CH93293A - Process for tanning animal hides. - Google Patents

Process for tanning animal hides.

Info

Publication number
CH93293A
CH93293A CH93293DA CH93293A CH 93293 A CH93293 A CH 93293A CH 93293D A CH93293D A CH 93293DA CH 93293 A CH93293 A CH 93293A
Authority
CH
Switzerland
Prior art keywords
sep
tanning
acid
leather
solution
Prior art date
Application number
Other languages
German (de)
Inventor
Aktiengesellschaft Chemi Worms
Original Assignee
Chemische Fabriken Worms Aktie
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chemische Fabriken Worms Aktie filed Critical Chemische Fabriken Worms Aktie
Publication of CH93293A publication Critical patent/CH93293A/en

Description

  

  Verführen zum     Gerben        tierischer        Hänte.       Der     gegenwärtige        Mangel    an vegetabili  schen     Gerbstoffen    gab die Veranlassung, nach  geeigneten     Ersatzprodukten        zrr        ,uchen.        Grof',e     Erwartungen setzte man anfangs auf die so  genannten     ..künstlichen        Gerbstoffe--,    welche       durch    Verkettung von     I'lienolsulfosäuren,

            Naphtalinsulfosäuren        lind        deren    Derivaten  mit Formaldehyd oder     andern        geeigneten     Mitteln erhalten werden. Die Erfahrung hat  aber gezeigt, dass die so hergestellten Produkte  zufolge     ihrersauren    Eigenschaften     dieLederbrii-          chig    und hart machen.     Besonders    eifrig ist     rnan     bemüht gewesen. wie aus der sehr     umfang-          reichen    Literatur Hervorgeht.

   die Abfallaugen  der     Sulfitzellstoff-Fabrikation    für     gerberische          Zwecke    brauchbar     zrr        machen,    doch konnte  bisher daraus kein einziges Produkt gewon  nen werden, welches für sich allein verwendet,  ein vollwertiges Leder ergibt (versgleiche Zeit  schrift:     "Kunststoffe-@,6.Jahrgang,   <B>1916,</B> Heft  Nr. 1, Seite 4, rechte     Spalte,    Absatz 2,  Zeile 4).  



  Es wurde nun die überraschende     Be-          obachtunggemacht,    dass man tierische Häute  
EMI0001.0036     
  
    dadtircli <SEP> gerben <SEP> kann. <SEP> daf> <SEP> man <SEP> gemischte
<tb>  Metallsalze, <SEP> einerseits <SEP> ein <SEP> Netallsalz <SEP> der
<tb>  Lignirisulfonstitrre. <SEP> und <SEP> andrerseits <SEP> ein <SEP> ent  2spreelientles <SEP> Metallsalz <SEP> einer <SEP> andern <SEP> Säure,
<tb>  wie <SEP> z. <SEP> B. <SEP> Scliwefelsiirrre, <SEP> Ameisensäure <SEP> oder
<tb>  Milch-üure <SEP> !benutzt.

   <SEP> Die <SEP> geniüss <SEP> dem <SEP> vor  liegenden <SEP> Verfahren <SEP> benutzten <SEP> Gerbstoffe <SEP> sind
<tb>  ausserordentlich <SEP> wertvolle <SEP> Gerbstoffe, <SEP> welche
<tb>  die <SEP> vegetabilischen <SEP> Gerbstoffe <SEP> voll <SEP> und <SEP> ganz
<tb>  zu <SEP> ersetzen <SEP> vermügen.
<tb>  



