CN101126014B - 一种耐低温自粘橡胶沥青防水卷材 - Google Patents

一种耐低温自粘橡胶沥青防水卷材 Download PDF

Info

Publication number
CN101126014B
CN101126014B CN2007101208098A CN200710120809A CN101126014B CN 101126014 B CN101126014 B CN 101126014B CN 2007101208098 A CN2007101208098 A CN 2007101208098A CN 200710120809 A CN200710120809 A CN 200710120809A CN 101126014 B CN101126014 B CN 101126014B
Authority
CN
China
Prior art keywords
self
coiled material
styrene butadiene
adhesive rubber
rubber asphalt
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2007101208098A
Other languages
English (en)
Other versions
CN101126014A (zh
Inventor
李卫国
段文峰
田凤兰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jinzhou Dongfang Yuhong Building Materials Co., Ltd.
Original Assignee
Beijing Oriental Yuhong Waterproof Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Beijing Oriental Yuhong Waterproof Technology Co Ltd filed Critical Beijing Oriental Yuhong Waterproof Technology Co Ltd
Priority to CN2007101208098A priority Critical patent/CN101126014B/zh
Publication of CN101126014A publication Critical patent/CN101126014A/zh
Application granted granted Critical
Publication of CN101126014B publication Critical patent/CN101126014B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明提供了一种耐低温自粘橡胶沥青防水卷材,其改性沥青层中含有碳酸钙和两种以上增粘剂,改变了目前自粘橡胶沥青防水卷材不能在5℃以下施工的缺陷,其在低至-10℃的低温下仍具有良好的粘结性能,剥离强度达到1.0N/mm以上。

Description

一种耐低温自粘橡胶沥青防水卷材
技术领域
本发明涉及一种耐低温自粘防水卷材,具体地说,涉及一种能在低温(-10℃)条件下自粘施工的自粘橡胶沥青防水卷材。
背景技术
目前,公知的自粘施工法自粘橡胶沥青防水卷材是以SBS等弹性体改性沥青为基料,强韧防水聚乙烯膜或铝箔作为卷材上表面材料或无膜(双面自粘),采用可剥离的涂硅膜或涂硅皱纹纸为下表面防粘隔离层材料制成的一种无胎自粘防水卷材。产品执行JC 840-1999《自粘橡胶沥青防水卷材》国家行业标准。
以上公知的自粘橡胶沥青防水卷材具有以下缺点:自粘橡胶沥青防水卷材需在5℃以上才能施工,5℃以下无法自粘施工。温度条件严重制约了自粘橡胶沥青防水卷材的应用。综上所述,目前公知的自粘橡胶沥青防水卷材受季节和地域的影响很大,适用范围窄。
发明内容
本发明的目的是提供一种能在低温条件下自粘施工的自粘橡胶沥青防水卷材。
本发明的耐低温自粘橡胶沥青防水卷材包含一改性沥青层,该改性沥青层含有热塑性丁苯橡胶(苯乙烯-丁二烯-苯乙烯嵌段共聚物)、粉末丁苯橡胶及两种以上增粘剂,优选的增粘剂是古马隆树脂、石油树脂、萜烯树脂、小分子量聚异丁烯的混合。本发明的耐低温自粘橡胶沥青防水卷材的改性沥青层中还含有碳酸钙。本发明的耐低温自粘橡胶沥青防水卷材改变了自粘橡胶沥青在低温下(5℃以下)不粘的缺陷,使自粘橡胶沥青防水卷材在-10℃低温下仍具有1.0N/mm以上的剥离强度,具有良好的粘接性能。
本发明的耐低温自粘橡胶沥青防水卷材的改性沥青层含有下述重量份的组分:
石油沥青                  40~60
减三线油                  5~15
热塑性丁苯橡胶            6~15
粉末丁苯橡胶              2~4
古马隆树脂                1~3
石油树脂                  0.2~1
萜烯树脂                  0.5~2
小分子量聚异丁烯          1~1.5
紫外线吸收剂              0.05~2
抗氧剂                    0.03~1,以及
碳酸钙                    9~18。
优选地,本发明的耐低温自粘橡胶沥青防水卷材的改性沥青层含有下述重量份的组分:
石油沥青                      48
减三线油                      12
热塑性丁苯橡胶                8
粉末丁苯橡胶                  4
古马隆树脂                    1
石油树脂                      0.5
萜烯树脂                      0.5
小分子量聚异丁烯              1
紫外线吸收剂                  0.1
抗氧剂                        0.1
碳酸钙                        16
其中,所述的紫外线吸收剂采用的是UV-531紫外线吸收剂;抗氧剂采用的是二叔丁基对甲酚。
本发明的耐低温自粘橡胶沥青防水卷材的制备方法,包括如下步骤:
(1)在石油沥青中加入减三线油,升温到120~180℃时加入热塑性丁苯橡胶、粉末丁苯橡胶,搅拌0.5~2小时,温度升到140~200℃后,研磨,加入古马隆树脂,石油树脂、萜烯树脂、小分子量聚异丁烯等多种增粘剂,在140~200℃搅拌0.5~2小时,加入碳酸钙、紫外线吸收剂、抗氧剂,搅拌0.5~2小时即制成自粘橡胶沥青。
(2)自粘橡胶沥青降温至150±5℃,经过隔离纸展开、自粘胶涂敷、冷却、覆膜、冷却定型制成自粘橡胶沥青防水卷材。
本发明的耐低温自粘橡胶沥青防水卷材,其改性沥青层含有碳酸钙和两种以上增粘剂,改变了目前自粘橡胶沥青防水卷材不能在5℃以下施工的缺陷,其在低至-10℃的低温下仍具有良好的粘结性能,剥离强度达到1.0N/mm以上,可用自粘法施工。
具体实施方式
以下实施例用于说明本发明,但不用来限制本发明的范围。
本发明的耐低温自粘橡胶沥青防水卷材剥离强度的测试方法采用JC840-1999中的实验方法。测试中使用的拉力机为微机控制电子万能试验机,型号为CMT 6104。
实施例1
在40g石油沥青中加入5g减三油,升温到120℃时加入6g热塑性丁苯橡胶、2g粉末丁苯橡胶,搅拌2小时,温度升到140℃后,进入胶体磨研磨,循环研磨三遍,加入1g古马隆树脂,0.2g石油树脂、0.5g萜烯树脂、1g小分子量聚异丁烯,在140℃±5℃搅拌2小时,加入9g碳酸钙、0.05g紫外线吸收剂UV-531、0.03g二叔丁基对甲酚,搅拌2小时即制成自粘橡胶沥青。
实施例2
在48g石油沥青中加入12g减三油,升温到150℃时加入10.5g热塑性丁苯橡胶、3g粉末丁苯橡胶,搅拌1小时,温度升到175℃后,进入胶体磨研磨,循环研磨三遍,加入2g古马隆树脂,0.6g石油树脂、1.25g萜烯树脂、1.25g小分子量聚异丁烯,在180℃±5℃搅拌1小时,加入13.5g碳酸钙、1g紫外线吸收剂UV-531、0.5g二叔丁基对甲酚,搅拌1小时即制成自粘橡胶沥青。
实施例3
在60g石油沥青中加入15g减三油,升温到180℃时加入,15g热塑性丁苯橡胶、4g粉末丁苯橡胶,搅拌0.5小时,温度升到200℃后,进入胶体磨研磨,循环研磨三遍,加入3g古马隆树脂,1g石油树脂、2g萜烯树脂、1.5g小分子量聚异丁烯,在200℃±5℃搅拌0.5小时,加入18g碳酸钙、2g紫外线吸收剂UV-531、1g二叔丁基对甲酚,搅拌0.5小时即制成自粘橡胶沥青。
实施例1至3所制得的自粘橡胶沥青降温至150±5℃,经过隔离纸展开、自粘胶涂敷、冷却、覆膜、冷却定型等工艺制成耐低温自粘橡胶沥青防水卷材,剥离强度如下表1所示。
表1.本发明的耐低温自粘橡胶沥青防水卷材的剥离强度(-10℃)
  实施例   剥离强度(N/mm)
  1   1.4
  2   1.6
  3   1.3

