一种补漏胶及其制备方法 Download PDF

Info

Publication number
CN100338166C
CN100338166C CNB2005101239580A CN200510123958A CN100338166C CN 100338166 C CN100338166 C CN 100338166C CN B2005101239580 A CNB2005101239580 A CN B2005101239580A CN 200510123958 A CN200510123958 A CN 200510123958A CN 100338166 C CN100338166 C CN 100338166C
Authority
CN
China
Prior art keywords
leakage
repairing glue
rosin
container
materials
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CNB2005101239580A
Other languages
English (en)
Other versions
CN1766026A (zh
Inventor
张时光
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Board Technology Co., Ltd.
Original Assignee
Shenzhen Polytechnic
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Polytechnic filed Critical Shenzhen Polytechnic
Priority to CNB2005101239580A priority Critical patent/CN100338166C/zh
Publication of CN1766026A publication Critical patent/CN1766026A/zh
Application granted granted Critical
Publication of CN100338166C publication Critical patent/CN100338166C/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种补漏胶制备方法,包括如下步骤:将松香与废机油按比例混合倒入容器中并置于加热炉上升温至75~150摄氏度,使材料熔化,熔化过程中进行搅拌;搅拌至呈熔化的浓浆状态后再加入石粉,继续加热至全部熔化后,即制成补漏胶。此外,将补漏胶倒入棒状凹模中逐渐冷却后即制得补漏胶棒。所述加热炉为电磁炉。本发明还提供一种补漏胶,按照如下质量份含量包括:松香70份、废机油5~10份、石粉20~25份。本发明的方法只需将各成分按比例加入容器中并加热熔化,同时搅拌,熔化完全后即制成补漏胶,操作非常简便,成本低。制得的补漏胶以松香为主要基料并添加无机材料制作而成,是一种无毒级防水密封材料,具有优良粘接性。