  Da" <SEP> Gerbverfahren, <SEP> das <SEP> sich <SEP> in <SEP> erster
<tb>  Linie <SEP> für <SEP> solche <SEP> Häute, <SEP> die <SEP> für <SEP> die <SEP> Unter  lederfabrikation <SEP> bestimmt <SEP> sind, <SEP> eignet, <SEP> kann
<tb>  beispielsweise <SEP> mit <SEP> den <SEP> nachfolgenden <SEP> gemisch  ten <SEP> Metallsalzen <SEP> ausgeübt <SEP> werden
<tb>  1. <SEP> Mit <SEP> Aluminiumsulfat <SEP> bei <SEP> CTegenwai-t
<tb>  von <SEP> ligninsulforisaureni <SEP> Aluminium;
<tb>   .@,. <SEP> -Mit <SEP> schwefelsaurem <SEP> Eisenoyv <SEP> d <SEP> Fee
<tb>  (50:,1):r <SEP> bei <SEP> Gegenwart <SEP> von <SEP> ligninsulfonsaui,ern
<tb>  Eisen.
<tb>  



  3. <SEP> MitChromsulfat <SEP> Cri <SEP> (S04);, <SEP> bei <SEP> Gegen  wart <SEP> von <SEP> ligninsulforisaureni <SEP> Chrom.
<tb>  



  CTerbt <SEP> man <SEP> mit <SEP> Aluminiumsulfat <SEP> allein, <SEP> so
<tb>  erhält <SEP> man <SEP> bekanritlieh <SEP> sogenanntes <SEP> weil.gares         Leder. Gerbt man     ausschliesslich    reit     Ferri-          srrlfat,    so erhält man Leder von     geringem          Ptendement,    Leder, die deshalb technisch für  Unterleder unbrauchbar sind. Dasselbe gilt  für die reine     Chromsulfatgerbung.     



  Die     Gerbung    mit     Ferrisulfat    in Gegen  wart von     ligninsulfonsaurern    Eisen ist als  eine richtige     Gerbung    anzusprechen; dieser       C@rerbstoff    wird sich, gleich wie die     pflanz-          lichen        Gerbstoffe,    kaum auswaschen lassen,  und infolgedessen sind die so hergestellten  Unterleder. zum Beispiel     Sohlen,    im Gebrauch  äusserst dauerhaft.  



  Bei der vorliegenden Art der     Gerbung     treten beide Komponenten gleichzeitig und  gleichmässig in das Leder ein. Sobald man  am Schnitt die Gare erkannt hat, hat man  Leder, die von beiden     Gerbstoffen    nahezu  gleichviel aufgenommen haben, und zwar  Leder von hohem     Rerrdement,    ohne dass mau  dies noch durch eine nachträgliche     Aufpolste-          rung    zu erreichen braucht.  



  Die     Verwendung    der     ligrrirrsulforrsarrrerr     Metallsalze in Mischung mit andern     lIetall-          salzen    hat gegenüber der Verwendung der  einheitlichen     ligrrirrsrrlforrsarrrerr    Salze den  grossen Vorteil, dass bei starker     Verdünnung     der wässerigen Lösung kein     Ausflocken    statt  findet.  



  Die     gemäh    dem neuen     Gerbverfahren    ver  wendeten     Mischungen    fällen tierischen Leim,  sind in Wasser löslich und zeigen die Eigen  schaften der gebräuchlichen     Gerbmittel,    indem  sie für sich, unter Beimischung natürlicher       Gerbstoffe    oder andrer Zusätze, wie auch für  die     Kombinationsgerbungen    benutzt werden  können.

           Beispiel   <I>1:</I>    Die vorbereitete Blösse wird mit     einer     etwa 2-3      ;'oigerr        Gerbbrühe,    deren     Gerbstoff          folgendermassen    hergestellt wird, behandelt  Eine wässerige Lösung von 100 kg     lignirr-          sulfonsaurem        Natrium    wird mit<B>100</B>     kg        kri-          stallisiertemAluminiumsulfat    umgesetzt. Die  Lösung kann unmittelbar als     Gerbbrühe    be  nutzt oder auch zur Trockne eingedampft  werden.

