CN101045309A - 一种木材防水处理的加工生产方法 - Google Patents

一种木材防水处理的加工生产方法 Download PDF

Info

Publication number
CN101045309A
CN101045309A CN 200710034892 CN200710034892A CN101045309A CN 101045309 A CN101045309 A CN 101045309A CN 200710034892 CN200710034892 CN 200710034892 CN 200710034892 A CN200710034892 A CN 200710034892A CN 101045309 A CN101045309 A CN 101045309A
Authority
CN
China
Prior art keywords
wood
water
waterproof material
drying
solid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200710034892
Other languages
English (en)
Inventor
李爱培
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200710034892 priority Critical patent/CN101045309A/zh
Publication of CN101045309A publication Critical patent/CN101045309A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种以杉木板、枋材为材料的木材防水处理的加工生产方法:先将木材干燥;然后将固态的AB防水材料放置于容器中加温至液态状态;再将干燥后的木材放置于高温液态的AB防水材料中、根据需要灵活控制温度浸泡2~5小时。采用本发明方法生产的防水杉木板块或材料,既可能保证杉木板块或材料具有良好的防水、防腐性能,又可使加工后的板块或材料,通过四面刨或机械加工后表面更加光洁平整、品质优良、质量稳定、性价比高;此外,本发明也适用于其它中软性杂木的加工生产。

Description

一种木材防水处理的加工生产方法
                                 技术领域
本发明涉及一种木质产品的加工生产方法,尤其是涉及一种杉木板枋材防水处理的加工生产方法。
                                 背景技术
随着人们崇尚自然意识的提高以及木材本身具有的天然独特优点,木质材料已经成为最受欢迎的家居装饰材料之一。据专家分析,今后我国各种木质板材市场的年增长率约在10~20%。这意味着木质板材的生产有着巨大的发展空间。但随着森林资源的日益减少,特别是珍贵材种的匮乏,木质板材供求矛盾日益突出,也变得越来越昂贵。尽管有各种仿木板材大量取代实木板材,但由于这种仿制木材档次不高,且防水性能较差,因此消费者还是愿意选择实木产品,尤其是防水性能好的实木板材。所以这种板材具有极其广阔的发展前景。
杉木是我国南方地区主要栽培树种,木材储蓄量较为丰富,年产量占全国商品木材20%以上。而且,杉木也是历史悠久的传统建材,它的“防潮耐腐,冬暖夏凉,环保舒适,经久耐用”的优良性能已是家喻户晓。但是由于缺少低成本、高效能的环保防水技术,使杉木难以在室内的厨房、卫生间和室外的亭台、楼阁等更大范围使用,因而难以在现代热火朝天的装饰大潮中展现它本来的优良品质。因此,如果能有一种加工生产方法,使杉木具备较好的防水、防腐性能,从而使普通的杉木成为多功能、广泛适用于现代家居装饰中不同环境的高品质、高附加值的产品。
                                发明内容
为解决上述技术问题,本发明提供一种木材防水处理的加工生产方法,主要加工步骤如下:
a、将木材干燥至8℃~18℃;
b、将环保固态的AB防水材料放置于容器中加温至液态状态;
c、将干燥后的木材放置入高温液态的AB防水材料中浸泡2~5小时;
D、AB防水材料的液态温度在20℃~200℃之间按需要灵活掌控。
                         具体实施方式:
实施方式1、将一根直径15cm长150cm的圆杉木齐边整形成一个边长为150cm宽12cm厚12cm的正方体木方,再用多片框锯机将方材加工成厚度10mm薄片,然后将木材干燥至8~13℃;随后将固态的AB防水材料放置于容器中加温至100℃,再将干燥过的木材放置入液态的AB防水材料中恒温浸泡2小时。
实施方式2、将一根直径20cm长200cm的杉圆木截成两段,每段各长100cm,然后齐边整形成一个边长为100cm宽18cm厚16cm的长方体木方,再用多片框锯机将木方加工成厚度15mm薄片,然后将木材干燥至10~13℃;随后将环保固态的AB防水材料放置于容器中加温至120℃,再将干燥过的木材放置入液态的AB防水材料中浸泡3小时。
实施方式3、将一根直径25cm长200cm的圆杉木齐边整形成一个边长为200cm宽厚均为22cm的正方体木方,随后用多片框锯机将枋材加工成厚度20mm薄片,然后将木材干燥至10~15℃;随后将环保固态的AB防水材料放置于容器中加温至150℃,再将干燥过的木材放置入液态的AB防水材料中浸泡5小时。
采用本发明方法生产的防水杉木薄片或板、枋材,既可能保证杉木薄片或板枋材具有良好的防水、防腐性能、不易损坏或开裂,又可使经过四面刨或机械加工出来的薄片或板枋材表面光洁平整、品质优良、质量稳定、性价比高。此外,本发明也适用于其它中软性杂木的加工生产。

Claims (2)

1、一种木材防水处理的加工生产方法,其特征在于,所述加工步骤为:
a、将木材干燥至8℃~18℃;
b、将环保、固态的AB防水材料放置于容器中加温至液态状态;
c、将干燥后的木材放置于加温液态的AB防水材料中浸泡2~5小时。
2、根据权利要求所述的木材防水处理的加工生产方法,其特征在于,所述AB防水材料的液态温度为20℃~200℃之间。
CN 200710034892 2007-04-30 2007-04-30 一种木材防水处理的加工生产方法 Pending CN101045309A (zh)