被破坏而影响性能;重新加包聚酯带;检测缆芯有无断、混线情况和线间电阻;对无断、混线情况和线间电阻合格的缆芯进行纵包铝塑复合带;挤制外护套,得到可用的翻新电缆。使用该方法对旧电缆进行翻新,可减少电信运营商的成本。
Description
技术领域
本发明涉及一种电缆生产方法。具体说,是将旧电缆翻新成可用电缆的电缆翻新方法,尤其适用于通信电缆的翻新。
背景技术
在电缆制造行业都知道,通信电缆在铺设后,如果不是人为行为其使用寿命都比较长。但随着道路的扩建和改造,原先铺设的好电缆需要进行移位或改道,于是众多使用过的电缆将被拆除。但在拆除过程中,充于电缆中的干燥压缩空气会泄漏,造成水汽进入电缆。尤其是管道电缆,在拆除过程中,管道里的积水会进入电缆,是电缆对地的绝缘强度降低,无法重新使用,浪费现象严重,从而增加了电信运营商的成本。
发明内容
本发明要解决的问题是提供一种电缆翻新方法。使用该方法对旧电缆进行翻新,可减少电信运营商的成本。
为解决上述问题,采取以下技术方案:
本发明的电缆翻新方法包括以下步骤:
先对需拆旧的电缆进行检测,判断其可修复程度;
再对可以修复的电缆进行外护套开剥;
之后,将大对数电缆拆分成多根小对数电缆;
之后,对小对数电缆的缆芯进行加固,防止原电缆芯线的结构被破坏而影响性能;
之后,重新加包聚酯带;
之后,检测缆芯有无断、混线情况和线间电阻;
再之后,对无断、混线情况和线间电阻合格的缆芯进行纵包铝塑复合带;
最后,挤制外护套,得到可用的翻新电缆。
采取上述方案,具有以下优点:
由于通过本发明的电缆翻新方法可以将拆除的旧电缆进行翻新,利用极小的代价,使这些拆旧电缆的技术指标达到合格要求,可以再次使用道线路中。不仅避免了浪费,还极大地降低了电信运营成本。仅以江苏省计算,通过拆旧翻新,一年可节约投资2亿元。
具体实施方法
首先对需拆旧电缆进行检测,判断其可修复程度;
再用专用设备对可以修复的电缆进行外护套开剥;
之后,利用电缆拆分装置将大对数电缆拆分成多根小对数电缆;
之后,对小对数电缆的缆芯进行加固,防止原电缆芯线的结构被破坏而影响性能;
之后,使用电缆绕包机重新加包聚酯带;
之后,利用全自动电缆检测仪检测缆芯有无断、混线情况和线间电阻;
再之后,利用电缆护套机对无断、混线情况和线间电阻合格的缆芯进行纵包铝塑复合带;
最后,利用电缆护套机挤制外护套,得到可用的翻新电缆。
Claims (1)
1.电缆翻新方法,其特征在于包括以下步骤:
先对需拆旧的电缆进行检测,判断其可修复程度;
再对可以修复的电缆进行外护套开剥;
之后,将大对数电缆拆分成多根小对数电缆;
之后,对小对数电缆的缆芯进行加固,防止原电缆芯线的结构被破坏而影响性能;
之后,重新加包聚酯带;
之后,检测缆芯有无断、混线情况和线间电阻;
再之后,对无断、混线情况和线间电阻合格的缆芯进行纵包铝塑复合带;
最后,挤制外护套,得到可用的翻新电缆。