   Die     (Terbung    erfolgt je nach der    Art des     Blössenrnaterials    in Hängefarben, im  Haspel oder     Walkfass,    dementsprechend der  Gehalt der Brühe eingestellt und die Gerb  dauer geändert werden muss. Das erhaltene  Leder wird alsdann gefettet und getrocknet.

           Beispiel   <I>2:</I>    Die     Gerbung    erfolgt wie in Beispiel 1,  mit einem     CTerbstoff,    erhalten durch     Umsetzung     von 100 kg     ligrrirrsulfonsaurem        Calcium    mit  <B>170</B> kg kristallisiertem     Ferrisulfat.    Nach  dem     Abfiltrieren    des Gipses ist die erhaltene  Brühe gebrauchsfertig.

           Beispiel   <I>3:</I>         Man    gerbt mit einem     verdünnten    Gerb  extrakt, dem man durch     Umsetzung    von  <B><I>100</I></B> g     ligninsrrlfonsaurem        Calcium    mit 230 g       Chrornisrrlfatlösung    von<B>52'</B>     Be    nach     Abfil-          trierung    des Gipses erhalten hat.

           Beisl)iel   <I>i</I>         Man    gerbt mit einem Gerbstoff, den man  dadurch erhalten hat, dass mau 100 g     lignin-          sulfonsaures    Chrom auf 200     ccm    eines syn  thetischen     Gerbstoffes        einwirken    liess, welch  letzterer durch     Erhitzen        von    200 g     hresolen     aus Urteer mit 360 g 30     0/(,igem        Forrnaldehyd     und 330 g neutralem     Natriumsrrlfit    in 600 g       Wasser.    durch.

       Ansäuern    des Reaktions  produktes, Verkochen der schwefligen Säure.  darauffolgendes     Neutralisieren    und     Urnsetzerr     mit 256 g     Chromisulfatlösung    von<B>52'</B>     Be     erhalten worden ist.

           Betspiel   <B><I>J:</I></B>         Man    gerbt mit einer     Gerbbrühe,        hergestellt     durch Verdünnung eines     Gerbextraktes.    den  man dadurch erhält, dass     rnan    eine Lösung  von 100 g     ligninsulfonsaurern    Natrium zu einer  durch Umsetzen von     .155    ccm     Aluminium-          sulfaltlösung    von 25       Be    mit einer Auflösung  von 130 g     Natriumformiat    in 200 ccm Wasser  erhaltenen     Aluminiumformiatlösung    gibt,

   und  das     Glaubersalz        auskristallisieren        lässt.              Beispiel   <I>G:</I>  Man gerbt mit einem entsprechend ver  dünnten     Gerbextrakt,

      erhalten durch Uni  setzung von 285 g     Chroinisulfatlösung    von  <B>25"</B>     B6    mit 210g     Natriuniformiat    in 250     g-          Wasser    und     Versetzung    mit einer     Auflösung     von 100     g        ligninsulfoiisaureni        Natrium    nach  dein Auskristallisieren des Glaubersalzes.

      <I>Beispiel 7:</I>    Man gerbt mit einem entsprechend ver  dünnten     Glerbextrakt,    erhalten durch Um  setzung von 100     g    mit     Natronlauge    neutrali  sierter Milchsäure     finit    88 g     Chroinisulfatlauge     von 52       Be,    Zusetzen einer Lösung von 150 g       li-ninsulfoiisaurein        Natrium    in     -100    g Wasser  und Auskristallisieren des     Glaubersalzes.  



  Seduce to tanning animal roosters. The current shortage of vegetable tanning agents gave rise to the search for suitable substitute products. Initially, great expectations were placed on the so-called ... artificial tannins, which are produced by the chain of lienol sulfonic acids,

            Naphthalene sulfonic acids and their derivatives can be obtained with formaldehyde or other suitable agents. However, experience has shown that the products made in this way make the leather fragile and hard due to their acidic properties. I tried particularly hard. as can be seen from the very extensive literature.

   to make the waste eyes of the sulphite pulp production usable for tanning purposes, but so far not a single product could be obtained from it which, when used on its own, results in a fully-fledged leather (different journal: "Kunststoffe - @, 6th year, <B. > 1916, </B> Issue No. 1, page 4, right column, paragraph 2, line 4).



