CN101143780A - 油田污泥在制砖材料中的运用 - Google Patents
油田污泥在制砖材料中的运用 Download PDFInfo
- Publication number
- CN101143780A CN101143780A CNA2006101046328A CN200610104632A CN101143780A CN 101143780 A CN101143780 A CN 101143780A CN A2006101046328 A CNA2006101046328 A CN A2006101046328A CN 200610104632 A CN200610104632 A CN 200610104632A CN 101143780 A CN101143780 A CN 101143780A
- Authority
- CN
- China
- Prior art keywords
- sludge
- percent
- oil field
- brick
- field sludge
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明解决了在石油开采、选油、运输、炼油等环节中产生的油田污泥进行掩埋、回填的问题,具体地说,本发明涉及油田污泥在制砖材料中的运用。其方法是把油田污泥收集起来,按含油量的高低,按不同比例与其它制砖材料混合配伍烧制成砖。按重量百分比由下列部分组成:粘土10%-40%,黄土20%-60%,油田污泥1%-90%。本发明不仅解决了油田污泥污染土地的问题,而且可回收部分资源,实现消除污染、资源转化、变废为宝的目的,并且用油田污泥制成的砖可应用在建筑行业上。
Description
技术领域:
本发明涉及制砖材料,更具体地说:本发明涉及油田污泥在制砖材料中的运用。
背景技术:
目前,对石油开采、选油、运输、炼油等环节中产生的油田污泥,除个别企业回收处理外,大部分采用收集、掩埋、回填。这既造成了资源的浪费又污染了环境,尤其对地表水体污染严重。
发明内容:
本发明的目的是克服现有技术中的不足,解决在石油开采、选油、运输、炼油等环节中产生的油田污泥进行掩埋、回填的问题,把油田污泥收集起来,按含油量的高低,按不同比例与其它制砖材料混合配伍烧制成砖,实现消除污染、资源转化、变废为宝的目的。
本发明的目的通过下述技术方案予以实现:
对零散少量的油田污泥可就近送往砖厂,按比例与制砖材料混合配伍烧制成砖。将集中收集起来的大量含油较高的油田污泥,可建立油田污泥处置站,用专用设备将油田污泥进行油、水、泥沙三相分离,实现油田污泥中的原油回收。将处置后的油田污泥送往砖厂进行与制砖材料配伍烧制成砖。
油田污泥在制砖材料中的运用,按重量百分比由下列部分组成:粘土10%-4 0%,黄土20%-6 0%,油田污泥1%-90%。
本发明不仅解决了油田污泥污染土地的问题,而且可回收部分资源,用油田污泥制成的砖可应用在建筑行业上。
具体实施方式:
下面结合实施例及制造工艺对本发明作进一步描述。
本发明由下列组分(重量百分比)构成:粘土10%-40%,黄土20%-60%,油田污泥1%-90%。
以每块砖2.5kg为例:
实施例1:
粘土0.99kg、黄土1.5kg、油田污泥0.01kg。
实施例2:
粘土1kg、黄土1.4kg、油田污泥0.1kg。
实施例3:
粘土1kg、黄土0.5kg、油田污泥1kg。
实施例4:
粘土0.75kg、油田污泥1.75kg。
实施例5:
粘土0.25kg、油田污泥2.25kg。
本发明的制造工艺:将制砖的原料按比例混合配料后,用水搅拌均匀,经皮带传送到砖机上,挤压成砖坯,将砖坯自然烘干或用烘干炉烘干,送入烧砖窑炉中加温900-1000℃左右烧成,即可使用。
Claims (1)
1.一种油田污泥在制砖材料中的运用,制砖材料按重量百分比由下列部分组成:粘土10%-40%,黄土20%-60%,油田污泥1%-90%。