CN101110475A - 一种镍电极的制作工艺 - Google Patents

一种镍电极的制作工艺 Download PDF

Info

Publication number
CN101110475A
CN101110475A CNA2006100617365A CN200610061736A CN101110475A CN 101110475 A CN101110475 A CN 101110475A CN A2006100617365 A CNA2006100617365 A CN A2006100617365A CN 200610061736 A CN200610061736 A CN 200610061736A CN 101110475 A CN101110475 A CN 101110475A
Authority
CN
China
Prior art keywords
nickel
nickel electrode
electrode
present
battery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2006100617365A
Other languages
English (en)
Inventor
王守军
刘新华
杨峰涛
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen EPT Battery Co Ltd
Original Assignee
Shenzhen EPT Battery Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen EPT Battery Co Ltd filed Critical Shenzhen EPT Battery Co Ltd
Priority to CNA2006100617365A priority Critical patent/CN101110475A/zh
Publication of CN101110475A publication Critical patent/CN101110475A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种电池电极的制作工艺。主要是通过在镍电极内添加一种或多种金属氧化物或化合物,达到提高电池的储存性能,改善含镍电极电池的综合性能的作用。本发明所述的一种或多种金属氧化物或化合物,是采用在碱性溶液中标准氧化/还原电位高于0.4V,且在碱性溶液中能保持稳定的,如:二氧化锰等。本发明在镍电极中添加的金属氧化物或化合物比例为活性物质重量的0.1~15%,其加入方式为:与活性物质氢氧化镍粉末混合均匀后填充到导电基体中,制作成本发明的镍电极。

Description

一种镍电极的制作工艺
本发明涉及一种电池电极的制作工艺,适用于含镍电极的碱性充电电池制作工艺。
背景技术:
目前含镍电极的充电电池的镍电极的制作工艺通常有以下几种:
1、以活性物质氢氧化镍为主体加入作为导电剂的金属钴或钴的氧化物或化合物构成镍电极;
2、以活性物质氢氧化镍为主体加入作为导电剂的金属钴或钴的化合物再加上至少一种过渡金属元素和至少一种稀土元素或碱土金属元素的复合氧化物构成镍电极;
3、以包覆二价或三价钴的氢氧化镍为主体加入适量添加剂而构成镍电极
以上几种工艺有一个共同的特点,即在镍电极中引入了钴的氧化物或化合物,不论钴以二价或三价的形式加入镍电极或氢氧化镍中,在化成后都会以三价的CoOOH作为导电网络的形式存在。因可充电电池均存在不同程度的自放电,所以在长期储存或高温储存时电池的镍电极的电位会显著降低,因CoOOH在镍电极的电位降低时会部分或全部还原为低价态的钴,引起电池容量不可逆的损失,从而使电池储存性能劣化,导致电池的耐过充性能、循环寿命、放电平台等性能的降低。
发明内容:
本发明的目的就在于提高电池的储存性能,改善含镍电极充电电池的综合性能。
本发明的目的是通过以下方法来实现的:
本发明主要是通过在镍电极内添加一种或多种金属氧化物或化合物,达到提高电池的储存性能,改善含镍电极电池的综合性能的作用。
本发明所述的一种或多种金属氧化物或化合物,是采用在碱性溶液中标准氧化/还原电位高于0.4V,且在碱性溶液中能保持稳定的,如:二氧化锰等。本发明在镍电极中添加的金属氧化物或化合物比例为活性物质重量的0.1~15%,其加入方式为:与活性物质氢氧化镍粉末混合均匀后填充到导电基体中,制作成本发明的镍电极。
具体实施例:氢镍AA2000mAh电池
正极导电基体采用面密度为350g/m2的发泡镍,氢氧化镍采用高密度型含钴球镍,添加1%MnO2,再加入1%CoO,0.5%的高纯石墨,加入0.5%的CMC,混合均匀,正极经过正常的拉浆上粉、碾压成型,制成正极片。
负极骨架采用面密度为260g/m2的镍网,合金粉采用富镧高容量型,添加1%的PTFE和0.5%CMC,制成负极片。
电解液采用高纯KOH、NaOH(AR级)、LiOH·H2O(AR级)、Ba(OH)2,摩尔比约为:7.5∶1.5∶0.5∶0.5,比重为1.28~1.33该氢镍电池经过化成检测证明,在荷电100%状况下,在60℃高温环境下,储存28天,电池的荷电保持率大于60%,电池的开路电压大于1.25伏;在荷电100%状况下,在室温环境下,储存180天,电池的荷电保持率大于60%,电池的开路电压大于1.24伏,极大地改善了电池的长期室温储存性能。

Claims (4)

1.一种镍电极的制作工艺,通过在碱性含镍电极中添加金属氧化物或化合物。
2.根据权力要求1所述的添加物,其特征是其在碱性溶液下标准氧化/还原电极电位高于0.4V。
3.根据权利要求1所述的添加物,其特征是其在碱性溶液中能保持稳定。
4.根据权利要求1所述的添加物,其特征是其添加比例为活性物质重量的0.1~15%。
CNA2006100617365A 2006-07-21 2006-07-21 一种镍电极的制作工艺 Pending CN101110475A (zh)