Description

一种补漏胶及其制备方法
【技术领域】
本发明涉及一种补漏材料及其制备方法,尤其是指一种补漏胶及其制备方法。
【背景技术】
随着各类房屋建筑的大量涌现,建筑屋顶、屋顶水箱、楼层和水管接口以及市政净水厂的建设有可能出现的缝隙越来越多。预计每座城市每年都有几千座各类建筑量,而这些工程的屋顶、清水池、污水处理池的伸缩缝防水措施,因施工、质量、材料老化等原因,产生后破裂等和破损等现象,直接影响了使用质量,破裂处经常出现漏水而不止水等情况,给工程的使用和管理造成损失,增加了麻烦。为此,业界研制出一种补漏胶,将其涂覆于缝隙处利用补漏胶的特性来完成堵漏防水。现有的补漏胶主要是文具类的固体浆糊、或人造化工高分子材料,其补漏效果持久性并不理想,而且其制备方法较复杂。
【发明内容】
本发明所要解决的技术问题是:提供一种补漏胶,其补漏效果好,
本发明进一步所要解决的技术问题是:提供一种补漏胶制备方法,其操作简单,且制作成本低。
为解决上述技术问题,本发明采用如下技术方案:提供一种补漏胶制备方法,包括如下步骤:
A、将松香与废机油按比例混合倒入容器中并置于加热炉上升温至75~150摄氏度,使材料逐渐熔化,熔化过程中进行搅拌;
B、搅拌至呈熔化的浓浆状态后,再加入石粉,继续加热熔化,待容器中的小颗粒全部熔化后,即制成补漏胶。
上述技术方案的进一步改进在于:所述加热炉为电磁炉。
本发明还提供一种补漏胶棒的制备方法,包括如下步骤:
A、将松香与废机油按比例混合倒入容器中并置于加热炉上升温至75~150摄氏度,使材料逐渐熔化,熔化过程中进行搅拌;
B、搅拌至呈熔化的浓浆状态后,再加入石粉,继续加热熔化,待容器中的小颗粒全部熔化后,即制成补漏胶;
C:将补漏胶倒入棒状凹模中逐渐冷却后即制成补漏胶棒。
本发明还提供一种补漏胶,包括如下质量份的成分:
松香:70份;
废机油:5~10份;
石粉:20~25份。
本发明的有益效果是:本发明制备补漏胶时,只需将各成分按比例加入容器中,并置于加热炉上加热熔化,同时搅拌,待熔化完全后即制成补漏胶,操作非常简便,且制作成本低。还可将热熔的补漏胶倒入相应棒型凹模中冷却后即得到补漏胶棒以方便包装运送。所制得的补漏胶以松香为主要基料并添加无机材料合成工艺制作而成,是一种无毒级的防水密封材料。产品具有优良的粘接性,并起到密封、隔音、防水、阻尼、抗震和节能保温等作用。
【具体实施方式】
本发明提供一种补漏胶制备方法,包括如下步骤:
A、将松香与废机油按比例混合倒入容器中并置于加热炉上升温至75~150摄氏度,使材料逐渐熔化,熔化过程中进行搅拌:
B、搅拌至呈熔化的浓浆状态后,再加入石粉,继续加热熔化,待容器中的小颗粒全部熔化后,即制成补漏胶。
其中,还可根据使用需要,在步骤B之后增加一步骤C:将补漏胶倒入棒状凹模中逐渐冷却后即制成补漏胶棒。
补漏胶的各成分质量份比为松香∶废机油∶石粉=70∶(5~10)∶(20~25)。
所述加热炉为电磁炉。
熔化时间约10-25分钟左右,因电磁炉功率大小、熔化材料多少、制造环境温度、盖不盖容器盖等因素的变化而有所不同。其中的组分比例为大约比例,稍有出入成品只会稍有软硬,不影响堵漏效果。加入顺序最好先加入松脂、废机油,熔化后再加入石粉填充料。使热效果容易发挥。
该补漏胶在加热时,会熔化成浓浆状,稍凉后,可倒在棒型的模板上,待凉后,取出,补漏胶呈固体棒状,即可包装。
本发明补漏胶棒是以松香为主要基料并添加无机材料合成工艺制作而成,是一种无毒级的防水密封材料。产品具有优良的粘接性,并起到密封、隔音、防水、阻尼、抗震和节能保温等作用。使用时,将补漏胶棒用打火机点燃,把溶液滴漏在修补处即可,或用热风枪将补漏胶棒熔融在修补处即可。从而可在各种建筑材料龟裂和风化纹裂中渗入,达到补漏目的。
本产品具有良好的水密性和气密性,且耐日晒、耐油、耐久、抗腐蚀、无毒性、使用寿命长等特点。

Claims (6)

1、一种补漏胶制备方法,包括如下步骤:
A、将松香与废机油按比例混合倒入容器中并置于加热炉上升温至75~150摄氏度,使材料逐渐熔化,熔化过程中进行搅拌;
B、搅拌至呈熔化的浓浆状态后,再加入石粉,继续加热熔化,待容器中的小颗粒全部熔化后,即制成补漏胶。
2、如权利要求1所述的补漏胶制备方法,其特征在于:其中,各成分质量份比为松香∶废机油∶石粉=70∶(5~10)∶(20~25)。
3、如权利要求1或2所述的补漏胶制备方法,其特征在于:所述加热炉为电磁炉。
4、如权利要求3所述的补漏胶制备方法,其特征在于:熔化时间为10~25分钟。
5、一种补漏胶棒的制备方法,其特征在于:包括如下步骤:
A、将松香与废机油按比例混合倒入容器中并置于加热炉上升温至75~150摄氏度,使材料逐渐熔化,熔化过程中进行搅拌;
B、搅拌至呈熔化的浓浆状态后,再加入石粉,继续加热熔化,待容器中的小颗粒全部熔化后,即制成补漏胶;
C:将补漏胶倒入棒状凹模中逐渐冷却后即制成补漏胶棒。
6、如权利要求1所述方法制备的补漏胶,其特征在于包括如下质量份的成分:
松香:70份;
废机油:5~10份;
石粉:20~25份。
CNB2005101239580A 2005-11-24 2005-11-24 一种补漏胶及其制备方法 Active CN100338166C (zh)