  The surprising observation has now been made that one can use animal skins
EMI0001.0036
  
    dadtircli <SEP> tan <SEP> can. <SEP> daf> <SEP> man <SEP> mixed
<tb> metal salts, <SEP> on the one hand <SEP> a <SEP> metal salt <SEP> the
<tb> Lignirisulfonstitrre. <SEP> and <SEP> on the other hand <SEP> a <SEP> ent 2spreelientles <SEP> metal salt <SEP> of a <SEP> other <SEP> acid,
<tb> like <SEP> e.g. <SEP> B. <SEP> sulfuric acid, <SEP> formic acid <SEP> or
<tb> Milk acid <SEP>! is used.

   <SEP> The <SEP> enjoy <SEP> the <SEP> present <SEP> procedure <SEP> used <SEP> tanning agents <SEP> are
<tb> extremely <SEP> valuable <SEP> tannins, <SEP> which
<tb> the <SEP> vegetable <SEP> tannins <SEP> full <SEP> and <SEP> whole
<tb> to replace <SEP> <SEP> may.
<tb>



  Since "<SEP> tanning process, <SEP> the <SEP> is <SEP> in <SEP> first
<tb> Line <SEP> for <SEP> such <SEP> skins, <SEP> which <SEP> for <SEP> which <SEP> are <SEP> intended under leather manufacture <SEP>, <SEP> suitable, <SEP > can
<tb> for example <SEP> with <SEP> the <SEP> following <SEP> mixed <SEP> metal salts <SEP> can be used <SEP>
<tb> 1. <SEP> With <SEP> aluminum sulfate <SEP> at <SEP> CTegenwai-t
<tb> of <SEP> ligninsulforisaureni <SEP> aluminum;
<tb>. @ ,. <SEP> - With <SEP> sulfuric acid <SEP> Eisenoyv <SEP> d <SEP> Fee
<tb> (50:, 1): r <SEP> at <SEP> presence <SEP> of <SEP> lignosulfonic acid, ern
<tb> iron.
<tb>



  3. <SEP> With chromium sulfate <SEP> Cri <SEP> (S04) ;, <SEP> at <SEP> present <SEP> of <SEP> ligninsulforisaureni <SEP> chromium.
<tb>



  CTake <SEP> one <SEP> with <SEP> aluminum sulfate <SEP> alone, <SEP> like this
<tb> receives <SEP> one <SEP> known <SEP> so-called <SEP> because.gares leather. If one tans exclusively on the basis of ferrite, leather of low pendulousness is obtained, leather which is therefore technically unusable for lower leather. The same applies to pure chromium sulfate tanning.



  The tanning with ferric sulphate in the presence of lignosulphonic acid iron is to be regarded as a correct tanning; Like the vegetable tanning agents, this cereal can hardly be washed out, and as a result the lower leathers produced in this way are. For example, soles, extremely durable in use.



  In the case of the present type of tanning, both components enter the leather simultaneously and evenly. As soon as you have recognized the grain from the cut, you have leather that has absorbed almost the same amount of both tannins, namely leather with a high level of dementia, without the need to achieve this by subsequent padding.



  The use of the metal salts in a mixture with other metal salts has the great advantage over the use of the uniform salts that no flocculation takes place if the aqueous solution is strongly diluted.



  The mixtures used according to the new tanning process precipitate animal glue, are soluble in water and show the properties of the common tanning agents in that they can be used by themselves, with the addition of natural tanning agents or other additives, as well as for combination tanning.

           Example <I> 1: </I> The prepared pelt is treated with about 2-3; 'oigerr tanning liquor, the tanning agent of which is prepared as follows. An aqueous solution of 100 kg of sodium lignin sulfonic acid is treated with <B> 100 </ B> kg of crystallized aluminum sulfate implemented. The solution can be used directly as a tanning liquor or it can be evaporated to dryness.