Claims (5)

1.一种耐低温自粘橡胶沥青防水卷材,其特征在于,包含改性沥青层,所述改性沥青层含有下述重量份的组分:
石油沥青            40~60
减三线油            5~15
热塑性丁苯橡胶      6~15
粉末丁苯橡胶        2~4
古马隆树脂          1~3
石油树脂            0.2~1
萜烯树脂            0.5~2
小分子量聚异丁烯    1~1.5
紫外线吸收剂        0.05~2
抗氧剂              0.03~1,以及
碳酸钙              9~18。
2.如权利要求1所述的耐低温自粘橡胶沥青防水卷材,其特征在于,所述改性沥青层含有下述重量份的组分:
石油沥青            48
减三线油            12
热塑性丁苯橡胶      8
粉末丁苯橡胶        4
古马隆树脂          1
石油树脂            0.5
萜烯树脂            0.5
小分子量聚异丁烯    1
紫外线吸收剂        0.1
抗氧剂              0.1
碳酸钙              16。
3.如权利要求1或2所述的耐低温自粘橡胶沥青防水卷材,其特征在于所述的紫外线吸收剂是UV-531,抗氧剂是二叔丁基对甲酚。
4.一种权利要求1至3任一所述的耐低温自粘橡胶沥青防水卷材的制备方法,包括如下步骤:
(1)在石油沥青中加入减三线油,升温到120~180℃时加入热塑性丁苯橡胶、粉末丁苯橡胶,搅拌0.5~2小时,温度升到140~200℃后,研磨,加入增粘剂,在140~200℃搅拌0.5~2小时,加入碳酸钙、紫外线吸收剂、抗氧剂,搅拌0.5~2小时即制成自粘橡胶沥青;
(2)自粘橡胶沥青降温至150±5℃,经过隔离纸展开、自粘胶涂敷、冷却、覆膜、冷却定型制成自粘橡胶沥青防水卷材。
5.如权利要求4所述的耐低温自粘橡胶沥青防水卷材的制备方法,其特征在于,在石油沥青中加入减三线油,升温到150℃时加入热塑性丁苯橡胶、粉末丁苯橡胶,搅拌1小时,温度升到175℃后,研磨,加入增粘剂,在180℃±5℃搅拌1小时,加入碳酸钙、紫外线吸收剂、抗氧剂,搅拌45分钟到1小时。
CN2007101208098A 2007-08-27 2007-08-27 一种耐低温自粘橡胶沥青防水卷材 Active CN101126014B (zh)