   The (tanning takes place depending on the type of pelt material in hanging colors, in a reel or drum, the content of the stock must be adjusted accordingly and the tanning time changed. The leather obtained is then greased and dried.

           Example <I> 2: </I> The tanning is carried out as in Example 1, with a C tanning agent obtained by reacting 100 kg of calcium sulfonic acid with 170 kg of crystallized ferrous sulfate. After filtering off the plaster of paris, the resulting broth is ready for use.

           Example <I> 3: </I> Tanning is carried out with a dilute tanning extract which is obtained by reacting <B><I>100</I> </B> g of calcium lignin with 230 g of chromium chloride solution of <B> 52 '</B> Be received after filtering off the plaster.

           For example, tanning is carried out with a tanning agent that has been obtained by letting 100 g of lignin sulfonic acid chromium act on 200 cc of a synthetic tanning agent, which the latter is produced by heating 200 g of hresols Primordial tar with 360 g of 30% formaldehyde and 330 g of neutral sodium chloride in 600 g of water.

       Acidification of the reaction product, boiling of the sulphurous acid. subsequent neutralization and conversion with 256 g chromium sulfate solution of <B> 52 '</B> Be has been obtained.

           Betspiel <B><I>J:</I> </B> One tans with a tanning broth, produced by diluting a tanning extract. which is obtained by adding a solution of 100 g of sodium lignosulphonic acid to an aluminum formate solution obtained by reacting .155 ccm of aluminum sulphalt solution of 25 Be with a dissolution of 130 g of sodium formate in 200 ccm of water,

   and lets the Glauber's salt crystallize. Example <I> G: </I> You tanning with an appropriately diluted tanning extract,

      obtained by adding 285 g of chroinisulphate solution of <B> 25 "</B> B6 with 210g of sodium formate in 250 g of water and adding 100 g of sodium lignin sulfate after the Glauber's salt has crystallized out.

      <I> Example 7: </I> One tans with a correspondingly diluted yellow extract, obtained by reacting 100 g of lactic acid neutralized with sodium hydroxide solution, 88 g of chroinisulphate liquor of 52 Be, adding a solution of 150 g of sodium in sodium sulphide -100 g water and crystallization of the Glauber's salt.

 

Claims (1)

PATEN TANSPRUCI3 Verfahren zum Gerben tierischer Häute, dadurch gekennzeichnet, dar geinischteMetall- salze, welche aus einem Ligninsulfonsiiure- metallsalz und einem entsprechenden Metallsalz einer andern Säure bestehen, benutzt werden. LT\TERANSPRüCIIE 1. Verfahren nach Patentanspruch, dadurch gekennzeichnet, dar die Säure eine or ganische ist. 2. Verfahren nach Patentanspruch, dadurch gekennzeichnet, dar die andre Säure eine anorganische ist. 3. Verfahren nach Patentanspruch, dadurch gekennzeichnet, dar den benutzten Metall salzen andre Gerbstoffe zugesetzt werden. PATEN TANSPRUCI3 Process for tanning animal skins, characterized in that mixed metal salts consisting of a lignosulfonic acid metal salt and a corresponding metal salt of another acid are used. LT \ TERANSPRüCIIE 1. Process according to claim, characterized in that the acid is an organic one. 2. The method according to claim, characterized in that the other acid is an inorganic one. 3. The method according to claim, characterized in that other tanning agents are added to the metal used. -1. Verfahren nach Patentansliruch, dadurch gekennzeichnet, daI den benutzten Metall salzen nicht gerbende Stoffe zugesetzt werden. -1. Method according to patent claim, characterized in that non-tanning substances are added to the metal salts used.
CH93293D 1918-11-16 1920-12-01 Process for tanning animal hides. CH93293A (en)